    摘要: Metallic alloys are disclosed containing Fe at 48.0 to 81.0 atomic percent, B at 2.0 to 8.0 atomic percent, Si at 4.0 to 14.0 atomic percent, and at least one or more of Cu, Mn or Ni, wherein the Cu is present at 0.1 to 6.0 atomic percent, Mn is present at 0.1 to 21.0 atomic percent and Ni is present at 0.1 to 16.0 atomic percent. The alloys may be heated at temperatures of 200° C. to 850° C. for a time period of up to 1 hour and upon cooling there is no eutectoid transformation. The alloys may then be formed into a selected shape.

    摘要翻译: 公开了含有48.0〜81.0原子%的Fe,2.0〜8.0原子%的B,4.0〜14.0原子%的Si,Cu,Mn或Ni中的至少一种以上的金属的合金,其中Cu以0.1〜 6.0原子%,Mn为0.1〜21.0原子%,Ni为0.1〜16.0原子%。 合金可以在200℃至850℃的温度下加热一段时间至多1小时,并且在冷却时不存在共析转变。 然后可以将合金形成为选定的形状。