公开(公告)号:US20220056229A1
公开(公告)日:2022-02-24
申请号:US17428781
申请日:2020-02-19
Applicant: UNITIKA LTD.
Inventor: Takashi Okabe , Nobuyasu Okumura , Masafumi Yamamoto , Kumi Ashihara , Midori Shimomura , Yoshimi Ueno
Abstract: A laminated film having a resin layer laminated on at least one surface of a base film. The laminated film is characterized by: the base film being a semi-aromatic polyamide film that has been at least uniaxially stretched; the resin layer having a thickness of 0.03 to 0.5 μm; and the close adhesion between the base film and the resin layer, according to the cross-cut method described in JIS K 5600, being 95% or more.
-
公开(公告)号:US12180347B2
公开(公告)日:2024-12-31
申请号:US17785564
申请日:2021-11-16
Applicant: UNITIKA LTD.
Inventor: Takashi Okabe , Nobuyasu Okumura , Kumi Ashihara
Abstract: A laminated film having a resin layer laminated on at least one surface of a base film. The laminated film is characterized by: the base film being a semi-aromatic polyamide film that has been at least uniaxially stretched; the resin layer containing fine particles; the thermal shrinkage factor in the longitudinal direction SMD and the thermal shrinkage factor in the width direction STD of the film measured under conditions of 250° C.×5 minutes each being −1.0 to 1.5%; the tensile elongations at break in the longitudinal direction and in the width direction each being 70% or more; and the haze being 3% or less.
-
公开(公告)号:US20220220256A1
公开(公告)日:2022-07-14
申请号:US17610468
申请日:2020-05-13
Applicant: UNITIKA LTD.
Inventor: Takashi Okabe , Masafumi Yamamoto , Sumito Kihara
Abstract: A semi-aromatic polyamide film having a thermal shrinkage factor in the longitudinal direction of the film, SMD, of −1.0 to 1.5% and a thermal shrinkage factor in the width direction of the film, STD, of −1.0 to 1.5% as measured under the conditions of 250° C. and 5 min, a tensile breaking elongation of 70% or more in the longitudinal direction and the width direction, and a haze of 14% or less.
-
公开(公告)号:US20150251389A1
公开(公告)日:2015-09-10
申请号:US14425486
申请日:2013-09-10
Applicant: UNITIKA LTD.
Inventor: Atsushi Maehara , Takashi Okabe , Kazunari Nanjo , Arihiro Anada
CPC classification number: B32B27/08 , B32B27/18 , B32B27/20 , B32B27/30 , B32B27/304 , B32B27/306 , B32B27/32 , B32B27/34 , B32B27/36 , B32B27/365 , B32B2307/518 , B32B2307/7244 , B32B2439/46 , B65D31/02 , C08J7/047 , C08J2367/00 , C08J2367/02 , C08J2377/00 , C08J2377/02 , C08J2429/04 , C08J2433/02 , Y10T428/1341 , Y10T428/31725 , Y10T428/31786
Abstract: Disclosed is a gas barrier laminate including a gas barrier layer (II) laminated on a plastic substrate (I), wherein the plastic substrate (I) includes a metal compound in a content of 0.1 to 70% by mass and the gas barrier layer (II) includes a polycarboxylic acid.
Abstract translation: 本发明公开了一种阻气性层压体,其包含层叠在塑料基板(I)上的阻气层(II),其中,所述塑料基板(I)含有0.1〜70质量%的金属化合物和阻气层 II)包括多元羧酸。
-
公开(公告)号:US11965072B2
公开(公告)日:2024-04-23
申请号:US18015180
申请日:2022-03-25
Applicant: UNITIKA LTD.
Inventor: Yuki Aoyama , Takashi Okabe , Shuhei Yamane , Tomoko Yamanaka
CPC classification number: C08J5/18 , B29C55/12 , B29C71/02 , B32B15/088 , B32B17/10724 , B32B27/34 , B32B2250/02 , B32B2307/558 , B32B2307/734 , B32B2457/20 , C08J2377/10
Abstract: Provided is a semiaromatic polyamide fil having an average linear expansion coefficient in the width direction, measured under conditions of 20 to 125° C., of −90 to 0 ppm/° C.
-
-
-
-