摘要:
The present invention provides a method of preparing a transparent polymer material, the method comprising steps i) and ii) in any order, the steps consisting in: i) mixing: mineral nanoparticles having a form factor strictly greater than 1.0; and a polymer matrix comprising a quantity of at least 80% by weight of a polycarbonate (PC) first thermoplastic polymer and of a second transparent thermoplastic polymer other than the first thermoplastic polymer, in order to obtain a mixture; and ii) heating the polymer matrix to the molten state, on its own or in the mixture; to obtain the transparent, polymer material, the mixture of step i) comprising a quantity of mineral nanoparticles having a form factor strictly greater than 1.0 that is strictly less than 5% by weight.
摘要:
The present invention provides a method of preparing a transparent polymer material, the method comprising steps i) and ii) in any order, the steps consisting in: i) mixing: mineral nanoparticles having a form factor strictly greater than 1.0; and a polymer matrix comprising a quantity of at least 80% by weight of a polycarbonate (PC) first thermoplastic polymer and of a second transparent thermoplastic polymer other than the first thermoplastic polymer, in order to obtain a mixture; and ii) heating the polymer matrix to the molten state, on its own or in the mixture; to obtain the transparent, polymer material, the mixture of step i) comprising a quantity of mineral nanoparticles having a form factor strictly greater than 1.0 that is strictly less than 5% by weight.
摘要:
A method of preparing a transparent polymer material includes mixing mineral nanoparticles selected from nanoparticles of alkaline-earth metal carbonates, alkaline-earth metal sulfates, metallic oxides, oxides of metalloids, and siloxanes, and a composition A including at least one thermoplastic polymer in the molten state selected from polycarbonate (PC), polystyrene (PS) and polymethyl methacrylate (PMMA) in order to obtain a master-batch, the mixture of step i) including at least 25% and at most 75% by weight of the mineral nanoparticles. The master-batch obtained in step i) is mixed with a composition B of a thermoplastic polycarbonate matrix (PCm) in the molten state, to obtain a transparent polymer material including at most 10% by weight of the mineral nanoparticles, preferably at most 5% by weight of the mineral nanoparticles.
摘要:
A method of preparing a transparent polymer material includes mixing mineral nanoparticles selected from nanoparticles of alkaline-earth metal carbonates, alkaline-earth metal sulfates, metallic oxides, oxides of metalloids, and siloxanes, and a composition A including at least one thermoplastic polymer in the molten state selected from polycarbonate (PC), polystyrene (PS) and polymethyl methacrylate (PMMA) in order to obtain a master-batch, the mixture of step i) including at least 25% and at most 75% by weight of the mineral nanoparticles. The master-batch obtained in step i) is mixed with a composition B of a thermoplastic polycarbonate matrix (PCm) in the molten state, to obtain a transparent polymer material including at most 10% by weight of the mineral nanoparticles, preferably at most 5% by weight of the mineral nanoparticles.
摘要:
A method of preparing a transparent polymer material includes i) obtaining composite nanoparticles having mineral nanoparticles at least partially coated with at least one monomer and/or at least one polymer suitable for promoting physicochemical interactions at the interface between the mineral nanoparticles and a thermoplastic polycarbonate matrix, the mineral nanoparticles being surface-modified by the monomer and/or the polymer, either directly by grafting or directly by adsorption of the monomer and/or polymer onto the surface of the mineral nanoparticles; or via a coupling agent selected from a chlorosilane or an organosilane including a functional group that is capable of reacting by a radical pathway. The composite nanoparticles obtained in step i) are mixed with the thermoplastic polycarbonate matrix in the molten state to obtain the transparent polymer material.
摘要:
A method of preparing a transparent polymer material includes i) obtaining composite nanoparticles having mineral nanoparticles at least partially coated with at least one monomer and/or at least one polymer suitable for promoting physicochemical interactions at the interface between the mineral nanoparticles and a thermoplastic polycarbonate matrix, the mineral nanoparticles being surface-modified by the monomer and/or the polymer, either directly by grafting or directly by adsorption of the monomer and/or polymer onto the surface of the mineral nanoparticles; or via a coupling agent selected from a chlorosilane or an organosilane including a functional group that is capable of reacting by a radical pathway. The composite nanoparticles obtained in step i) are mixed with the thermoplastic polycarbonate matrix in the molten state to obtain the transparent polymer material.