    摘要: The present invention relates to nonwoven webs or fabrics. In particular, the present invention relates to nonwoven webs having superior abrasion resistance and excellent softness characteristics. The nonwoven materials comprise monocomponent fibers having a surface comprising a polyethylene, said nonwoven material having a fuzz/abrasion of less than 0.7 mg/cm3. The present invention is also related to fibers having a diameter in a range of from 0.1 to 50 denier, said fibers comprising a polymer blend, wherein the polymer blend comprises: from 40 weight percent to 80 weight percent (by weight of the polymer blend) of a first polymer which is a homogeneous ethylene/α-olefin interpolymer having: a melt index of from about 1 to about 1000 grams/10 minutes, and a density of from 0.870 to 0.950 grams/centimeter3, and from 74 to 20 percent by weight of a second polymer which is an ethylene homopolymer or an ethylene/α-olefin interpolymer having a melt index of from about 1 to about 1000 grams/10 minutes, and preferably a density which is at least 0.01 grams/centimeter3 greater than the density of the first polymer.

    摘要翻译: 本发明涉及非织造纤维网或织物。 特别地,本发明涉及非织造纤维网,其具有优异的耐磨性和优异的柔软性。 非织造材料包括具有包含聚乙烯的表面的单组分纤维,所述非织造材料具有小于0.7mg / cm 3的绒毛/磨损。 本发明还涉及直径在0.1-50旦范围内的纤维,所述纤维包括聚合物共混物,其中聚合物共混物包含:40重量%至80重量%(以聚合物共混物的重量计) 的第一聚合物,其是均匀的乙烯/α-烯烃互聚物,其熔体指数为约1至约1000克/ 10分钟,密度为0.870-0.950克/厘米3 ,和74至20重量%的第二聚合物,其是熔体指数为约1至约1000克/ 10分钟的乙烯均聚物或乙烯/α-烯烃互聚物,优选至少为密度 0.01克/厘米3比第一聚合物的密度大。

    CROSSLINKED POLYETHYLENE COMPOSITION HAVING IMPROVED PROCESSABILITY
    5.
    发明申请
    CROSSLINKED POLYETHYLENE COMPOSITION HAVING IMPROVED PROCESSABILITY 有权
    交联聚乙烯组合物具有改进的可加工性

    公开(公告)号:US20150291774A1

    公开(公告)日:2015-10-15

    申请号:US14405220

    申请日:2012-06-04

    IPC分类号: C08K5/36 C08K5/3492 C08K5/14

    摘要: Disclosed in the present invention is a crosslinked polyethylene composition having improved processability comprises: 100 parts by weight of polyethylene, 0.03-5 parts by weight of crosslinking agent, 0.03-5 parts by weight of crosslinking promoter, and 0.01-1.5 parts by weight of free radical inhibitor, wherein the polyethylene is a copolymer and/or homopolymer containing at least 90 wt. % of vinyl and at least one C3-C8 α-alkenyl, and has a density in the range of 0.920-0.970 g/cm3, a melt index in the range of 2.5-17.5 g/10 min; the crosslinking agent is a peroxide crosslinking agent; the crosslinking promoter is an organic substance containing maleimido, (meth)acrylate group, and/or allyl, and/or a polymer containing more than 50% of vinyl; the free radical inhibitor is an organic antioxidant, a quinhydrone and/or a substituted quinhydrone. The crosslinked polyethylene composition of the present invention has a crosslinking efficiency index of more than 1,100 Nm/g and a δ torque value of more than 10 Nm at the temperature of 200° C., a significantly higher safety process temperature and a significantly improved crosslinking retardation time compared to the conventional crosslinked polyethylene composition, which make it especially be suitable for the production of rotational molding articles.

    摘要翻译: 在本发明中公开的是具有改进的加工性的交联聚乙烯组合物,包括:100重量份的聚乙烯,0.03-5重量份的交联剂,0.03-5重量份的交联促进剂和0.01-1.5重量份的 自由基抑制剂,其中聚乙烯是共聚物和/或均聚物,其含有至少90wt。 %的乙烯基和至少一个C 3 -C 8α-烯基,其密度在0.920-0.970g / cm 3范围内,熔体指数在2.5-17.5g / 10min的范围内; 交联剂是过氧化物交联剂; 交联促进剂是含有马来酰亚胺基,(甲基)丙烯酸酯基和/或烯丙基的有机物,和/或含有50%以上乙烯基的聚合物; 自由基抑制剂是有机抗氧化剂,醌氢醌和/或取代的氢醌。 本发明的交联聚乙烯组合物在200℃的温度下具有大于1100Nm 3 / g的交联效率指数和大于10Nm的δ扭矩值,显着更高的安全性工艺温度和明显改善的交联 延迟时间与传统的交联聚乙烯组合物相比,特别适用于生产旋转模塑制品。