A laminate (C) of a thermoplastic polymer composition comprising: a thermoplastic resin composition (A) having an permeation coefficient of 10×10−12 cc·cm/cm2·sec·cmHg or less, laminated with a thermoplastic polymer composition (B) having a melt viscosity of 500-2000 Pa·s and a Young's modulus at a room temperature of 1-400 MPa, wherein the thickness of a layer of the thermoplastic resin composition (A) is 0.05-10 μm and the air permeation coefficient of the laminate (C) of 20×10−12 cc·cm/cm2·sec·cmHg or less, and a pneumatic tire using the above laminate (C) as an inner liner.
摘要:
A polyamide resin composition, having an excellent extensibility and flexing fatigue, composed of a polyamide resin (A), as a matrix, and a modifying polymer (C), dispersed therein, having a functional group (B) reactive with the polyamide resin (A), wherein a tensile stress at break of the modifying polymer (C) is 30 to 70% of the tensile stress at break of the polyamide resin (A), and a tensile elongation at break of the modifying polymer (C) is 100 to 500% of the tensile elongation at break of the polyamide resin (A) as well as a pneumatic tire and hose using the same.
摘要:
A polyamide resin composition, having an excellent extensibility and flexing fatigue, composed of a polyamide resin (A), as a matrix, and a modifying polymer (C), dispersed therein, having a functional group (B) reactive with the polyamide resin (A), wherein a tensile stress at break of the modifying polymer (C) is 30 to 70% of the tensile stress at break of the polyamide resin (A), and a tensile elongation at break of the modifying polymer (C) is 100 to 500% of the tensile elongation at break of the polyamide resin (A) as well as a pneumatic tire and hose using the same.
摘要:
A laminate (C) of a thermoplastic polymer composition comprising: a thermoplastic resin composition (A) having an permeation coefficient of 10×10−12 cc·cm/cm2·sec·cmHg or less, laminated with a thermoplastic polymer composition (B) having a melt viscosity of 500-2000 Pa·s and a Young's modulus at a room temperature of 1-400 MPa, wherein the thickness of a layer of the thermoplastic resin composition (A) is 0.05-10 μm and the air permeation coefficient of the laminate (C) of 20×10−12 cc·cm/cm2·sec·cmHg or less, and a pneumatic tire using the above laminate (C) as an inner liner.
摘要:
Provided is a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The composition can be used as an inner liner of a pneumatic tire.
摘要:
Provided is a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The composition can be used as an inner liner of a pneumatic tire.
摘要:
Provided is a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The composition can be used as an inner liner of a pneumatic tire.
摘要:
Provided is a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The composition can be used as an inner liner of a pneumatic tire.
摘要:
An object of the invention is to provide a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide resin, even if a halogenated isoolefin/para-alkylstyrene copolymer rubber is finely dispersed and loaded to a high content. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The thermoplastic elastomer composition can be favorably used as an inner liner of a pneumatic tire.
摘要:
A low permeability laminate obtained by laminating (A) a thermoplastic resin composition layer containing (i) 50 to 90% by weight of an ethylene vinyl alcohol copolymer having an ethylene content of 20 to 50 mol % and a saponification degree of 90% or more, (ii) 50 to 10% by weight of an aliphatic polyamide resin having 90 mol % or more of an ε-caprolactam-derived component and (iii) 3 to 50 parts by weight of a sulfonamide-based plasticizer, based upon 100 parts by weight of the total amount of the components (i) and (ii) and (B) at least one rubber composition layer, a layer of a thickness εB of layer (B)/a thickness εA of layer (A) (εB/εA) being 10 or more, followed by being heat treated within a range of 130° C. to 210° C. capable of molding and processing for a long time and a pneumatic tire using the same.