摘要:
Heat-resistant resin composition comprising (A) 100 parts by weight of a poly(arylene sulfide) of a substantially linear structure containing 50% by weight or higher of recurring units of the formula ##STR1## and a logarithmic viscosity number of 0.1 to 1.0 dl/g; (B) from 0.01 to less than 25 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR2## wherein the --CO-- and --S-- are in the para position to each other, and having a melting point of 310.degree.-380.degree. C., a residual melt crystallization enthalpy of at least 10 J/g, a melt crystallization temperature of at least 210.degree. C. and a reduced viscosity of 0.2 to 2 dl/g; and (C) at least one of fibrous fibers and/or at least one of inorganic fillers in a proportion of 0 to 400 parts by weight per 100 parts by weight of the resin component comprising said poly(arylene sulfide) and said poly(arylene thioether-ketone). Heat-resistant articles obtained by melt-molding or forming said resin compositions and a method for the production of such articles are also described.
摘要:
Disclosed herein is a melt-stable poly(arylene thioether-ketone) composition, which comprises:(A) 100 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C. and a reduced viscosity of 0.2-2 dl/g;(B) 0-400 parts by weight of at least one of thermoplastic resins; and(C) at least one of fibrous fillers and/or at least one of inorganic fillers in a proportion of 0-400 parts by weight per 100 parts by weight of the sum of said components (A) and (B).At least either one of the components (B) or (C) is contained in a proportion of at least 0.1 part by weight per 100 parts by weight of the component (A).
摘要:
Disclosed herein are a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.2-2 dl/g as measured at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 wt. % sulfuric acid as well as a production process of the poly(arylene thioether-ketone). The poly(arylene thioether-ketone) has melt stability so that conventional melt processing techniques can be applied easily. The poly(arylene thioether-ketone) is a highly-crystalline polymer whose density is at least 1.34 g/cm.sup.3 when annealed at 280.degree. C. for 30 minutes.
摘要:
Heat-resistant resin composition including (A) 100 parts by weight of a poly(arylene sulfide) of a substantially linear structure containing 50% by weight or higher or recurring units of the formula ##STR1## and a logarithmic viscosity number of 0.1 to 1.0 dl/g; (B) from 0.01 to less than 25 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR2## wherein the --CO-- and --S-- are in the para position to each other, and having a melting point of 310.degree.-380.degree. C., a residual melt crystallization enthalpy of at least 10 J/g, a melt crystallization temperature of at least 210.degree. C. and a reduced viscosity of 0.2 to 2 dl/g; and (C) at least one of fibrous fibers and/or at least one of inorganic fillers in a proportion of 0 to 400 parts by weight per 100 parts by weight of the resin component including said poly(arylene sulfide) and said poly(arylene thioether-ketone). Heat-resistant articles obtained by melt-molding or forming said resin compositions and a method for the production of such articles are also described.
摘要:
Disclosed herein are a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.2-2 dl/g as measured at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 wt. % sulfuric acid as well as a production process of the poly(arylene thioether-ketone). The poly(arylene thioether-ketone) has melt stability so that conventional melt processing techniques can be applied easily. The poly(arylene thioether-ketone) is a highly-crystalline polymer whose density is at least 1.34 g/cm.sup.3 when annealed at 280.degree. C. for 30 minutes.
摘要:
Disclosed herein are poly(arylene thioether-ketone) fibers obtained by melt-spinning a thermoplastic material which comprises 100 parts by weight of a melt-stable poly(arylene thioether-ketone) (PTK) and optionally, up to 50 parts by weight of at least one of thermoplastic resins. The PTK has predominant recurring units of the formula ##STR1## wherein the --CO-- and --S-- are in the para position to each other, and has a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.3-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sulfuric acid. The PTK fibers of this invention have high heat resistance and strength.
摘要:
Disclosed herein is a stretched poly(arylene thioether-ketone) film made of a thermoplastic material which comprises (A) 100 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g and a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.3-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sufuric acid; and optionally, (B) up to 100 parts by weight of at least one of thermoplastic resins and/or up to 15 parts by weight of at least one of fillers. Its production process is also disclosed.
摘要:
Disclosed herein are poly(arylene thioetherketone) fibers obtained by melt-spinning a thermoplastic material which comprises 100 parts by weight of a melt-stable poly(arylene thioether-ketone) (PTK) and optionally, up to 50 parts by weight of at least one of thermoplastic resins. The PTK has predominant recurring units of the formula ##STR1## wherein the --CO-- and --S-- are in the para position to each other, and has a melting point, Tm of 310-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.3-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sulfuric acid. The PTK fibers of this invention have high heat resistance and strength.
摘要:
Disclosed herein is a molded or formed poly(arylene thioether-ketone) article made of a thermoplastic material which comprises 100 parts by weight of a melt-stable poly(arylene thioether-ketone) (PTK) and if desired, up to 100 parts by weight of at least one of thermoplastic resins and/or up to 300 parts by weight of at least one of fibrous fillers and/or least one of inorganic fillers. The PTK has predominant recurring units of the formula ##STR1## wherein the --CO-- and --S-- are in the para position to each other, and has a melting point, Tm of 310.degree.-380.degree. C., a residual melt cyrstallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g, a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.2-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sulfuric acid. This invention provides extruded articles, injection-molded articles, unstretched films and the like, all of which have practical physical properties, by using a novel high-density and high crystallinity PTK having melt stability sufficient to apply conventional melt processing techniques.
摘要:
Disclosed herein is a stretched poly(arylene thioether-ketone) film made of a thermoplastic material which comprises (A) 100 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g and a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.3-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sulfuric acid; and optionally, (B) up to 100 parts by weight of at least one of thermoplastic resins and/or up to 15 parts by weight of at least one of fillers. Its production process is also disclosed.