FOAM SHEET, PRODUCT, AND METHOD FOR PRODUCING FOAM SHEET

    公开(公告)号:US20220162377A1

    公开(公告)日:2022-05-26

    申请号:US17530593

    申请日:2021-11-19

    摘要: Provided is a foam sheet including a composition including polylactic acid. The polylactic acid includes, as monomer units, D-lactic acid and L-lactic acid, and an amount of the D-lactic acid or the L-lactic acid in the polylactic acid is 90 mol % or greater but less than 98 mol %. An amount of the polylactic acid is 97% by mass or greater relative to a total amount of organic matter in the foam sheet. When the foam sheet is cut into a square test piece, and the test piece is heated and stored for 90 minutes in a hot air circulation dryer a temperature of which is maintained at 90° C.±2° C., a change rate of an area of the test piece before and after the heat storage is within ±15%. An average thickness of the foam sheet is 0.5 mm or greater.

    Toner, developer, toner storage unit, image forming apparatus, and image forming method

    公开(公告)号:US10599058B2

    公开(公告)日:2020-03-24

    申请号:US16238566

    申请日:2019-01-03

    IPC分类号: G03G9/08 G03G9/087 G03G15/08

    摘要: A toner comprising a binder resin is provided. When the toner is observed with an atomic force microscope in tapping mode to obtain a phase image and the phase image is binarized with an intermediate value between maximum and minimum phase difference values in the phase image to obtain a binarized image, the binarized image consists of first phase-contrast portions having a large phase difference and second phase-contrast portions having a small phase difference, where the first phase-contrast portions are dispersed in the second phase-contrast portions and a dispersion diameter of the first phase-contrast portions is in a range of from 150 to 500 nm. The toner has at least two glass transition temperatures (Tg) in respective ranges of from 40° C. to 65° C. and from −30° C. to 20° C., determined from a DSC curve obtained at a first temperature rise in a differential scanning calorimetric measurement by a midpoint method.

    METHOD FOR PRODUCING POLYMER AND POLYMER PRODUCT
    8.
    发明申请
    METHOD FOR PRODUCING POLYMER AND POLYMER PRODUCT 审中-公开
    生产聚合物和聚合物产品的方法

    公开(公告)号:US20140350209A1

    公开(公告)日:2014-11-27

    申请号:US14374065

    申请日:2013-01-25

    IPC分类号: C08G63/08 C08G63/78

    摘要: A method for producing a polymer, including: (i) bringing a compressive fluid and raw materials containing a ring-opening polymerizable monomer into contact with each other at a mixing ratio represented by the following formula, to thereby allow the ring-opening polymerizable monomer to carry out ring-opening polymerization in the presence of a metal catalyst: 1{Mass of the raw materials/(Mass of the raw materials+Mass of the compressive fluid)}0.5.

    摘要翻译: 一种聚合物的制造方法,其特征在于,包括:(i)使含有开环聚合性单体的压缩液和原料以下述式表示的混合比例进行接触,由此使开环聚合性单体 在金属催化剂存在下进行开环聚合:1 {原料质量/(原料质量+压缩流体质量)} 0.5。