Method for producing coated steel sheet
    1.
    发明申请
    Method for producing coated steel sheet 有权
    涂层钢板的制造方法

    公开(公告)号:US20050064107A1

    公开(公告)日:2005-03-24

    申请号:US10502670

    申请日:2003-01-24

    摘要: In a process for manufacturing a coated steel sheet such as a coated electromagnetic steel sheet using a water-based coating liquid containing an organic resin, to perform steps subsequent to an annealing step continuously at high speed without causing appearance defects such as coating unevenness; to provide an electromagnetic steel sheet having an insulating film thereon, in which properties of the film are satisfactory, superior weldability and punchability can be obtained without deteriorating the space factor, and the satisfactory film properties can be maintained even if the electromagnetic steel sheet having the insulating film thereon is temper-rolled. A coating liquid is applied onto an untreated steel sheet. The applied liquid is heated on the side close to the steel sheet in such a manner that the time elapsed until the steel sheet temperature is increased to 100° C. after the application is completed is 10 seconds or less, thereby drying the coating liquid. The steel sheet temperature is further increased to a predetermined temperature, thereby forming a coating film. When insulating films for electromagnetic steel sheets are formed, the coating liquid preferably further contains a water based inorganic component.

    摘要翻译: 在使用含有有机树脂的水性涂布液的涂布电磁钢板的涂布钢板的制造方法中,高速连续地进行退火工序后的工序,不会引起涂布不均匀等的外观缺陷; 为了提供一种其上具有绝缘膜的电磁钢板,其中膜的性能令人满意,可以获得优异的焊接性和冲压性,而不会使空间因素变差,并且即使具有 对其上的绝缘膜进行回火。 将涂布液施加到未处理的钢板上。 所施加的液体在靠近钢板的一侧被加热,使得在施加完成之后直到钢板温度升高到100℃的时间为10秒以下,从而使涂布液干燥。 钢板温度进一步提高到预定温度,从而形成涂膜。 当形成用于电磁钢板的绝缘膜时,涂布液优选还含有水基无机组分。

    Method for producing coated steel sheet
    2.
    发明授权
    Method for producing coated steel sheet 有权
    涂层钢板的制造方法

    公开(公告)号:US08709550B2

    公开(公告)日:2014-04-29

    申请号:US10502670

    申请日:2003-01-24

    IPC分类号: B05D5/06

    摘要: In a process for manufacturing a coated steel sheet such as a coated electromagnetic steel sheet using a water-based coating liquid containing an organic resin, to perform steps subsequent to an annealing step continuously at high speed without causing appearance defects such as coating unevenness; to provide an electromagnetic steel sheet having an insulating film thereon, in which properties of the film are satisfactory, superior weldability and punchability can be obtained without deteriorating the space factor, and the satisfactory film properties can be maintained even if the electromagnetic steel sheet having the insulating film thereon is temper-rolled. A coating liquid is applied onto an untreated steel sheet. The applied liquid is heated on the side close to the steel sheet in such a manner that the time elapsed until the steel sheet temperature is increased to 100° C. after the application is completed is 10 seconds or less, thereby drying the coating liquid. The steel sheet temperature is further increased to a predetermined temperature, thereby forming a coating film. When insulating films for electromagnetic steel sheets are formed, the coating liquid preferably further contains a water based inorganic component.

    摘要翻译: 在使用含有有机树脂的水性涂布液的涂布电磁钢板的涂布钢板的制造方法中,高速连续地进行退火工序后的工序,不会引起涂布不均匀等的外观缺陷; 为了提供一种其上具有绝缘膜的电磁钢板,其中膜的性能令人满意,可以获得优异的焊接性和冲压性,而不会使空间因素变差,并且即使电磁钢板具有 对其上的绝缘膜进行回火。 将涂布液施加到未处理的钢板上。 所施加的液体在靠近钢板的一侧被加热,使得在施加完成之后直到钢板温度升高到100℃的时间为10秒以下,从而使涂布液干燥。 钢板温度进一步提高到预定温度,从而形成涂膜。 当形成用于电磁钢板的绝缘膜时,涂布液优选还含有水基无机组分。

    Semiprocessed nonoriented magnetic steel sheet having excellent magnetic
characteristics and method for making the same
    3.
    发明授权
    Semiprocessed nonoriented magnetic steel sheet having excellent magnetic characteristics and method for making the same 失效
    具有优异磁特性的半加工非取向磁钢板及其制造方法

    公开(公告)号:US5876520A

    公开(公告)日:1999-03-02

    申请号:US930396

    申请日:1997-09-30

    摘要: The present invention relates to a semiprocessed nonoriented magnetic steel sheet which is used in iron cores of motors and transformers, finished to a final product by rolling having a reduction rate of 2 to 18% after final annealing by a manufacturer, and assures desired magnetic characteristics due to coarsening of crystal grains during strain-relief annealing after processing by a user. The excellent magnetic characteristics can be achieved by increasing lubrication during second cold rolling so as to satisfy the equation: e.sub.c .ltoreq.e.sub.s .ltoreq.1.18e.sub.c wherein e.sub.s represents a strain value at the surface layer of the steel sheet and e.sub.c represents a strain value at the central layer.

    摘要翻译: PCT No.PCT / JP97 / 00287 Sec。 371日期:1997年9月30日 102(e)1997年9月30日PCT PCT 1997年2月6日提交PCT公布。 出版物WO97 / 30180 PCT 日期:1997年8月21日本发明涉及用于电动机和变压器的铁芯的半加工非取向磁钢板,其通过制造商进行最终退火后的轧制精度为2〜18%的轧制成品, 并且由用户处理之后的应变消除退火期间由于晶粒粗化而确保期望的磁特性。 可以通过在第二次冷轧期间增加润滑来实现优异的磁特性,以满足以下等式:其中es表示钢板表层的应变值,ec表示应变 价值在中央层。

    Method of manufacturing a nonoriented electromagnetic steel sheet
    4.
    发明申请
    Method of manufacturing a nonoriented electromagnetic steel sheet 审中-公开
    制造无取向电磁钢板的方法

    公开(公告)号:US20080060728A1

    公开(公告)日:2008-03-13

    申请号:US11978406

    申请日:2007-10-29

    IPC分类号: C21D8/02

    摘要: A method for manufacturing a non-oriented electrical steel sheet including hot-rolling a steel slab containing 0-0.010% of C; at least one of Si and Al in a total amount of 0.03% to 0.5%; 0.5% or less of Mn; 0.10% or more to 0.26% or less of P; 0.015% or less of S; and 0.010% or less of N, on a mass percentage basis, the remainder being Fe and unavailable impurities, under conditions of a heating temperature in a single-phase austenite region and a coiling temperature of 650° C. or less; descaling the hot-rolled sheet to cold-roll the descaled sheet once or twice or more with an intermediate annealing sub-step therebetween; and then finish-annealing the cold-rolled sheet at a temperature of 700° C. or more in the single-phase ferrite region.

    摘要翻译: 一种无取向电工钢板的制造方法,其特征在于,包括:含0-0.010%C的钢板的热轧; Si和Al中的至少一种总量为0.03%至0.5%; 0.5%以下的Mn; 0.10%以上至0.26%以下的P; 0.015%以下的S; 在单相奥氏体区域的加热温度和卷绕温度为650℃以下的条件下,以质量%计,为0.010%以下的N,余量为Fe和不可见的杂质; 对热轧板进行除鳞,将其剥离后的中间退火子步骤冷轧一次或两次以上, 然后在单相铁素体区域中在700℃以上的温度下对冷轧板进行最终退火。

    PI-ELECTRON CONJUGATED BLOCK COPOLYMER AND PHOTOELECTRIC CONVERSION ELEMENT
    5.
    发明申请
    PI-ELECTRON CONJUGATED BLOCK COPOLYMER AND PHOTOELECTRIC CONVERSION ELEMENT 审中-公开
    PI-ELECTRON共混嵌段共聚物和光电转换元件

    公开(公告)号:US20140084220A1

    公开(公告)日:2014-03-27

    申请号:US14004563

    申请日:2012-03-09

    IPC分类号: H01L51/00

    摘要: Provided is a conjugated block copolymer that is capable of morphology control and that can achieve superior conversion efficiency. A π-electron conjugated block copolymer contiguously or non-contiguously bonding polymer block (A) involving a monomer unit having in a portion of a chemical structure at least one heteroaryl skeleton selected from a thiophene, a fluorine, a carbazole, a dibenzosilole and a dibenzogermole; and a polymer block (B) involving a monomer unit similarly having at least one heteroaryl skeleton; wherein the polymer block (A) comprises a homopolymer block of a monomer unit having a substituent RnA that is an alkoxy group or an alkyl group having 1-18 carbon atoms, and the polymer block (B) comprises a copolymer block of at least two different each other types of monomer units having substituent RnB selected from an alkoxy group or an alkyl group having 1-18 carbon atoms, which may be substituted with an alkoxy group, a halogen atom, a hydroxyl group, an amino group, a thiole group, a silyl group, an ester group, an aryl group, hetero aryl group.

    摘要翻译: 提供能够形态控制并且可以实现优异的转化效率的共轭嵌段共聚物。 涉及具有化学结构部分中的至少一个选自噻吩,氟,咔唑,二苯并噻唑的杂芳基骨架的单体单元的邻苯二胺共轭嵌段共聚物连续或非连续键合聚合物嵌段(A) 二苯并呋喃; 和包含类似地具有至少一个杂芳基骨架的单体单元的聚合物嵌段(B); 其中所述聚合物嵌段(A)包含具有取代基RnA(其为烷氧基或具有1-18个碳原子的烷基)的单体单元的均聚物嵌段,并且所述聚合物嵌段(B)包含至少两个 具有可以被烷氧基,卤素原子,羟基,氨基,硫代基团取代的具有1-18个碳原子的烷氧基或烷基的取代基RnB的不同类型的单体单元 甲硅烷基,酯基,芳基,杂芳基。

    GROOVED NOODLES AND PROCESS FOR PRODUCING THE SAME
    6.
    发明申请
    GROOVED NOODLES AND PROCESS FOR PRODUCING THE SAME 审中-公开
    用于生产其的花岗岩及其工艺

    公开(公告)号:US20100080882A1

    公开(公告)日:2010-04-01

    申请号:US12524460

    申请日:2008-01-17

    IPC分类号: A23L1/16

    摘要: It is intended to provide noodles which require a highly shortened boiling time compared with non-grooved noodles and are still comparable to non-grooved noodles in appearance, taste, and texture after cooking. The above described problem is solved by providing grooved noodles in which a maximum diameter in the cross-section of a single noodle band is from 1.2 mm to 3.0 mm and the major outer shape thereof is an arc of a circle or ellipse, or the cross-section of a single noodle band has a rectangular or substantially rectangular shape, wherein: said noodles have a plurality of grooves formed along the longitudinal direction of said noodle band; and the total area of the section of said plurality of grooves in the cross-section of said noodle band is 20 to 50% of the area of the circle or ellipse formed by the major outer shape of the cross-section of said noodle band, or the rectangular or substantially rectangular shape of said cross-section.

    摘要翻译: 旨在提供与非沟槽面相比需要高度缩短的煮沸时间的面条,并且在烹饪后的外观,味道和质地上仍然可以与非沟槽面相当。 上述问题是通过提供一种带状的面条来解决的,其中单面条带的横截面中的最大直径为1.2mm至3.0mm,其主外形为圆形或椭圆形,或十字形 单条面条的切片具有矩形或大致矩形形状,其中:所述面条具有沿着所述面条的纵向方向形成的多个凹槽; 所述面条的横​​截面中的所述多个槽的截面的总面积为由所述面条的横​​截面的主外形形成的圆或椭圆的面积的20〜50% 或所述横截面的矩形或大致矩形形状。

    Silver halide photographic light-sensitive material
    7.
    发明授权
    Silver halide photographic light-sensitive material 失效
    卤化银照相感光材料

    公开(公告)号:US5374498A

    公开(公告)日:1994-12-20

    申请号:US061310

    申请日:1993-05-13

    IPC分类号: G03C1/047 G03C1/053 G03C1/06

    摘要: A silver halide photographic light-sensitive material is disclosed. The light-sensitive material comprises a support having thereon a silver halide emulsion layer, wherein the silver halide emulsion layer contains a hydrazine derivative, and at least one of the silver halide emulsion layer and another hydrophilic colloid layer provided on the emulsion layer-coated side of the support contains a latex comprising polymer particles stabilized with gelatin.

    摘要翻译: 公开了一种卤化银照相感光材料。 感光材料包括其上具有卤化银乳剂层的载体,其中卤化银乳剂层含有肼衍生物,并且在乳剂层涂覆侧上提供至少一种卤化银乳剂层和另一亲水胶体层 的载体含有包含用明胶稳定的聚合物颗粒的胶乳。

    Extruded elongate pasta, and die structure and extruder for forming the
same
    8.
    发明授权
    Extruded elongate pasta, and die structure and extruder for forming the same 失效
    挤压细长面条,以及用于成型的模具结构和挤出机

    公开(公告)号:US4752205A

    公开(公告)日:1988-06-21

    申请号:US42880

    申请日:1987-04-27

    摘要: Extruded elongate pasta is disclosed, each pasta strand having at least one groove formed longitudinally in the pasta strand in such a manner that the total cross sectional area of the groove is 2 to 25% of the cross sectional area of the pasta strand, and the groove in the pasta strand is substantially closed after the elongate pasta is boiled or dipped in hot water. A die structure for extruding the elongate pasta is also disclosed, the die structure being so arranged that a projection is projected toward the axis of a die hole from the inner surface of the die hole and that the coefficient of friction of the inner surface of the die hole is 0.4 or less. It is preferable that a tapered portion is formed on the upstream end of the projection. Further, an extruder for forming the elongate pastas which has a number of such die holes is also disclosed, in which projections of the die holes are projected perpendicularly to the aligning direction of the die holes.

    摘要翻译: 公开了挤压细长面条,每个面条均具有至少一个在面料线中纵向形成的凹槽,该凹槽的总横截面面积为面条的横截面面积的2至25% 在将细长的面食煮沸或浸入热水中之后,面条中的凹槽基本上封闭。 还公开了用于挤出细长面条的模具结构,模具结构被布置成使得突出部从模孔的内表面朝向模孔的轴线突出,并且内表面的摩擦系数 模孔为0.4以下。 优选在突起的上游端形成有锥形部。 此外,还公开了一种用于形成具有多个这种模孔的细长面料的挤出机,其中模孔的突出部垂直于模孔的对准方向突出。

    Rubber vibration isolator for muffler
    9.
    发明授权
    Rubber vibration isolator for muffler 失效
    消声器橡胶隔振器

    公开(公告)号:US4727957A

    公开(公告)日:1988-03-01

    申请号:US945752

    申请日:1986-12-23

    申请人: Akio Fujita

    发明人: Akio Fujita

    CPC分类号: F01N13/1822 F16F7/108

    摘要: A rubber vibration isolator is used as a muffler hanger or muffler mount between a car body and a muffler to hang the latter from the former. The isolator includes a body made of rubber-like elastic material whose damping factor is high, two holes, upper and lower, formed in the center of the body of rubber-like elastic material, and a weight provided between the two holes and supported at opposite sides thereof by rubber-like elastic members. The rubber vibration isolator is advantageous in that coefficients of transfer of vibrations of both high and low frequencies, respectively, are lowered.