摘要:
A Steckel mill has a reversing unit for rolling a rolled product and winding furnaces arranged on the entrance side and exit side of the reversing unit. When rolling the rolled product in a region of a head of the rolled product, a target thickness of the rolled product is ignored, while measuring a current thickness and/or a hardness of the rolled product and comparing this with a setpoint value. One the measured variable reaches or is below the setpoint value, the reversing unit is operated with a view to achieving the target thickness of the rolled product. The Steckel mill is operated to allow for rolling of a cold, non-rollable piece of the rolled product, so that malfunctions are avoided and the usable part of the rolled product is as large as possible.
摘要:
A rolling mill edger includes a pair of work rolls (1, 2) and a feed roll assembly. The assembly includes one or more driven feed rolls (23) and a drive for the feed rolls. The feed roll assembly is mounted on a moveable (25) mount such that the feed roll assembly is movable by pivoting the assembly between an operative rolling position (54) in the edger and a roll change position (55) out of the edger.
摘要:
A hot coiler drum working at 900-1200° C. includes: a drum body (3), two flanges (1), several radial rib plates (5) and several axial rib plates (6). The several radial rib plates (5) are fixedly arranged on an inner wall of the drum body (3) uniformly along the axial direction of the drum body (3), the several axial rib plates (6) are arranged on the inner wall of the drum body (3) uniformly except a window (4) zone of the drum body (3), and the axial rib plates (6) and the radial rib plates (5) are welded with the drum body (3) into a whole. A method for producing the drum is also provided. The manufacturing method replaces casting with welding, which eliminates the need for a large-sized casting device, thereby enhancing the finished product rate using simple processing.
摘要:
The present disclosure relates to a hot rolling apparatus for manufacturing a metal plate by hot-rolling-treating a metal material including copper. The apparatus includes: a rough rolling device for rolling-treating the metal material, which has been heating-treated, a plurality of times with a back-and-forth movement of the metal material, to mold the metal material into a metal plate; a heat retention/application treatment device for retaining heat of or applying heat to the metal plate molded by the rough rolling device at lower temperatures than in the heating treatment, without applying bending; a finish rolling device for further rolling-treating the metal plate that has been heat-treated by the heat retention/application treatment device; a cooling device for cooling the metal plate that has been rolling-treated by the finish rolling device; and a support table for movably supporting the metal plate from below before and after the rough rolling device while the metal material is moved back and forth by the rough rolling device. According to the present disclosure, it is possible to improve the quality of the metal plate manufactured in the hot rolling apparatus, and also to improve the speed of the process required for rolling.
摘要:
In a method for producing hot strips from a deformable lightweight steel which includes as main elements Fe, Mn, Si and Al, melt is cast close to its final dimension in a horizontal continuous strip casting installation under a protective gas to form a pre-strip between 6 and 20 mm, and the temperature of the pre-strip is adjusted after complete solidification and before the beginning of a hot-rolling process. The pre-strip is passed through a device under a protective gas for homogenization in concert with a selective maintenance of the temperature, cooling or heating, and subsequently subjected to a hot-rolling process having at least one pass with a total degree of deformation of at least 50%, and is then reeled as a hot strip following the cooling process. The hot-rolling process is executed in-line or in decoupled manner depending on the ratio of casting speed to rolling speed.
摘要:
Surface defects in rolled steel are remedied by quenching a surface layer of the steel product downstream of the caster and upstream of the reheat furnace by transversely differentiated quenching to match the transverse temperature profile of the steel product. The flow rate of the quench spray is differentially adjustable across the width and optionally the length of the steel product. An array of spray nozzles controlled in transversely or longitudinally arranged groups provides the quench spray.
摘要:
A method and a plant for the hot rolling of strip, in which the rolling stock is rolled in at least one reversing roughing stand with a number of roughing passes into a broken-down strip, and the broken-down strip is transported over an intermediate roller table into at least one Steckel finishing stand and the strip is finish-rolled in the finishing stand with a number of passes into a finished strip having a predetermined thickness, and the strip is finally wound into a coil. The length of the intermediate roller table determined by the length of the broken-down strip is shortened and tandem rolling is carried out in the roughing stand and the finishing stand at least during the last breaking-down pass of the strip.
摘要:
The present invention is a method and apparatus for the production of both discrete metal plate and coiled metal plate products. In a mill having at least two in-line reversing plate mill stands, a reheated slab can be rolled on a first reversing plate mill in several reversing flat passes. The rolled product can then be sent to a second in-line reversing plate mill for additional rolling followed by winding in a downstream coiler. In the present invention, while the rolled product is sent to the second reversing plate mill, a virgin reheated slab can be introduced and rolled on the first reversing plate mill in several reversing flat passes. This product, subsequent to a slab which is rolled and sent to the second reversing plate mill, can be sent upstream along runout tables for further processing in finishing equipment. When the first reversing plate mill is again clear of rolled product, another virgin reheated slab can be introduced to the first mill and the above process can be repeated. By this method and apparatus, at least two reversing plate mill stands can be operated to produce both discrete metal plate product and coiled metal product.
摘要:
The in-line combination of a reversing rolling mill (Steckel mill) and its coiler furnaces with accelerated controlled cooling apparatus immediately downstream thereof and associated method permits steel to be sequentially reversingly rolled to achieve an overall reduction of at least about 3:1, imparted by a first reduction while the steel is kept at a temperature above the T.sub.nr by the coiler furnaces so as to preserve an optimum opportunity for controlled recrystallization of the steel after each rolling pass, and a second reduction while the temperature of the steel drops from about the T.sub.nr to about the Ar.sub.3. The second reduction is preferably of the order of 2:1 as a result of which the steel reaches a final plate thickness. The steel product then passes through the accelerated controlled cooling apparatus, preferably applying laminar flow cooling at least to the upper surface of the steel passing therethrough so as to reduce the temperature of the steel from about the Ar.sub.3 to a temperature at least about 250 C. to about 300 C. or more below the Ar.sub.3 at a cooling rate of at about 12 C. to about 20 C. and preferably about 15 C. per second, thereby to achieve a preferred fine-grained predominantly bainite structure affording enhanced strength and toughness in the final steel product.
摘要:
A Steckel mill or coiler rolling mill includes at least one reversing stand and drivers and coiler furnaces arranged on the entry side and the exit side of the reversing stand, wherein the reversing stand, the drivers and the coiler furnaces are connected to one another through roller conveyors for the strip to be rolled. At least one heating unit is provided in at least one of the sections formed between the coiler furnaces and the reversing stand, wherein the heating unit covers at least a portion of the section.