Method for making multiple durometer bulb seals
    1.
    发明授权
    Method for making multiple durometer bulb seals 有权
    制造多个硬度灯泡密封件的方法

    公开(公告)号:US09321209B2

    公开(公告)日:2016-04-26

    申请号:US14211651

    申请日:2014-03-14

    摘要: Method for making multiple durometer bulb seals includes cooling separately at least one structural member and at least one bulb portion of the bulb seal, which have different durometers and shapes. At least a first extrusion is drawn through a die of an extruder for forming a structural member profile and the extruded material is pulled by a first pulling device along a longitudinal axis to a first calibrator device and then through a first cooling tank to cool the structural member profile to a predetermined temperature. Cooling medium directly contacts the outer and inner surfaces of the first profile. The bulb portion is extruded and attached onto the cooled structural member and pulled downstream to a second calibrator device and through a second cooling tank to cool the profile a predetermined amount. Disparity in cooling expansion and cooling differential between the multiple durometers and shapes is avoided or overcome.

    摘要翻译: 制造多个硬度计灯泡密封件的方法包括分别冷却具有不同硬度和形状的至少一个结构构件和灯泡密封件的至少一个灯泡部分。 至少第一挤出物通过用于形成结构构件轮廓的挤出机的模头被拉伸,并且将挤出的材料沿着纵向轴线由第一牵引装置拉动到第一校准器装置,然后通过第一冷却罐以冷却结构 构件轮廓到预定温度。 冷却介质直接接触第一型材的外表面和内表面。 将灯泡部分挤出并附着在冷却的结构件上,并将其下游拉到第二校准器装置,并通过第二冷却槽将轮廓冷却预定量。 避免或克服了多个硬度计和形状之间的冷却膨胀和冷却差异的差异。

    METHOD FOR MAKING MULTIPLE DUROMETER BULB SEALS
    4.
    发明申请
    METHOD FOR MAKING MULTIPLE DUROMETER BULB SEALS 有权
    制造多个DUROMETER BULB密封件的方法

    公开(公告)号:US20140265051A1

    公开(公告)日:2014-09-18

    申请号:US14211651

    申请日:2014-03-14

    IPC分类号: B29C47/06 B29C47/00

    摘要: Method for making multiple durometer bulb seals includes cooling separately at least one structural member and at least one bulb portion of the bulb seal, which have different durometers and shapes. At least a first extrusion is drawn through a die of an extruder for forming a structural member profile and the extruded material is pulled by a first pulling device along a longitudinal axis to a first calibrator device and then through a first cooling tank to cool the structural member profile to a predetermined temperature. Cooling medium directly contacts the outer and inner surfaces of the first profile. The bulb portion is extruded and attached onto the cooled structural member and pulled downstream to a second calibrator device and through a second cooling tank to cool the profile a predetermined amount. Disparity in cooling expansion and cooling differential between the multiple durometers and shapes is avoided or overcome.

    摘要翻译: 制造多个硬度计灯泡密封件的方法包括分别冷却具有不同硬度和形状的至少一个结构构件和灯泡密封件的至少一个灯泡部分。 至少第一挤出物通过用于形成结构构件轮廓的挤出机的模头被拉伸,并且将挤出的材料沿着纵向轴线由第一牵引装置拉动到第一校准器装置,然后通过第一冷却罐以冷却结构 构件轮廓到预定温度。 冷却介质直接接触第一型材的外表面和内表面。 将灯泡部分挤出并附着在冷却的结构件上,并将其下游拉到第二校准器装置,并通过第二冷却槽将轮廓冷却预定量。 避免或克服了多个硬度计和形状之间的冷却膨胀和冷却差异的差异。

    METHOD FOR MAKING MULTIPLE DUROMETER SEALS
    10.
    发明申请
    METHOD FOR MAKING MULTIPLE DUROMETER SEALS 有权
    制造多个密度计的方法

    公开(公告)号:US20160046056A1

    公开(公告)日:2016-02-18

    申请号:US14926577

    申请日:2015-10-29

    IPC分类号: B29C47/06 B29C47/88 B29C47/00

    摘要: Method for making multiple durometer bulb seals and any other types of multiple durometer seals and moldings includes cooling separately at least one structural member and at least one sealing portion, which have different durometers and shapes. At least a first extrusion is drawn through an extruder, forming a structural member profile and the extruded material is pulled along a longitudinal axis to a first calibrator device and first cooling tank to cool the structural member profile to a predetermined temperature. Cooling medium directly contacts the outer and inner surfaces of the first profile. Downstream, the sealing portion is extruded and affixed onto the cooled structural member and pulled further downstream to a second calibrator device and through a second cooling tank to cool the final profile a predetermined amount. Disparity in cooling expansion and cooling differential between the multiple durometers and shapes is avoided or overcome.

    摘要翻译: 用于制造多个硬度计灯泡密封件和任何其它类型的多重硬度密封件和模制件的方法包括分别冷却至少一个结构构件和至少一个具有不同硬度和形状的密封部分。 至少第一挤出物通过挤出机拉伸,形成结构构件轮廓,并且将挤出的材料沿着纵向轴线拉动到第一校准器装置和第一冷却罐以将结构构件轮廓冷却至预定温度。 冷却介质直接接触第一型材的外表面和内表面。 在下游,将密封部分挤出并固定在冷却的结构件上,并进一步向下游延伸到第二校准器装置,并通过第二冷却箱将最终轮廓冷却至预定量。 避免或克服了多个硬度计和形状之间的冷却膨胀和冷却差异的差异。