COMPOSITION AND METHOD FOR MANUFACTURING SULFONE POLYMER MEMBRANE
    3.
    发明申请
    COMPOSITION AND METHOD FOR MANUFACTURING SULFONE POLYMER MEMBRANE 审中-公开
    制备磺化聚合物膜的组合物和方法

    公开(公告)号:WO2017157933A1

    公开(公告)日:2017-09-21

    申请号:PCT/EP2017/055984

    申请日:2017-03-14

    Abstract: The invention pertains to a polyaryl ether sulfone polymer solution [solution (SP)] comprising: - at least one sulfone polymer [polymer (PSI)] having recurring units, wherein more than 50 % moles, with respect to all the recurring units of polymer (PSI), are recurring units (R PSI ) selected from the group consisting of those of formulae (R PSI -1) and (R PSI -2) herein below : (R PSI -1) (R PSI -2) wherein : - each of E', equal to or different from each other and at each occurrence, is selected from the group consisting of those of formulae (E'-1) to (E'-3): (E'-I) (E'-II) (E'-III) - each R' is independently selected from the group consisting of halogen, alkyl, alkenyl, alkynyl, aryl, ether, thioether, carboxylic acid, ester, amide, imide, alkali or alkaline earth metal sulfonate, alkyl sulfonate, alkali or alkaline earth metal phosphonate, alkyl phosphonate, amine and quaternary ammonium; and - j' is zero or an integer of 1 to 4; is a bond or a divalent group optionally comprising one or more than one heteroatom; preferably T is selected from the group consisting of a bond, -CH 2 -, -C(O)-, -C(CH 3 ) 2 -, -C(CF 3 ) 2 -, -C(=CCI 2 )-, -C(CH 3 )(CH 2 CH 2 COOH)-, and a group of formula : (A) - at least one polar organic solvent [solvent (S)]; and - at least one mixture of polyhydroxyl aliphatic alcohols having from 1 to 6 carbon atoms or derivatives thereof [mixture (PHA)], said mixture (PHA) comprising at least one ethylene glycol compound [compound (EthyGly)] and at least one glycerol compound [compound (Gly)], to its use for manufacturing membranes, and to membranes obtained therefrom.

    Abstract translation: 本发明涉及一种聚芳基醚砜聚合物溶液[溶液(SP)],其包含: - 至少一种具有重复单元的砜聚合物[聚合物(PSI)],其中多于50%摩尔与 (PSI)的重复单元是重复单元(R PSI),其选自式(R PSI-1)和(R PSI-1) (PSI-2)(PSI-2),其中: - 每个E'等于(R PSI-2) (E'-1)(E'-I)(E'-I)(E'-I)的那些化合物(E' -III) - 每个R'独立地选自卤素,烷基,链烯基,炔基,芳基,醚,硫醚,羧酸,酯,酰胺,酰亚胺,碱金属或碱土金属磺酸盐,烷基磺酸盐,碱金属或 碱土金属膦酸盐,膦酸烷基酯,胺和季铵; 和-j'为零或1至4的整数; 是任选地包含一个或多于一个杂原子的键或二价基团; 优选T选自键,-CH 2 - , - C(O) - , - C(CH 3)2 - -C(CF 3)2 - , - C(= CCl 2) - , - C(CH 3) (A) - 至少一种极性有机溶剂[溶剂(S) - (甲基)丙烯酸酯) ]。 和 - 至少一种具有1至6个碳原子的多羟基脂肪醇或其衍生物[混合物(PHA)]的混合物,所述混合物(PHA)包含至少一种乙二醇化合物[化合物(乙基甘油)]和至少一种甘油 化合物[化合物(Gly)],用于制造膜的用途,以及由其获得的膜。

    FLAT SHEET MEMBRANE
    4.
    发明申请
    FLAT SHEET MEMBRANE 审中-公开
    平板薄膜

    公开(公告)号:WO2017143395A1

    公开(公告)日:2017-08-31

    申请号:PCT/AU2017/050155

    申请日:2017-02-22

    Inventor: ERSKINE, Craig

    Abstract: A method of forming a titanium membrane plate (18) for use in a cross flow filtration system (10) wherein a resin layer is sprayed onto a template and dried; a layer of titanium powder is coated onto the dried resin layer using supersonic particle deposition to form the titanium membrane plate (18); and the titanium membrane plate (18) and dried resin layer are dipped in a chemical bath that dissolves the resin layer leaving the titanium membrane plate (18).

    Abstract translation: 一种形成用于错流过滤系统(10)中的钛膜板(18)的方法,其中将树脂层喷涂到模板上并干燥; 使用超声粒子沉积将干燥的树脂层涂覆一层钛粉以形成钛膜板(18); 并将钛膜板(18)和干燥树脂层浸入溶解离开钛膜板(18)的树脂层的化学浴中。

    ゼオライト膜構造体及びその製造方法
    9.
    发明申请
    ゼオライト膜構造体及びその製造方法 审中-公开
    沸石膜结构及其生产方法

    公开(公告)号:WO2016158583A1

    公开(公告)日:2016-10-06

    申请号:PCT/JP2016/059048

    申请日:2016-03-22

    Abstract:  ゼオライト膜構造体(10)は、多孔質支持体(20)と、ゼオライト膜(30)とを備える。ゼオライト膜(30)は、多孔質支持体(20)の表面(23S)の内側に配置される第1ゼオライト層(31)と、多孔質支持体(20)の表面(23S)の外側に配置され、第1ゼオライト層(31)と一体形成される第2ゼオライト層(32)とを有する。多孔質支持体(20)は、第1ゼオライト層(31)が配置される最表層(23a)を有する。第1ゼオライト層(31)の平均厚みは、5.4μm以下である。最表層(23a)の平均細孔径は、0.050μm以上0.150μm以下である。

    Abstract translation: 这种沸石膜结构(10)设有多孔载体(20)和沸石膜(30)。 沸石膜(30)具有设置在多孔性支撑体(20)的表面(23S)的内侧的第一沸石层(31)和设置在表面(23S)的外侧的第二沸石层(32) 的多孔支撑体(20),并与第一沸石层(31)整体形成。 多孔载体(20)具有设置第一沸石层(31)的最外层(23a)。 第一沸石层(31)的平均厚度为5.4μm以下。 最外层(23a)的平均孔径为0.050〜1.50μm。

    シリカ膜及び分離膜フィルタ
    10.
    发明申请
    シリカ膜及び分離膜フィルタ 审中-公开
    硅胶膜和分离膜过滤器

    公开(公告)号:WO2016148132A1

    公开(公告)日:2016-09-22

    申请号:PCT/JP2016/058109

    申请日:2016-03-15

    Abstract: シリカ膜フィルタ10は、多孔質基材13と、多孔質基材13上に形成されアリール基を有するシリカ膜18とを備える。このシリカ膜18は、エネルギー分散型X線分光法(EDX)での元素分析による原子数比Si/Cが0.2以上15以下の範囲である。また、シリカ膜18は、膜厚が30nm以上300nm以下の範囲であることが好ましく、フーリエ変換赤外吸収スペクトル(FT-IR)における、Si-O-Si結合の吸収強度Xとアリール基に基づく吸収強度Yとの比X/Yが5.0以上200以下の範囲であることが好ましい。

    Abstract translation: 二氧化硅膜过滤器10设置有形成在多孔基材13上并含有芳基的多孔基材13和二氧化硅膜18。 根据使用能量色散X射线光谱法(EDX)进行的元素分析,二氧化硅膜18中的Si原子数与C原子数的比例为0.2〜15。二氧化硅膜18的厚度 优选为30nm〜300nm。 如果X是傅里叶变换红外(FTIR)吸收光谱中的Si-O-Si键的吸收强度,Y是基于所述光谱中的芳基的吸收强度,则X / Y的比例优选为 为5.0〜200。