Abstract:
A surface-modified silicate luminophore includes a silicate luminophore and a coating includes at least one of (a) a fluorinated coating including a fluorinated inorganic agent, a fluorinated organic agent, or a combination of fluorinated inorganic and organic agents, the fluorinated coating generating hydrophobic surface sites and (b) a combination of the fluorinated coating and at least one moisture barrier layer. The moisture barrier layer includes MgO, Al2O3, Y2O3, La2O3, Gd2O3, Lu2O3, and SiO2 or the corresponding precursors, and the coating is disposed on the surface of the silicate luminophore.
Abstract translation:表面改性硅酸盐发光体包括硅酸盐发光体,涂层包括(a)包含氟化无机物,氟化有机物或氟化无机和有机物的组合的氟化涂层中的至少一种,氟化涂层产生疏水性 表面部位和(b)氟化涂层和至少一个防潮层的组合。 防潮层包括MgO,Al 2 O 3,Y 2 O 3,La 2 O 3,Gd 2 O 3,Lu 2 O 3和SiO 2或相应的前体,并且涂层设置在硅酸盐发光体的表面上。
Abstract:
Disclosed are non-stoichiometric Copper Alkaline Earth Silicate phosp hors activated by divalent europium for using them as high temperature stable luminescent mat erials for ultraviolet or daylight excitation. The phosphors are represented as the formula (BauSryCawCux)3−y(Zn,Mg,Mn)zSi1+bO5+2b:Eua. The non-stoichiometric tetragonal silicat e is prepared in a high temperature solid state reaction with a surplus of silica in the starting mixture. Furthermore, luminescent tetragonal Copper Alkaline Earth Silicates are provided for LED applications, which have a high color temperature range from about 2,000K to 8,000K or 10,000 K showing a CRI with Ra=80˜95, when mixed with other luminescent materials.
Abstract:
Exemplary embodiments of the present invention relate to inorganic phosphors based on silicate compounds having improved stability under a resulting radiation load and resistance to atmospheric humidity, which are capable of converting higher-energy excitation radiation, i.e. ultraviolet (UV) or blue light, with high efficiency into a longer-wavelength radiation which may be in the visible spectral range. A calcium molar fraction x having a value between 0 and 0.05 is added to a silicate phosphor having the general formula Sr3-x-y-zCaxMIIySiO5:Euz.
Abstract:
The present invention refers to bisphosphonate and phosphonate/phosphate compounds of Formulae I and its use as inhibitors of aSMase enzyme activity.
Abstract:
Disclosed is a light emitting device employing non-stoichiometric tetragonal Alkaline Earth Silicate phosphors. The light emitting device comprises a light emitting diode emitting light of ultraviolet or visible light, and non-stoichiometric luminescent material disposed around the light emitting diode. The luminescent material adsorbs at least a portion of the light emitted from the light emitting diode and emits light having a different wavelength from the absorbed light. The non-stoichiometric luminescent material has tetragonal crystal structure, and contains more silicon in the crystal lattice than that in the crystal lattice of silicate phosphors having stoichiometric crystal structure. The luminescent material is represented as the formula (BauSrvCawCux)3-y(Zn,Mg,Mn)zSi1+bO5+2b:Eua. Light emitting devices having improved temperature and humidity stability can be provided by employing the non-stoichiometric tetragonal Alkaline Earth Silicate phosphors.
Abstract:
Exemplary embodiments of the present invention relate to inorganic phosphors based on silicate compounds having improved stability under a resulting radiation load and resistance to atmospheric humidity, which are capable of converting higher-energy excitation radiation, i.e. ultraviolet (UV) or blue light, with high efficiency into a longer-wavelength radiation which may be in the visible spectral range. A calcium molar fraction x having a value between 0 and 0.05 is added to a silicate phosphor having the general formula Sr3-x-y-zCaxMIIySiO5:Euz.
Abstract:
Disclosed herein is a light emitting device including one or more light emitting diodes to primarily emit light having different wavelengths in the wavelength range of ultraviolet rays and/or blue light, and a wavelength-conversion means to convert the primary light into secondary light in the visible light wavelength range. The light emitting device of the current invention has a high color temperature of 2000 to 8000 K or 10000 K and a high color rendering index of 90 or more, thus easily realizing desired emission on the color coordinate system. Therefore, the lighting emitting device is applicable to mobile phones, notebook computers, and keypads or backlight units for various electronic products, and, in particular, automobiles and exterior and interior lighting fixtures.
Abstract:
A light emitting device can include a substrate, electrodes provided on the substrate, a light emitting diode configured to emit light, the light emitting diode being provided on one of the electrodes, phosphors configured to change a wavelength of the light, and an electrically conductive device configured to connect the light emitting diode with another of the plurality of electrodes. The phosphors can substantially cove at least a portion of the light emitting diode. The phosphor may include aluminate type compounds, lead and/or copper doped silicates, lead and/or copper doped antimonates, lead and/or copper doped germanates, lead and/or copper doped germanate-silicates, lead and/or copper doped phosphates, or any combination thereof.
Abstract:
A luminous body of prolonged fluorescence lifetime characterized by comprising not only an activator but also at least one coactivator selected from the group consisting of La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Bi, Sn, Sb and analogues thereof as a further luminescent center for enhancing the thermostability of luminous body. This luminous body excels in thermostability and fluorescence lifetime, so that it is useful as a luminous body for LED.
Abstract:
This invention relates to luminescent materials for ultraviolet light or visible light excitation containing lead and/or copper doped chemical compounds. The luminescent material is composed of one or more than one compounds of aluminate type, silicate type, antimonate type, germanate/or germanate-silicate type, and/or phosphate type. Accordingly, the present invention is a good possibility to substitute earth alkaline ions by lead and copper for a shifting of the emission bands to longer or shorter wave length, respectively. Luminescent compounds containing copper and/or lead with improved luminescent properties and also with improved stability against water, humidity as well as other polar solvents are provided. The present invention is to provide lead and/or copper doped luminescent compounds, which has high color temperature range about 2,000K to 8,000K or 10,000K and CRI over 90.