摘要:
A hot-dip galvanized cold-rolled steel sheet has a tensile strength of 750 MPa or higher, a composition consisting, in mass percent, C: more than 0.10% and less than 0.25%, Si: more than 0.50% and less than 2.0%, Mn: more than 1.50% and 3.0% or less, and optionally containing one or more types of Ti, Nb, V, Cr, Mo, B, Ca, Mg, REM, and Bi, P: less than 0.050%, S: 0.010% or less, sol. Al: 0.50% or less, and N: 0.010% or less, and a main phase as a low-temperature transformation product and a second phase as retained austenite. The retained austenite volume fraction is more than 4.0% and less than 25.0% of the whole structure, and has an average grain size of less than 0.80 μm. A number density of retained austenite grains having a grain size of 1.2 μm or more is 3.0×10−2/μm2 or less.
摘要:
A method for producing a high-tensile cold-rolled steel sheet includes subjecting a slab having a composition containing C: more than 0.020% and less than 0.30%, Si: more than 0.10% and 3.00% or less, and Mn: more than 1.00% and 3.50% or less to hot rolling wherein the roll draft of the final one pass is higher than 15%, and rolling is finished in the temperature region of Ar3 point or higher, optionally annealing wherein the hot-rolled steel sheet is heated to 300° C. or higher after being cooled to 780° C. or lower, coiling higher than 400° C. or lower than 400° C., cold rolling the hot-rolled steel sheet or the annealed steel sheet, and annealing wherein the cold-rolled steel sheet is soaked in the temperature region of (Ac3 point−40° C.) or higher, cooling to 500° C. or lower and 300° C. or higher, and holding in that temperature region for 30 seconds or longer.
摘要:
A hot-dip galvanized cold-rolled steel sheet has a tensile strength of 750 MPa or higher, a composition consisting, in mass percent, of C: more than 0.10% and less than 0.25%, Si: more than 0.50% and less than 2.0%, Mn: more than 1.50% and 3.0% or less, and optionally containing one or more types of Ti, Nb, V, Cr, Mo, B, Ca, Mg, REM, and Bi, P: less than 0.050%, S: 0.010% or less, sol. Al: 0.50% or less, and N: 0.010% or less, and a main phase as a low-temperature transformation product and a second phase as retained austenite. The retained austenite volume fraction is more than 4.0% and less than 25.0% of the whole structure, and has an average grain size of less than 0.80 □m. A number density of retained austenite grains having a grain size of 1.2 □m or more is 3.0□10−2/□m2 or less.
摘要:
A steel sheet excellent in mechanical strength, workability and thermal stability and suited for use as a raw material in such fields of manufacturing automobiles, household electric appliances and machine structures and of constructing buildings, and a manufacturing method thereof are provided.The steel sheet is a hot-rolled steel sheet of carbon steel or low-alloy steel, the main phase of which is ferrite, and is characterized in that the average ferrite crystal grain diameter D (μm) at the depth of ¼ of the sheet thickness from the steel sheet surface satisfies the relations respectively defined by the formulas (1) and (2) given below and the increase rate X (μm/min) in average ferrite crystal grain diameter at 700° C. at the depth of ¼ of the sheet thickness from the steel sheet surface and said average crystal grain diameter D (μm) satisfy the relation defined by the formula (3) given below: 1.2≦D≦7 formula (1) D≦2.7+5000/(5+350·C+40·Mn)2 formula (2) D·X≦0.1 formula (3) wherein C and Mn represent the contents (in % by mass) of the respective elements in the steel.
摘要:
A steel sheet excellent in mechanical strength, workability and thermal stability and suited for use as a raw material in such fields of manufacturing automobiles, household electric appliances and machine structures and of constructing buildings, and a manufacturing method thereof are provided. The steel sheet is a hot-rolled steel sheet of carbon steel or low-alloy steel, the main phase of which is ferrite, and is characterized in that the average ferrite crystal grain diameter D (μm) at the depth of ¼ of the sheet thickness from the steel sheet surface satisfies the relations respectively defined by the formulas (1) and (2) given below and the increase rate X (μm/min) in average ferrite crystal grain diameter at 700° C. at the depth of ¼ of the sheet thickness from the steel sheet surface and said average crystal diameter D (μm) satisfy the relation defined by the formula (3) given below: 1.2≦D≦7 formula (1) D≦2.7+5000/(5+350·C+40·Mn)2 formula (2) D·X≦0.1 formula (3) wherein C and Mn represent the contents (in % by mass) of the respective elements in the steel.
摘要:
In a semiconductor device including a semiconductor element to be protected having first and second electrodes, and a protection circuit coupled between the first and second electrodes, a switch circuit is inserted between the first and second electrodes in series to the protection circuit. The switch circuit is turned ON by such a voltage that turns ON the semiconductor element.
摘要:
A semiconductor integrated circuit device includes an output transistor, an overcurrent detection circuit and overcurrent limitation circuit. The overcurrent detection circuit includes a first transistor detecting an overcurrent of the output transistor. The overcurrent limitation circuit is connected between a gate and a source of the output transistor. The overcurrent limitation circuit includes a plurality of resistance elements and a diode connected in series between the gate and the source of the output transistor in series, and a second transistor whose gate is connected to a connection point between the resistance elements and that is cascade connected to the first transistor.
摘要:
The article storage facility comprises an article transporter configured to move along a path via an article transfer location with respect to an article storage rack; an article loader for bringing articles into and taking articles out of the article storage rack, provided to the article storage rack so as to project and retract between a protruding position for article receipt that projects to an outside of the article storage rack, and a retracted position for retracting toward the article storage rack; and a protrusion and retraction operating device provided to the article transporter, for causing the article loader to protrude and retract between the protruding position and the retracted position when the article transporter is at the article transfer location.
摘要:
An article transport facility includes an article transporting mobile body configured to move along a path and having an article holder; an article support for storing an article, the article support is configured to be moved between an article transfer position and an article storage position; a lock device provided on the article support to be switchable between a locking state for locking the article support in the article storage position, and an unlocking position for releasing the locking state; and an operating device provided on the mobile body for moving the article support and switching the lock device.
摘要:
In a dead time control circuit, a delay circuit is connected to an input terminal and adapted to delay signals therethrough by a delay time corresponding to a dead time. A logic circuit has a first input connected via the delay circuit to the input terminal, a second input connected directly to the input terminal, and an output connected to an output terminal. The dead time having adjustable temperature characteristics.