Coating and method for forming the same

    公开(公告)号:US11504738B2

    公开(公告)日:2022-11-22

    申请号:US17009315

    申请日:2020-09-01

    Abstract: A coating is formed on a surface of a base material of a furnace, and includes a base layer and a sliding material layer that is formed on a surface of the base layer and contains an oxide ceramic and a compound having a layered crystal structure. The sliding material layer causes the collided ashes to be slipped and facilitates the drop off of the adhered ashes. The base material forms a heat transfer tube or a wall surface of the furnace. The coating is also applied to a coal gasification furnace, a pulverized coal fired boiler, a combustion apparatus, or a reaction apparatus containing a furnace.

    METHOD FOR PRODUCING SURFACE-MODIFIED COMPONENT

    公开(公告)号:US20200087771A1

    公开(公告)日:2020-03-19

    申请号:US15746795

    申请日:2016-06-27

    Abstract: A method for producing a surface-modified component includes: a process of forming a thermal sprayed coating on a substrate; a process of irradiating a surface of the thermal sprayed coating with a high energy beam so as to cause an entirety of the thermal sprayed coating and a part of the substrate in a thickness direction to melt and then solidify, and thereby forming a densified modified layer; a process of forming a thermal sprayed coating on the modified layer which has been formed in the latest; and a process of irradiating a surface of the thermal sprayed coating with a high energy beam so as to cause an entirety of the thermal sprayed coating and a part of the modified layer which has been formed in the latest in the thickness direction to melt and then solidify, and thereby forming a densified modified layer.

    SURFACE TREATMENT METHOD
    10.
    发明申请

    公开(公告)号:US20220281033A1

    公开(公告)日:2022-09-08

    申请号:US17637790

    申请日:2020-08-20

    Abstract: A surface treatment method is for processing a surface of a substrate. The method includes irradiating a surface having unevenness with a laser beam satisfying all of the three following requirements: a power density in a range with a radius of 25 μm from a center of a laser beam spot is 1.0×103 to 1.0×105 kW/cm2; a power density of an entire laser beam spot is 0.08 to 0.12 times the power density in the range with the radius of 25 μm from the center of the laser beam spot; and an action time in the range with the radius of 25 μm from the center of the laser beam spot is 1.7×10-6 to 1.0×10-5 seconds. The method leaves a certain roughness on the surface of the substrate while removing fine and sharp protrusions on the surface.