Abstract:
Provided are a toughness modifier for a curable resin which has good dispersibility in a curable resin containing a thermoplastic resin as well as in a cured product formed from a curable resin composition, and also has an excellent toughness-improving effect; and a curable resin composition containing the toughness modifier. The toughness modifier for a curable resin (D) is obtained by emulsion-polymerizing 5 to 50% by mass of a vinyl monomer (B) in the presence of 50 to 95% by mass of a rubber polymer (A) latex (calculated as the rubber polymer component) using 0.5 to 15 parts by mass of a nonionic reactive surfactant (C) (relative to 100 parts by mass of a total of (A) and (B)).
Abstract:
A resin composition including 40 parts by weight or more and less than 95 parts by weight of a polycarbonate resin and 5 parts by weight or more and less than 60 parts by weight of a polyester-polyether copolymer as a base resin, wherein the polyester-polyether copolymer is a copolymer which is obtained by a polymerization using a germanium compound catalyst, includes aromatic polyester units and modified polyether units represented by the following general formula 1, and has an IV value within a range of 0.30 to 1.00 can be well-balanced in moldability, heat resistance, impact resistance, and low linear expansion property, without deteriorating a surface appearance of a molding obtained therefrom.
Abstract:
An object is to obtain a flame-retardant polyester-based resin composition that uses no halogen-based flame retardant, has high flame retardance, and is excellent in strength retention after long-term heat resistance test under high temperature. The flame-retardant polyester-based resin composition according to the present invention contains 100 parts by weight of a thermoplastic polyester-based resin (A), 5 to 80 parts by weight of an organophosphorus-based flame retardant (B) represented by the following general formula 1, and 1 to 20 parts by weight of at least one amorphous thermoplastic resin (C) selected from the group consisting of a polyetherimide resin, a polysulfone-based resin, and a polyarylate resin. (wherein n is an integer of 2 to 40)
Abstract:
Provided are a toughness modifier for a curable resin which has good dispersibility in a curable resin containing a thermoplastic resin as well as in a cured product formed from a curable resin composition, and also has an excellent toughness-improving effect; and a curable resin composition containing the toughness modifier. The toughness modifier for a curable resin (D) is obtained by emulsion-polymerizing 5 to 50% by mass of a vinyl monomer (B) in the presence of 50 to 95% by mass of a rubber polymer (A) latex (calculated as the rubber polymer component) using 0.5 to 15 parts by mass of a nonionic reactive surfactant (C) (relative to 100 parts by mass of a total of (A) and (B)).
Abstract:
A resin composition including 40 parts by weight or more and less than 95 parts by weight of a polycarbonate resin and 5 parts by weight or more and less than 60 parts by weight of a polyester-polyether copolymer as a base resin, wherein the polyester-polyether copolymer is a copolymer which is obtained by a polymerization using a germanium compound catalyst, includes aromatic polyester units and modified polyether units represented by the following general formula 1, and has an IV value within a range of 0.30 to 1.00 can be well-balanced in moldability, heat resistance, impact resistance, and low linear expansion property, without deteriorating a surface appearance of a molding obtained therefrom.