Wet friction material
    2.
    发明授权
    Wet friction material 有权
    湿摩擦材料

    公开(公告)号:US06265066B1

    公开(公告)日:2001-07-24

    申请号:US09441065

    申请日:1999-11-16

    IPC分类号: C08J514

    摘要: A wet friction material contains a fibrous base, a filler, a friction adjuster and a binder. The binder contains a material having siloxane bond. For example, the binder is a product of hardening of a hydrolytic solution of a silicon alkoxide.

    摘要翻译: 湿摩擦材料包含纤维基材,填料,摩擦调节剂和粘合剂。 粘合剂含有具有硅氧烷键的材料。 例如,粘合剂是使硅醇盐的水解溶液硬化的产物。

    Wet friction material
    3.
    发明申请
    Wet friction material 失效
    湿摩擦材料

    公开(公告)号:US20060223907A1

    公开(公告)日:2006-10-05

    申请号:US11388094

    申请日:2006-03-24

    IPC分类号: C08J5/14

    摘要: The invention provides a wet friction material having high friction coefficient, excellent compression fatigue property and positive gradient of a μ-V property. The wet friction material contains a paper base material and a binder, in which the binder contains a cured material of a liquid resin composition obtained by mixing a hydrolyzed solution of a silane coupling agent represented by the following formula (1) and a resol-type phenol resin, and a weight ratio (S/R) between respective non-volatile components of the hydrolyzed solution (S) of the silane coupling agent and the resol-type phenol resin (R) is in the range of from 80/20 to 20/80: (X)(R1)nSi(OR2)3-n (1), in which X represents an alkylamino group having a primary amine at a terminal; R1 and R2 each independently represent an alkyl group having from 1 to 3 carbon atoms; and n represents an integer of 0 or 1.

    摘要翻译: 本发明提供具有高摩擦系数,优异的压缩疲劳特性和μ-V特性的正梯度的湿摩擦材料。 湿摩擦材料包含纸基材料和粘合剂,其中粘合剂含有通过将下式(1)表示的硅烷偶联剂的水解溶液与甲阶酚醛树脂型 酚醛树脂,硅烷偶联剂和甲阶酚醛树脂型酚醛树脂(R)的水解溶液(S)的各非挥发成分的重量比(S / R)为80/20〜 20/80:(X)(R 1)N 2 Si(OR 2)3-n(1) ),其中X表示末端具有伯胺的烷基氨基; R 1和R 2各自独立地表示具有1至3个碳原子的烷基; n表示0或1的整数。

    Wet friction material
    4.
    发明授权
    Wet friction material 有权
    湿摩擦材料

    公开(公告)号:US06667103B1

    公开(公告)日:2003-12-23

    申请号:US09570015

    申请日:2000-05-12

    IPC分类号: B32B904

    摘要: There is provided a wet friction material excellent in heat resistance and durability, high in friction coefficient, small in initial fluctuation of the friction coefficient, excellent in heat spot resistance and superior in physical strength to a wet friction material using a phenol resin as a binder. In the wet friction material composed of a fiber base material, a filler, a friction adjustor, and a binder, the binder is a hardened substance of a hydrolyzed solution of a silane coupling agent represented by the following formula (1) (R1)(R2)nSi(OR3)3−n  (1) in which R1 represents an alkylamino group containing primary amine at a terminal, each of R2 and R3 represents an alkyl group containing 1 to 3 carbon atoms, and n represents an integer of 0 or 1.

    摘要翻译: 提供耐热性和耐久性优异的摩擦系数,摩擦系数的初始波动小,耐热斑性优异,并且使用酚醛树脂作为粘合剂的湿摩擦材料的物理强度优异的湿摩擦材料 。 在由纤维基材,填料,摩擦调节剂和粘合剂构成的湿式摩擦材料中,粘合剂是由下式(1)表示的硅烷偶联剂的水解溶液的硬化物质,其中R < 1>表示在末端含有伯胺的烷基氨基,R 2和R 3各自表示含有1〜3个碳原子的烷基,n表示0或1的整数。

    Wet friction material
    5.
    发明授权
    Wet friction material 失效
    湿摩擦材料

    公开(公告)号:US07491664B2

    公开(公告)日:2009-02-17

    申请号:US11388094

    申请日:2006-03-24

    IPC分类号: B32B5/02 B32B9/00

    摘要: The invention provides a wet friction material having high friction coefficient, excellent compression fatigue property and positive gradient of a μ-V property. The wet friction material contains a paper base material and a binder, in which the binder contains a cured material of a liquid resin composition obtained by mixing a hydrolyzed solution of a silane coupling agent represented by the following formula (1) and a resol-type phenol resin, and a weight ratio (S/R) between respective non-volatile components of the hydrolyzed solution (S) of the silane coupling agent and the resol-type phenol resin (R) is in the range of from 80/20 to 20/80: (X)(R1)nSi(OR2)3−n (1), in which X represents an alkylamino group having a primary amine at a terminal; R1 and R2 each independently represent an alkyl group having from 1 to 3 carbon atoms; and n represents an integer of 0 or 1.

    摘要翻译: 本发明提供具有高摩擦系数,优异的压缩疲劳特性和μ-V特性的正梯度的湿摩擦材料。 湿摩擦材料包含纸基材料和粘合剂,其中粘合剂含有通过将下式(1)表示的硅烷偶联剂的水解溶液与甲阶酚醛树脂型 酚醛树脂,硅烷偶联剂和甲阶酚醛树脂型酚醛树脂(R)的水解溶液(S)的各非挥发成分的重量比(S / R)为80/20〜 20/80:(X)(R1)nSi(OR2)3-n(1),其中X表示在末端具有伯胺的烷基氨基; R 1和R 2各自独立地表示具有1至3个碳原子的烷基; n表示0或1的整数。

    Wet friction material
    6.
    发明授权
    Wet friction material 失效
    湿摩擦材料

    公开(公告)号:US06231977B1

    公开(公告)日:2001-05-15

    申请号:US09376364

    申请日:1999-08-18

    IPC分类号: C08J514

    摘要: A wet friction material with small initial variations in friction coefficient, suppressing occurrence of heat spots, and with excellent heat resistance and friction resistance is provided. In the wet friction material including a fiber base material, a filler, a friction controller, and a resin binder, the resin binder is a phenolic resin modified with p-nonyl phenol.

    摘要翻译: 提供摩擦系数初始变化小,抑制热斑发生,耐热性和耐摩擦性优异的湿摩擦材料。 在包括纤维基材,填料,摩擦控制器和树脂粘合剂的湿摩擦材料中,树脂粘合剂是用对壬基苯酚改性的酚醛树脂。

    Process for producing resin composition
    9.
    发明授权
    Process for producing resin composition 有权
    树脂组合物的制造方法

    公开(公告)号:US08481620B2

    公开(公告)日:2013-07-09

    申请号:US13125730

    申请日:2009-10-22

    摘要: A method for producing a resin composition, including the steps of melt-kneading a raw material A containing a polylactic acid resin, a crystal nucleating agent, and a plasticizer containing an ester compound formed between a polycarboxylic acid having a hydrocarbon group having 1 to 7 carbon atoms and a mono-alcohol having a hydrocarbon group having 1 to 7 carbon atoms, to prepare a polylactic acid-containing melt-kneaded mixture having a relative crystallinity of 70% or more (step A); and further melt-kneading the polylactic acid-containing melt-kneaded mixture obtained by the step A and a raw material B containing a polypropylene resin and a compatibilizing agent (step B). The resin composition obtainable by the method of the present invention can be suitably used in various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.

    摘要翻译: 一种树脂组合物的制造方法,其特征在于,包括将含有聚乳酸树脂的原料A,结晶成核剂和含有具有1〜7个烃基的多元羧酸形成的含有酯化合物的增塑剂进行熔融混炼的工序 碳原子和具有1〜7个碳原子的烃基的单醇制备相对结晶度为70%以上的聚乳酸熔融混炼物(步骤A)。 进一步将通过工序A得到的含聚乳酸的熔融混炼混合物和含有聚丙烯树脂和相容剂的原料B进行熔融捏合(工序B)。 通过本发明的方法得到的树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。

    Image forming apparatus including a blower member and a heating device
    10.
    发明授权
    Image forming apparatus including a blower member and a heating device 有权
    图像形成装置,包括鼓风机构件和加热装置

    公开(公告)号:US08396382B2

    公开(公告)日:2013-03-12

    申请号:US12905768

    申请日:2010-10-15

    IPC分类号: G03G15/00 G03G21/20

    CPC分类号: G03G15/6573 G03G2221/1645

    摘要: An image forming apparatus includes: a heating device that heats images that have been formed on a sheet-like recording medium to thereby fix the images to the recording medium; an ejection member that rotates in a forward direction and ejects to the outside the recording medium that has been conveyed from the heating device; a blower member that blows air onto the recording medium conveyed between the heating device and the ejection member; and a controller that controls the blower member such that the blower member operates when a recording page count where images are continuously formed on the recording medium is equal to or greater than a predetermined recording page count.