摘要:
The present invention relates to rubber compounds containing polymeric bis-succinimide polysulfides of the formula: wherein R is selected from the group consisting of phenylene and xylylene; R1 is selected from the group consisting hydrogen and alkyls having from 1 to 18 carbon atoms; x is an integer of from 2 to 8 and y is an integer of from 2 to 10.
摘要:
This invention relates to the discovery that the combination of a bismaleimide compound and a bis benzothiazolyldithio end capped compound provides for excellent vulcanization of rubbers and results in desirable reversion resistant rubbers properties.
摘要:
This invention relates to the discovery that the combination of a bismaleimide compound and a bis benzothiazolyldithio end capped compound provides for excellent vulcanization of rubbers and results in desirable reversion resistant rubbers properties.
摘要:
The present invention relates to rubber compounds containing polymeric bis-succinimide polysulfides of the formula: ##STR1## wherein R is selected from the group consisting of phenylene and xylylene; R.sup.1 is selected from the group consisting hydrogen and alkyls having from 1 to 18 carbon atoms; x is an integer of from 2 to 8 and y is an integer of from 2 to 10.
摘要:
A method for processing an elastomer comprising mixing 100 parts by weight of an elastomer having olefinic unsaturation with from 0.05 to 10 phr of a hydrated zinc-sodium thiosulfate. The hydrated zinc-sodium thiosulfate may be used in place of in whole or in part for conventional adhesion promoting cobalt compounds.
摘要:
This invention discloses a process for manufacturing an elastomeric article by liquid injection molding, said process comprising the steps of: (I) heating a curable composition comprised of (1) a liquid polymer comprised of repeat units that are derived from a conjugated diolefin monomer, wherein said liquid polymer has a weight average molecular weight which is within the range of 5,000 to 100,000, and wherein the liquid polymer is functionalized with an amine moiety, (2) a carbonyl inhibited platinum catalyst, and (3) a tetrakis(dialkyl siloxy) silane crosslinking agent, to a temperature which is within the range of 30° C. to 100° C.; (II) injecting the heated curable composition into a mold at a temperature which is within the range of 100° C. to 210° C. to produce the elastomeric article; and (III) removing the elastomeric article from the mold.
摘要:
This invention discloses a process for manufacturing an elastomeric article by liquid injection molding, wherein the article has improved tensile strength and improved tear strength, said process comprising the steps of: (I) heating a curable composition comprised of (1) a liquid polymer comprised of repeat units that are derived from a conjugated diolefin monomer, wherein said liquid polymer has a weight average molecular weight which is within the range of 5,000 to 100,000, and wherein the liquid polymer is functionalized with an ether moiety, (2) a carbonyl inhibited platinum catalyst, and (3) a tetrakis(dialkyl siloxy) silane crosslinking agent, to a temperature which is within the range of 30° C. to 100° C.; (II) injecting the heated curable composition into a mold at a temperature which is within the range of 100° C. to 210° C. to produce the elastomeric article; and (III) removing the elastomeric article from the mold. This invention also discloses that the elasticity of such cured elastomeric articles can be increased without reducing cure levels by incorporating a liquid C5 tackifier resin into the liquid polymer.
摘要:
This invention discloses a process for manufacturing an elastomeric article by liquid injection molding, wherein the article has improved tensile strength and improved tear strength, said process comprising the steps of: (I) heating a curable composition comprised of (1) a liquid polymer comprised of repeat units that are derived from a conjugated diolefin monomer, wherein said liquid polymer has a weight average molecular weight which is within the range of 5,000 to 100,000, and wherein the liquid polymer is functionalized with an ether moiety, (2) a carbonyl inhibited platinum catalyst, and (3) a tetrakis(dialkyl siloxy) silane crosslinking agent, to a temperature which is within the range of 30° C. to 100° C.; (II) injecting the heated curable composition into a mold at a temperature which is within the range of 100° C. to 210° C. to produce the elastomeric article; and (III) removing the elastomeric article from the mold. This invention also discloses that the elasticity of such cured elastomeric articles can be increased without reducing cure levels by incorporating a liquid C5 tackifier resin into the liquid polymer.