The present invention relates to a pneumatic tire with a built-in sealant layer comprised of a depolymerized butyl rubber based sealant precursor. The butyl rubber of the built-in sealant precursor composition is depolymerized in situ within the tire with an activated free radical generating organoperoxide. The organoperoxide is activated with a 2,2,6,6-tetra alkyl piperidine hindered amine. Representative of such hindered amines are, for example, a poly[[6-[1,1,3,3,-tetramethylbutyl)amino]-s-triazine-2,4-diyl][2,2,6,6,-tetramethyl-4-piperidyl)imino]hexamethylene[(2,2,6,6-tetramethyl-4-piperidyl)imino]] compound. The sealant layer, if desired, may be of a color which contrasts with black. For such purpose the sealant layer may contain a colorant of a non-black color to a substantial exclusion of carbon black. The butyl rubber-based sealant precursor is built into the tire as a layer to form a tire assembly wherein the butyl rubber-based composite portion of the sealant precursor layer is at least partially depolymerized by a said activated organoperoxide during a subsequent curing of the tire at an elevated temperature in a suitable mold to form the tire having the resultant built-in sealant layer. The sealant composition may additionally contain conventional clay, exfoliated intercalated clay platelets and/or calcium carbonate.
摘要:
A method of producing a tire including mixing in a non-productive phase at least one elastomer with a polyamide having a melting temperature of less than 180° C. The polyamide is allowed to heat to at least its melting temperature. During the productive phase, at least one curing agent is added to the elastomeric composition. The curing agent may be a sulfur containing curing agent and/or a non-sulfur containing curing agent. The elastomeric composition may optionally include a crystalline EPDM elastomer. The resulting compositions may then be formed into a tire component which may be built into a tire and cured.
摘要:
A retreaded tire comprised of a tread and carcass with an intervening rubber layer, conventionally referred to as a cushion, wherein the tread has an oil rich rubber-based adhesive on its inner surface at the interface between said tread and cushion. Said oil rich rubber based adhesive is free, or substantially free, of volatile organic compounds, particularly volatile organic solvents. Alternately, the oil-rich rubber-based adhesive may contain oil and volatile organic solvent wherein oil is the major component insofar as the oil and solvent is concerned.
摘要:
A method is disclosed for processing a rubber composition comprising thermomechanically mixing at a rubber temperature in a range of 140.degree. C. to 190.degree. C. for a mixing time of 1 to 20 minutes (i) 100 parts by weight of at least one sulfur vulcanizable elastomer selected from conjugated diene homopolymers and copolymers, natural rubber and copolymers of at least one conjugated diene and aromatic vinyl compound; (ii) 10 to 250 phr of particulate precipitated silica; (iii) 0.01 to 1.0 parts by weight per weight of said silica of an organosilicon compound; and (iv) 0.05 to 10 phr of sodium thiosulfate pentahydrate. Addition of the sodium thiosulfate pentahydrate to sulfur vulcanizable rubber, silica and sulfur containing organosilicon compound decreases the mixing/processing time without sacrificing end product properties.
摘要:
The present invention is directed to a tire retread cushion laminate, comprising a first rubber layer, a second rubber layer, and an intermediate rubber layer disposed between the first and second rubber layers such that the first and second rubber layers do not meet; the first rubber layer comprising a sulfur donor and substantially devoid of vulcanization accelerators; the second rubber layer comprising a vulcanization accelerator and substantially devoid of sulfur donors; the intermediate rubber layer being substantially devoid of sulfur donors or vulcanization accelerators.
摘要:
An improved method of bonding at least two cured or uncured elastomeric layers is disclosed. The method comprising placing an uncured elastomeric component (22) between the two elastomeric layers, and curing the elastomeric component to bond the elastomeric layers together. The improvement is characterized by forming the uncured elastomeric component (22) by preparing two non-productive elastomer compounds (10, 12), wherein each non-productive compound (10 or 12) is prepared with a co-reacting agent of a co-reacting cure package not added to the other non-productive compound (12 or 10), and layering the non-productive elastomer compounds (10, 12) in alternating layers with a thickness relative to the diffusion rate of the co-reacting agents in each non-productive elastomeric layer (10, 12) to effect diffusion of the co-reacting cure agents through the adjacent layers.
摘要:
A method is disclosed for increasing the rate of vulcanization of a sulfur rubber composition comprising heating a sulfur vulcanizable rubber composition to a temperature ranging from 100.degree. C. to 200.degree. C., said rubber composition, containing a sulfur vulcanizable rubber, a sulfenamide compound and a hydrated thiosulfate. Addition of the hydrated thiosulfate to a sulfur vulcanizable rubber and a sulfenamide compound significantly increases the rate of vulcanization of the rubber.
摘要:
A method of forming a tread comprising two or more layers of rubber is described. The method includes the steps of: extruding a rubber compound through an extruder and a gear pump and mixing with an accelerant and then applying a continuous strip of rubber directly onto a tire building machine to form a first layer of rubber having a first cure rate; adjusting the amount of accelerant to obtain a second cure rate different than said first cure rate, and then applying a strip of rubber having a second cure rate onto the tire building machine, wherein one of the cure rates is faster than the other cure rate.
摘要:
A method of forming a tread comprising two or more layers of rubber is described. The method includes the steps of: extruding a rubber compound through an extruder and a gear pump and mixing with an accelerant and then applying a continuous strip of rubber directly onto a tire building machine to form a first layer of rubber having a first cure rate; adjusting the amount of accelerant to obtain a second cure rate different than said first cure rate, and then applying a strip of rubber having a second cure rate onto the tire building machine, wherein one of the cure rates is faster than the other cure rate.