HOT FORMING TOOL
    92.
    发明申请
    HOT FORMING TOOL 审中-公开

    公开(公告)号:US20170333964A1

    公开(公告)日:2017-11-23

    申请号:US15519988

    申请日:2015-11-04

    申请人: Hua Guo

    发明人: Hua Guo

    IPC分类号: B21B25/00 B21B19/04

    CPC分类号: B21B25/00 B21B19/04

    摘要: Disclosed is a hot forming tool (1) which consists of a main tool member (2) having an at least partial surface coating (4) and which can be obtained by providing the main tool member with a raised metal relief that is then entirely or partly oxidized and converted into a protective layer.

    Poly(phenylene ether) copolymer and method of making
    94.
    发明授权
    Poly(phenylene ether) copolymer and method of making 有权
    聚(苯醚)共聚物及其制备方法

    公开(公告)号:US09018342B2

    公开(公告)日:2015-04-28

    申请号:US13881480

    申请日:2012-07-27

    摘要: A poly(phenylene ether) copolymer comprises about 5 to 40 mole percent repeat units derived from 2-phenylphenol and 60 to about 95 mole percent repeat units derived from 2,6-dimethylphenol, wherein the poly(phenylene ether) copolymer has a weight average molecular weight of at least 8,000 atomic mass units, as measured by gel permeation chromatography. A method of preparing the poly(phenylene ether) copolymer, comprises oxidatively copolymerizing a monomer mixture comprising about 5 to 40 mole percent 2-phenylphenol and about 60 to about 95 mole percent 2,6-dimethylphenol in the presence of a solvent, molecular oxygen, and a polymerization catalyst comprising a metal ion and at least one amine ligand to form a solution of the poly(phenylene ether) copolymer in the solvent, wherein a ratio of total moles of 2-phenylphenol and 2,6-dimethylphenol to moles of metal ion is about 10:1 to about 1200:1.

    摘要翻译: 聚(苯醚)共聚物包含约5-40摩尔%的衍生自2-苯基苯酚的重复单元和60-约95摩尔%的衍生自2,6-二甲基苯酚的重复单元,其中聚(苯醚)共聚物具有重均分子量 通过凝胶渗透色谱法测量的至少8,000个原子质量单位的分子量。 制备聚(苯醚)共聚物的方法包括在溶剂存在下氧化共聚包含约5至40摩尔%的2-苯基苯酚和约60至约95摩尔%的2,6-二甲基苯酚的单体混合物,分子氧 ,以及包含金属离子和至少一种胺配体的聚合催化剂,以在溶剂中形成聚(苯醚)共聚物的溶液,其中2-苯基苯酚和2,6-二甲基苯酚的总摩尔数与摩尔数 金属离子为约10:1至约1200:1。

    Poly(phenylene ether) process
    95.
    发明授权
    Poly(phenylene ether) process 有权
    聚(苯醚)工艺

    公开(公告)号:US08859646B2

    公开(公告)日:2014-10-14

    申请号:US13417451

    申请日:2012-03-12

    IPC分类号: C08F6/08 C08G65/38

    CPC分类号: C08G65/46

    摘要: A method of purifying a poly(phenylene ether) is described. The method includes mixing a poly(phenylene ether) solution comprising a poly(phenylene ether) and a poly(phenylene ether) solvent with first washing solvents including a C1-C4 alkanol and water to form a first liquid phase including poly(phenylene ether) and poly(phenylene ether) solvent, and a second liquid phase comprising C1-C4 alkanol and water, and separating the first liquid phase from the second liquid phase. The first and second liquid phases combined comprise about 60 to about 95 weight percent poly(phenylene ether) solvent, about 4 to about 32 weight percent C1-C4 alkanol, and about 1 to about 36 weight percent water. When optionally combined with evaporative removal of the poly(phenylene ether) solvent, the method reduces C1-C4 alkanol usage compared to the antisolvent precipitation method, and it produces poly(phenylene ether) having reduced catalyst metal ion residue and reduced color.

    摘要翻译: 描述了一种纯化聚(苯醚)的方法。 该方法包括将包含聚(苯醚)和聚(苯醚)溶剂的聚(苯醚)溶液与包含C1-C4链烷醇和水的第一洗涤溶剂混合以形成包含聚(苯醚) 和聚(苯醚)溶剂,以及包含C 1 -C 4链烷醇和水的第二液相,并且将第一液相与第二液相分离。 组合的第一和第二液相包含约60至约95重量%的聚(苯醚)溶剂,约4至约32重量%的C 1 -C 4链烷醇和约1至约36重量%的水。 当与蒸馏除去聚(苯醚)溶剂相结合时,与反溶剂沉淀法相比,该方法降低了C1-C4链烷醇的用量,并且产生具有降低的催化剂金属离子残余物和降低颜色的聚苯醚。

    Process for formation of poly(arylene ethers) with lower fine particle content
    96.
    发明授权
    Process for formation of poly(arylene ethers) with lower fine particle content 有权
    形成具有较低微粒含量的聚(亚芳基醚)的方法

    公开(公告)号:US08779081B2

    公开(公告)日:2014-07-15

    申请号:US13048225

    申请日:2011-03-15

    IPC分类号: C08G63/18

    摘要: The invention is directed to a method for producing poly(arylene) ethers with improved particle size characteristics. The improved particle size characteristics of the polyphenylene ether include one or both of: (i) up to about 50 weight percent of particles smaller than 38 micrometers; and a (ii) mean particle size greater than 100 or more micrometers.

    摘要翻译: 本发明涉及一种具有改进粒度特性的聚(亚芳基)醚的制备方法。 聚苯醚的改进的粒度特性包括以下之一或两者:(i)至多约50重量%的小于38微米的颗粒; 和(ii)平均粒度大于100微米或更大。

    STEEL RAIL FOR HIGH SPEED AND QUASI-HIGH SPEED RAILWAYS AND METHOD OF MANUFACTURING THE SAME
    98.
    发明申请
    STEEL RAIL FOR HIGH SPEED AND QUASI-HIGH SPEED RAILWAYS AND METHOD OF MANUFACTURING THE SAME 审中-公开
    用于高速和高速铁路的钢轨及其制造方法

    公开(公告)号:US20130193223A1

    公开(公告)日:2013-08-01

    申请号:US13820493

    申请日:2011-09-02

    IPC分类号: E01B5/02

    摘要: The present discloses a steel rail for high speed and quasi-high speed railways and a manufacturing method thereof. The steel rail having a superior rolling contact fatigue property can be obtained by reducing content of carbon in conjunction with controlled cooling after rolling. The steel rail includes 0.40-0.64% by weight of C, 0.10-1.00% by weight of Si, 0.30-1.50% by weight of Mn, less than or equal to 0.025% by weight of P, less than or equal to 0.025% by weight of S, less than or equal to 0.005% by weight of Al, more than 0 and less than or equal to 0.05% by weight of a rare earth element, more than 0 and less than or equal to 0.20% by weight of at least one of V, Cr, and Ti, and a remainder of Fe and inevitable impurities. The steel rail manufactured according to the method of the present invention maintains the strength and hardness of the existing steel rail for the high speed railways, while enhancing the toughness, plasticity and yield strength, and an energy value required for initiating and expanding microcracks formed at the surface of the steel rail due to fatigue is increased, and thus under the same conditions, the rolling contact fatigue property of the steel rail can be improved, thereby finally improving the service lifetime and the transportation safety of the steel rail.

    摘要翻译: 本发明公开了一种用于高速和准高速铁路的钢轨及其制造方法。 具有优异的滚动疲劳性能的钢轨可以通过在轧制后与可控制的冷却相结合地减少碳含量来获得。 钢轨包含0.40-0.64重量%的C,0.10-1.00重量%的Si,0.30-1.50重量%的Mn,小于或等于0.025重量%的P,小于或等于0.025重量% 的S,小于或等于0.005重量%的Al,大于0和小于或等于0.05重量%的稀土元素,大于0重量%且小于等于0.20重量% V,Cr和Ti中的至少一种,剩余的Fe和不可避免的杂质。 根据本发明的方法制造的钢轨在提高韧性,塑性和屈服强度的同时保持现有的高速铁路钢轨的强度和硬度,以及形成的微裂纹所需的能量值 钢轨的疲劳表面增加,因此在相同条件下,能够提高钢轨的滚动疲劳特性,从而最终提高钢轨的使用寿命和运输安全性。

    Morpholine-substituted poly(arylene ether) and method for the preparation thereof
    99.
    发明授权
    Morpholine-substituted poly(arylene ether) and method for the preparation thereof 有权
    吗啉取代的聚(亚芳基醚)及其制备方法

    公开(公告)号:US08124717B2

    公开(公告)日:2012-02-28

    申请号:US13083696

    申请日:2011-04-11

    IPC分类号: C08G65/38 C08G2/00

    CPC分类号: C08G65/46

    摘要: A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.

    摘要翻译: 使用含吗啉的聚合催化剂制备的聚(2,6-二甲基-1,4-亚苯基醚)具有单分子分子量分布,具有非常高的分子量物质含量降低。 它还表现出高分子量级分中增加的吗啉掺入。 与使用含有二正丁胺的聚合催化剂制备的市售聚(2,6-二甲基-1,4-亚苯基醚)相比,聚(2,6-二甲基-1,4-亚苯基醚) 发明显示减少的气味。 与使用含吗啉的聚合催化剂制备的其它聚(2,6-二甲基-1,4-亚苯基醚)相比,本发明的聚(2,6-二甲基-1,4-亚苯基醚)表现出改善的分子量 在复合期间建立并改善与聚酰胺的相容性。