摘要:
An anodized layer formation method includes: providing an aluminum film provided on a support or an aluminum base; and forming a porous alumina layer which has minute recessed portions by applying a voltage between an anode which is electrically coupled to a surface of the aluminum film or the aluminum base and a cathode which is provided in an electrolytic solution with the surface of the aluminum film or the aluminum base being in contact with the electrolytic solution. The forming of the porous alumina layer includes increasing the voltage to a target value and, before the voltage is increased to the target value, increasing the voltage to a first peak value which is lower than the target value and thereafter decreasing the voltage to a value which is lower than the first peak value. As such, an anodized layer with reduced variation of recessed portions can be formed.
摘要:
An anodized layer formation method of an embodiment of the present invention includes the step a of providing an aluminum film which is formed on a first principal surface of a support and the step b of anodizing a surface of the aluminum film to form a porous alumina layer which has a plurality of minute recessed portions. In the step a, a second principal surface of the support which is opposite to the first principal surface is provided with a low heat conduction member that has a predetermined pattern. According to an embodiment of the present invention, a porous alumina layer can be formed which includes regions of different minute structures in the predetermined pattern.
摘要:
A mold is disclosed, which is capable of producing a nanoimprint film without a problem of clogging of irregularities of the mold with a resin material. A method for producing the mold and a method for producing a nanoimprint film using the mold are further disclosed. In an embodiment, the mold includes: a first surface having a nanostructure including plural recesses spaced at an interval of less than 1 μm between bottom points of adjacent recesses; and at least two second surfaces substantially not having the nanostructure, wherein the first surface is coplanar with the at least two second surfaces and is positioned between two second surfaces.
摘要:
A method is provided for manufacturing a mold that has a porous alumina layer over its surface, which is capable of preventing formation of pits (recesses). A moth-eye mold manufacturing method of an embodiment of the present invention is a method for manufacturing a mold which has a porous alumina layer over its surface, including the steps of: providing a mold base which includes an aluminum base and an aluminum film deposited on a surface of the aluminum base, the aluminum film having a purity of not less than 99.99 mass %; anodizing a surface of the aluminum film to form a porous alumina layer which has a plurality of minute recessed portions; and bringing the porous alumina layer into contact with an etching solution to enlarge the plurality of minute recessed portions of the porous alumina layer.
摘要:
An electrode structure of the present invention includes: an aluminum electrode which is to be in contact with a surface of an aluminum base; a fixing member for fixing the aluminum electrode on the surface of the aluminum base; an elastic member provided between the fixing member and the aluminum base; a lead wire which is electrically connected to the aluminum electrode at least under a certain condition; and a cover member which is tightly closed with the lead wire penetrating through an opening.
摘要:
A mold of the present invention includes: a base 12 made of glass or plastic; an inorganic underlayer 14 provided on a surface of the base 12; a buffer layer 16 provided on the inorganic underlayer 14, the buffer layer 16 containing aluminum; an aluminum layer 18a provided on a surface of the buffer layer 16; and a porous alumina layer 20 provided on a surface of the aluminum layer 18a. The porous alumina layer 20 has a plurality of recessed portions 22 whose two-dimensional size viewed in a direction normal to the surface is not less than 10 nm and less than 500 nm. The mold of the present invention has excellent adhesion between the aluminum layer and the base.
摘要:
One of the objects of the present invention is to provide a method for readily manufacturing a seamless mold in the form of a roll which has a porous alumina layer over its surface. The mold manufacturing method of the present invention is a method for manufacturing a mold which has a porous alumina layer over its surface, including the steps of: providing a hollow cylindrical support; forming an insulating layer on an outer perimeter surface of the hollow cylindrical support; depositing aluminum on the insulating layer to form an aluminum film; and anodizing a surface of the aluminum film to form a porous alumina layer which has a plurality of minute recessed portions.
摘要:
A method for manufacturing a moth-eye mold of an embodiment of the present invention employs a mold base including a metal base, an organic insulating layer provided on the metal base, and an aluminum alloy layer provided on the organic insulating layer, the aluminum alloy layer containing aluminum and a non-aluminum metal element M, an absolute value of a difference between a standard electrode potential of the metal element M and a standard electrode potential of aluminum being not more than 0.64 V, and a content of the metal element M in the aluminum alloy layer not exceeding 10 mass %.
摘要:
A moth-eye mold fabrication method includes: (a) providing an aluminum film deposited on a base, the aluminum film having a thickness of not less than 0.5 μm and not more than 5 μm, a surface of the aluminum film having a plurality of crystal grains whose average crystal grain diameter is not less than 200 nm and not more than 5 μm; (b) after step (a), anodizing the surface of the aluminum film to form a porous alumina layer which has a plurality of minute recessed portions; and (c) after step (b), bringing the porous alumina layer into contact with an etching solution, thereby enlarging the plurality of minute recessed portions of the porous alumina layer. A method of readily fabricating a mold is produced that is for manufacture of an antireflection film in which a moth-eye structure is superposed over an antiglare structure.
摘要:
A method for manufacturing a moth-eye mold of an embodiment of the present invention employs a mold base including a metal base, an organic insulating layer provided on the metal base, and an aluminum alloy layer provided on the organic insulating layer, the aluminum alloy layer containing aluminum and a non-aluminum metal element M, an absolute value of a difference between a standard electrode potential of the metal element M and a standard electrode potential of aluminum being not more than 0.64 V, and a content of the metal element M in the aluminum alloy layer not exceeding 10 mass %.