Abstract:
The present invention is directed to positively charged nanofiltration (NF) membranes comprising a substrate layer (S) based on a sulfonated polymer and a positively charged film layer (F) on top of said substrate, and to a method for their preparation. Furthermore, the present invention is directed to nanofiltration processes making use of said composite membrane.
Abstract:
A process for welding porous membranes, the process containing i) providing first and second porous membranes; ii) at least partially superimposing the first and second porous membranes to obtain an at least partial superimposition region; iii) welding the first and second porous membranes at least in a portion of the at least one superimposition region at a temperature in the range from 100 to 300° C. to obtain an at least partially welded composite of the first and second porous membranes, wherein the first and second porous membranes are made of at least one thermoplastic elastomer selected from the group consisting of a polyurethane elastomer, a polyester elastomer, a polyetherester elastomer, a polyesterester elastomer, a polyamide elastomer, a polyetheramide elastomer, a polystyrene elastomer, and an ethylene-vinyl acetate elastomer, and wherein the first and second porous membranes have pores having an average pore diameter of less than 2000 nm.
Abstract:
Process for making membranes M comprising the following steps: a) providing a dope solution D comprising at least one polymer P and at least one solvent S, b) adding at least one coagulant C to said dope solution D to coagulate said at least one polymer P from said dope solution D to obtain a membrane M, wherein said at least one solvent S comprises more than 50% by weight of at least one compound according to formula (I) (I), wherein R1 and R2 are independently C1 to C20 alkyl, R3 is selected from H or an aliphatic rest, 20 R4 is selected from H or an aliphatic rest, AO represents at least one alkylene oxide, n is a number from 0 to 100.
Abstract:
The invention relates to a method for preparing polyarylethersulfone-polyalkylene oxide block copolymers (PPC) comprising the polycondensation of a reaction mixture (RG) comprising the components: (A1) at least one aromatic dihalogen compound, (B1) at least one aromatic dihydroxyl compound, (B2) at least one polyalkylene oxide having at least two hydroxyl groups, (C) at least one aprotic polar solvent and (D) at least one metal carbonate, where the reaction mixture (RG) does not comprise any substance which forms an azeotrope with water.
Abstract:
The present invention relates to a process for the production of low-halogen-content polybiphenyl sulfone polymers, to the resultant polybiphenyl sulfone polymers, to polybiphenyl sulfone polymers having less than 400 ppm content of polymer-bonded halogen, to thermoplastic molding compositions comprising these polybiphenyl sulfone polymers, and to their use for the production of moldings, of fibers, of films, of membranes, or of foams.
Abstract:
The present invention relates to a process for the work-up of polymer solutions comprising N-methyl-2-pyrrolidone and a polymer where the polymer solution is hydrogenated with hydrogen in the presence of a hydrogenation catalyst.The present invention also relates to the product obtainable from said process, and to its use for producing, in particular, polyarylene ether products.
Abstract:
Thermoplastic molding compositions comprisingA) from 10 to 69% by weight of a thermoplastic polyester B) from 30 to 79% by weight of an aluminum oxide C) from 0.01 to 10% by weight of an organic or inorganic acid or mixture of these D) from 0 to 10% by weight of D1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN 53240, part 2), or D2) at least one highly branched or hyperbranched polyester of AxBy type, where x is at least 1.1 and y is at least 2.1, or a mixture of these E) from 0 to 50% by weight of other additives, where the entirety of the percentages by weight of components A) to E) gives 100%.
Abstract:
The present invention relates to a process for producing a shaped body by selective laser sintering of a sinter powder (SP). The sinter powder (SP) comprises at least one semicrystalline polyamide, at least one nylon-6I/6T and at least one polyaryl ether. The present invention further relates to a shaped body obtainable by the process of the invention and to the use of a polyaryl ether in a sinter powder (SP) for broadening the sintering window (WSP) of the sinter powder (SP).
Abstract:
A composition has at least one polyarylene (ether) sulfone, semi-aromatic polyamide, aluminum phosphate, and acid scavenger. The composition may further include at least one compatibilizer, fibrous or particulate filler, impact modifier, or auxiliary. The compositions can form a fiber, film, foam, or shaped article. The composition also has 20 to 80% by weight of the polyarylene (ether) sulfone. The polyarylene (ether) sulfone has at most 0.05% by weight of phenolic end groups.
Abstract:
Copolymer C comprising polyarylene ether blocks A and polyalkylene oxide blocks PAO, wherein said polyarylene ether blocks A are blocks of at least one partially sulfonated polyarylene ether.