Abstract:
The present invention relates to a polyolefin composition comprising (a) a heterophasic propylene copolymer, wherein the xylene cold soluble fraction of the heterophasic propylene copolymer has an intrinsic viscosity of lower than 2.0 dl/g, (b) a high density polyethylene having a density of at least 940 kg/m3, (c) a linear low density polyethylene, and (d) an inorganic filler, wherein the polyolefin composition has a MFR2 (230° C.) of at least 20 g/10 min.
Abstract:
Heterophasic polypropylene composition comprising (A) 45 to 70 wt % of a propylene homo- or copolymer matrix with an MFR2 in accordance with ISO 1133 (230° C., 2.16 kg load) of ≧80 g/10 min and (B) 25 to 40 wt % of an elastomeric propylene-ethylene copolymer, having an intrinsic viscosity IV (ISO 1628, with decalin as solvent) of ≧3.3 dl/g and an ethylene content of 20 to 50 wt %, (C) 0-15 wt % of an elastomeric ethylene/alpha-olefin random copolymer (D) 3-25 parts per weight of inorganic filler, the heterophasic polypropylene compositions having a total MFR2 (230° C./2.16 kg) in accordance with ISO 1133 of ≧5 g/10 min, a Charpy notched impact strength according to ISO 179/1eA at +23° C. of ≧15.0 kJ/m2, preferably ≧25.0 kJ/m2, a minimum value for the Charpy notched impact strength according to ISO 179/1eA at −20° C. of ≧7.0 kJ/m2, preferably ≧10.0 kJ/m2 and a tensile modulus according to ISO 527-3 of ≧1200 MPa; their preparation and use for producing injection moulded articles being free of flow marks.
Abstract translation:多相聚丙烯组合物,其包含(A)45至70重量%的丙烯均聚物或共聚物基体,其具有根据ISO 1133(230℃,2.16kg负荷)≥80g/ 10min的MFR 2和(B)25 至40重量%的丙烯 - 乙烯共聚物,其特性粘度IV(ISO 1628,作为溶剂的十氢化萘)为≥3.3dl/ g,乙烯含量为20〜50重量%,(C)为0〜15重量% %的弹性体乙烯/α-烯烃无规共聚物(D)3-25重量份的无机填料,根据ISO 1133的总共MFR 2(230℃/ 2.16kg)的多相聚丙烯组合物为≥5g / 10分钟,根据ISO 179 / 1eA在+ 23℃下的夏比缺口冲击强度为≥15.0kJ/ m 2,优选≥25.0kJ/ m 2,根据ISO 179 / 1eA的夏比缺口冲击强度的最小值 在-20℃,≥7.0kJ/ m 2,优选≥10.0kJ/ m 2,并且根据ISO 527-3的≧1200MPa的拉伸模量; 它们的制备和用于生产没有流痕的注塑制品。
Abstract:
Heterophasic polypropylene composition comprising (A) 45 to 70 wt % of a propylene homo- or copolymer matrix with an MFR2 in accordance with ISO 1133 (230° C., 2.16 kg load) of ≧80 g/10 min and (B) 25 to 40 wt % of an elastomeric propylene-ethylene copolymer, having an intrinsic viscosity IV (ISO 1628, with decalin as solvent) of ≧3.3 dl/g and an ethylene content of 20 to 50 wt %, (C) 0-15 wt % of an elastomeric ethylene/alpha-olefin random copolymer (D) 3-25 parts per weight of inorganic filler, the heterophasic polypropylene compositions having a total MFR2 (230° C./2.16 kg) in accordance with ISO 1133 of ≧5 g/10 min, a Charpy notched impact strength according to ISO 179/1eA at +23° C. of ≧15.0 kJ/m2, preferably ≧25.0 kJ/m2, a minimum value for the Charpy notched impact strength according to ISO 179/1eA at −20° C. of ≧7.0 kJ/m2, preferably ≧10.0 kJ/m2 and a tensile modulus according to ISO 527-3 of ≧1200 MPa; their preparation and use for producing injection moulded articles being free of flow marks.
Abstract:
Polypropylene composition comprising a polypropylene base material, a carbon fibre and an adhesion promoter with an excellent impact/stiffness balance, its preparation, articles comprising the composition and the use of the composition.
Abstract:
Polypropylene composition comprising a polypropylene base material, a carbon fibre and an adhesion promoter with an excellent impact/stiffness balance, its preparation, articles comprising the composition and the use of the composition.
Abstract:
Tiger stripe modifier being a heterophasic polypropylene composition comprising a propylene homopolymer and an elastomeric propylene copolymer, wherein said propylene homopolymer has a melt flow rate MFR2 (230° C.) in the range of above 70 to 300 g/l Omin; the xylene cold soluble fraction of the heterophasic polypropylene composition has an intrinsic viscosity in the range of more than 4.0 to below 12.0 dl/g; and the comonomer content of the xylene cold soluble fraction of the heterophasic polypropylene composition is in the range of 20.0 to 60.0 wt.-%; wherein further the heterophasic polypropylene composition fulfills the inequation (I) 0.30≧(0.241×C)−(1.14×IV) (I) wherein C is the comonomer content of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1), and IV is the intrinsic viscosity of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1).
Abstract:
Tiger stripe modifier being a heterophasic polypropylene composition having a melt flow rate MFR2 (230° C.) in the range of 0.5 to 20 g/10 min and comprises a propylene homopolymer and an elastomeric propylene copolymer, wherein said propylene homopolymer has a melt flow rate MFR2 (230° C.) in the range of above 10 to 300 g/10 min; the xylene cold soluble fraction of the heterophasic polypropylene composition has an intrinsic viscosity in the range of more than 2.5 to below 11.0 dl/g; and the comonomer content of the xylene cold soluble fraction of the heterophasic polypropylene composition is in the range of 10.0 to 25.0 wt.-%; wherein further the heterophasic polypropylene composition fulfills the inequation (I) 0.3≧(0.241×C)-(1.14×IV) (I) wherein C is the comonomer content of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1), and IV is the intrinsic viscosity of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1).
Abstract:
The invention relates to a novel polyolefin composition having a low coefficient of thermal expansion (CLTE) and having a reduced occurrence of flow marks. The novel polyolefin compositions comprise a heterophasic polypropylene composition, ethylene/1-butene elastomer and an inorganic filler.