Abstract:
The invention provides compositions, each comprising an ethylene/alpha-olefin interpolymer, which has a reduced level of a low density, low molecular weight oligomeric fraction, as indicated by an HCC value, as described herein, and reduced levels of inorganic content or lower Tm. The invention also provides processes for forming such interpolymers.
Abstract:
The invention provides compositions, each comprising an ethylene/alpha-olefin interpolymer, which has a reduced level of a low density, low molecular weight oligomeric fraction, as indicated by an HCC value, as described herein, and reduced levels of inorganic content or lower Tm. The invention also provides processes for forming such interpolymers.
Abstract:
The present application relates to a composition comprising the following components: A) at least one ethylene/alpha-olefin interpolymer; B) a peroxide; C) at least one filler selected from one or more carbon black samples, MgO, or a combination thereof; and optionally, at least one filler selected from silica, ZnO, CaCO3, Al (OH)3, Mg (OH)2, or a combination thereof; D) a calculated P content from 0.010 wt % to 0.300 wt %, based on the weight of the composition, and wherein the calculated P content is the calculated content the phosphorus element present in one or more phosphate compounds selected from Structure 1 below: O═P (OR1) (OR2) (OR3) (Structure 1), wherein R1, R2 and R3 are each, independently, selected from i) a non-aromatic hydrocarbon or ii) a non-aromatic hydrocarbon comprising at least one heteroatom, excluding P.
Abstract:
A method to determine the weight percent of an “amorphous” fraction in an olefin-based polymer composition, comprising one or more olefin-based polymers; said method comprising the following steps: a) dissolving the olefin-based polymer composition in an organic solvent to form a polymer solution; b) injecting at least a portion of the polymer solution onto a support material, and wherein the support material has a Co-crystallization Index (CI) value from 0.70 to 1.20; c) cooling the support material at a rate greater than, or equal to, 0.2C/min; d) increasing the temperature of the support material to elute the polymers of the olefin-based polymer composition; e) generating a chromatogram; f) determining the peak area of the first elution from its lower integration limit to its upper integration limit; g) calculating the “amorphous” fraction” based on the following Equation A below: wt % “amorphous” fraction=PAamorphous/PAtotal×100 (Eqn. A); wherein PAamorp=peak area of the first elution, and PAtotal#191=total peak area of the polymers of the olefin-based polymer composition.
Abstract:
A method increase of the Resolution Index (Rl) of a chromatogram generated from a polymer sample comprising at least two olefin-based polymers of different microstructures and/or at least two olefin-based polymer fractions of different microstructures. The method comprises separating the mixture on a low-porosity stationary phase and repeatedly cycling the sample-stationary phase through a series of cooling and heating stages with active eluent flow only during the cooling stages and during the last heating stage to elute the separated analytes off the column.
Abstract:
A hot melt adhesive (HMA) composition includes (A) from 1-60 wt % of a block composite compatibilizer comprising (i) a hard polymer that includes propylene, (ii) a soft polymer that includes ethylene, and (iii) a block copolymer having a soft block and a hard block, the hard block of the block copolymer having the same composition as the hard polymer of the block composite compatibilizer and the soft block of the block copolymer having the same composition as the soft polymer of the block composite compatibilizer; (B) from 1-70 wt % of a tackifier; (C) from 1-40 wt % of at least one selected from the group of a wax and an oil; and (D) Optionally, from greater than zero to 97 wt % of a polymer component that includes an ethylene-based polymer and/or a propylene-based polymer.
Abstract:
A composition includes (A) 30-95 wt % of a random or homogeneous propylene-based interpolymer having: (i) a comonomer content of at least one of C2 and C4-10 α-olefins of 7 wt % to 49 wt % based on the total weight of the propylene-based interpolymer, (ii) a density of 0.90 g/cc or less, and (iii) an MFR of 1 g/10 min or greater (230° C./2.16 kg); and (B) 5-70 wt % of a block composite nucleator comprising: (1) a first polymer that includes polypropylene; (2) a second polymer that includes an alpha-olefin based polymer, the alpha-olefin being selected from at least one of a C2 and C4-10 α-olefins, and (3) a block copolymer having a first segment and a second segment, the first segment of the block copolymer having the same composition as the first polymer in the block composite nucleator and the second segment of the block copolymer having the same composition as the second polymer of the block composite nucleator.
Abstract:
The invention provides compositions, each comprising an ethylene/alpha-olefin interpolymer, which has a reduced level of a low density, low molecular weight oligomeric fraction, as indicated by an HCC value, as described herein, and reduced levels of inorganic content or lower Tm. The invention also provides processes for forming such interpolymers.
Abstract:
Processes of polymerizing olefin monomers. The process includes reacting ethylene and optionally one or more olefin monomers in the presence of a catalyst system, wherein the catalyst system comprises: modified-hydrocarbyl methylaluminoxane having less than 50 mole percent AlRA1RB1RC1 based on the total moles of aluminum, where RA1, RB1, and RC1 are independently is linear (C1-C40)alkyl, branched (C1-C40)alkyl, or (C6-C40)aryl; and one or more metal-ligand complexes according to formula (I).
Abstract:
A packing material for chromatography, the packing material comprising coated particles, wherein the coated particles comprise non-porous particles and a portion of the surface area of the non-porous particles is coated with a coating composition comprising graphene and/or graphene oxide.