Abstract:
Embodiments are directed to polymer blends and molded articles including polymer blends. Embodiments of the polymer blend may include 1 to 40 wt. % of a crystalline block composite and from 60 wt. % to 99 wt. % of an ionomer formed from a partially neutralized precursor acid copolymer. The crystalline block composite may include an EP-iPP diblock polymer, an isotactic polypropylene homopolymer, and a copolymer of ethylene and propylene. The crystalline block composite may include greater than 50 wt. % of the isotactic polypropylene homopolymer. The precursor acid copolymer may include copolymerized units of ethylene and 5 wt. % to 30 wt. %, based on the total weight of the precursor acid copolymer, of copolymerized units of an α,β-ethylenically unsaturated carboxylic acid having 3 to 8 carbon atoms. About 25% to about 65% of the acid groups derived from the α,β-ethylenically unsaturated carboxylic acid of the precursor acid copolymer may be neutralized.
Abstract:
The present disclosure provides a plastic living hinge. The plastic living hinge includes a blend containing (A) an ethylene-based polymer; and (B) a composite component selected from the group consisting of a block composite, a crystalline block composite, and a combination thereof.
Abstract:
The invention provides functionalized block composites and crystalline block composites. In particular, the invention provides a functionalized olefin-based polymer formed from at least (A) and (B): (A) a crystalline block composite comprising: a block copolymer comprising a propylene-based crystalline block and crystalline ethylene-based block; a propylene-based crystalline polymer; and, a crystalline ethylene-based polymer; and (B) at least one functionalization agent or a functionalized olefin-based polymer formed from at least (A) and (B): (A) a crystalline block composite comprising: a block copolymer comprising a propylene-based crystalline block and crystalline ethylene-based block; a propylene-based crystalline polymer; and, a crystalline ethylene-based polymer; and (B) at least one functionalization agent.
Abstract:
Embodiments relate to a high melt flow thermoplastic polyolefin composition and of a method of preparing a high melt flow thermoplastic polyolefin composition, in which the composition includes from 5 wt % to 45 wt % of a modifier including a blend of from 5 wt % to 40 wt % of a block composite and from 60 wt % to 95 wt % of a polyolefin copolymer, based on a total weight of the modifier, and from 30 wt % to 95 wt % of a polypropylene polymer base that has a melt flow rate of at least 40 g/10 min. The high melt flow thermoplastic polyolefin composition has a blended melt flow rate of at least 25 g/10 min and an MFR ratio is less than 2.0, the MFR ratio being a ratio of the melt flow rate of the polypropylene polymer base to the blended melt flow rate of the high melt flow thermoplastic polyolefin composition.
Abstract:
A composition comprising from 10 wt % to 86 wt % of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt %, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm3 to 0.965 g/cm3; from 10 wt % to 86 wt % of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt % and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; from 2 wt % to 22 wt % of an octene component including at least one octene based polymer having an octene content of at least 80 wt %; and from 2 wt % to 20 wt % of a composite component including at least one selected from the group of a crystalline block composite and a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract:
Disclosed herein is a multilayer film comprising two outer layers; where each outer layer comprises polyethylene; two tie layers; where each tie layer comprises a crystalline block copolymer composite; where each tie layer has a first face and a second face that are opposed to each other, and where the first face of each tie layer contacts at least one outer layer; and a core layer; where the core layer comprises a polypropylene; where the second face of each tie layer contacts the core layer. Disclosed herein is a method comprising coextruding a multilayered film comprising two outer layers; where each outer layer comprises polyethylene; two tie layers; where each tie layer comprises a crystalline block copolymer composite; where each tie layer has a first face and a second face that are opposed to each other, and where the first face of each tie layer contacts at least one outer layer; and a core layer; where the core layer comprises a polypropylene; where the second face of each tie layer contacts the core layer; and coextruding the multilayered blown film.
Abstract:
The invention provides functionalized block composites and crystalline block composites. In particular, the invention provides a functionalized olefin-based polymer formed from at least (A) and (B): (A) a crystalline block composite comprising: a block copolymer comprising a propylene-based crystalline block and crystalline ethylene-based block; a propylene-based crystalline polymer; and, a crystalline ethylene-based polymer; and (B) at least one functionalization agent or a functionalized olefin-based polymer formed from at least (A) and (B): (A) a crystalline block composite comprising: a block copolymer comprising a propylene-based crystalline block and crystalline ethylene-based block; a propylene-based crystalline polymer; and, a crystalline ethylene-based polymer; and (B) at least one functionalization agent.
Abstract:
The present disclosure provides a plastic living hinge. The plastic living hinge includes a blend containing (A) an ethylene-based polymer; (B) a propylene-based polymer; and (C) a composite component selected from the group consisting of a block composite, a crystalline block composite, and a combination thereof.
Abstract:
Disclosed herein is a multilayer film comprising two outer layers; where each outer layer comprises polyethylene; two tie layers; where each tie layer comprises a crystalline block composite; where each tie layer has a first face and a second face that are opposed to each other, and where the first face of each tie layer contacts at least one outer layer; and a core layer; where the core layer comprises a polypropylene; where the second face of each tie layer contacts the core layer. Disclosed herein is a method that includes coextruding the aforementioned multilayered film.
Abstract:
A multilayer film structure comprising a top encapsulation layer A, a tie Layer B between top Layer A and bottom Layer C and a bottom layer C, the multilayer film structure characterized in that tie Layer B comprises a crystalline block composite resin or a block composite resin and bottom Layer C comprises a polyolefin having at least one melting point greater than 125° C.