Abstract:
A dianhydride and a polyimide formed by the same are provided. The dianhydride has a chemical structure represented below: wherein Ar is a fluorene-containing group. The dianhydride can be polymerized with a diamine to form a polyimide with a repeating unit of a chemical formula: wherein Ar is the fluorene-containing group, and n is a positive integer from 1 to 5. The polyimide simultaneously has excellent thermal stability and hot workability, and can therefore be applied in several industries.
Abstract:
A copolyester is formed by copolymerizing a depolymerized polyester and succinic acid. The depolymerized polyester includes depolymerized polyethylene terephthalate (PET), and the depolymerized PET is formed by depolymerizing PET with ethylene glycol. The repeating unit of PET and the succinic acid have a molar ratio of 40:60 to 50:50. The repeating unit of PET and the ethylene glycol have a molar ratio of 100:100 to 100:500. The copolyester has a storage modulus of 1*104 Pa to 1*106 Pa at 80° C. The copolyester can be used in a hot melt adhesive.
Abstract:
Liquid-crystal polymer is composed of the following repeating units: 10 mol % to 35 mol % of 10 mol % to 35 mol % of 10 mol % to 50 mol % of and 10 mol % to 40 mol % of 10 mol % to 40 mol % of or a combination thereof. Each of AR1, AR2, AR3, and AR4 is independently AR5 or AR5-Z-AR6, in which each of AR5 and AR6 is independently or a combination thereof, and Z is —O—, or C1-5 alkylene group. Each of X and Y is independently H, C1-5 alkyl group, CF3, or wherein R2 is H, CH3, CH(CH3)2, C(CH3)3, CF3, or n=1 to 4 ; and wherein R1 is C1-5 alkylene group.
Abstract:
A thin film is provided, which includes a polymer formed by reacting (a) p-hydroxybenzoic acid, (b) 6-hydroxy 2-naphthoic acid and (c) branched-monomer. (c) branched-monomer is or a combination thereof, wherein R is aryl group, heteroaryl group, or cycloalkyl group, and each of R1 is independently —OH, —NH2, or —COOH. The molar ratio of (a) p-hydroxybenzoic acid over (b) 6-hydroxy 2-naphthoic acid is between 50:50 and 90:10. The molar ratio of (c) branched-monomer over the sum of (a) p-hydroxybenzoic acid and (b) 6-hydroxy 2-naphthoic acid is between 0.25:100 and 0.5:100. The polymer has an intrinsic viscosity of 4dL/g to 6dL/g.
Abstract:
A method for preparing a polyarylene sulfide includes reacting a methyl 4-(arylthio)aryl sulfoxide compound with sulfuric acid, methanesulfonic acid, benzenesulfonic acid, p-toluenesulfonic acid or trifluoromethanesulfonic acid to obtain a polysulfonium intermediate; and demethylating the polysulfonium intermediate to obtain a polyarylene sulfide, wherein the polysulfonium intermediate is demethylated with aqueous HCl, HBr, or HI.
Abstract:
The disclosure provides a polyester composition and a polyester article. According to an embodiment, the polyester composition includes a polyester and a branched monomer. The branched monomer has a structure represented by formula (I) or formula (H): wherein R is independently hydrogen, fluorine, chlorine, bromine, or C1-6 alkyl.