Abstract:
Provided is a light emitting device capable of realizing color reproducibility in a broad range. The light emitting device contains a light emitting element having an emission peak wavelength in a range of 430 nm or more and 470 nm or less, a first fluorescent material having a composition represented by formula (I), which has an emission peak wavelength in a range of 510 nm or more and 525 nm or less and has an average particle diameter that is 10.0 μm or more and 30.0 μm or less, and a second fluorescent material having an emission peak wavelength in a range of 620 nm or more and 670 nm or less: X1aMgbMncAldOa+b+c+1.5d (I) wherein X1 represents at least one element selected from the group consisting of Ba, Sr and Ca, and a, b, c and d satisfy 0.5≦a≦1.0, 0.0≦b≦0.7, 0.3≦c≦0.7, and 8.5≦d≦13.0.
Abstract:
A method of producing a fluorescent material that is capable of providing a light emitting device having excellent durability, a fluorescent material, and a light emitting device are provided. The method of producing the fluorescent material includes: preparing a calcined product having a chlorosilicate composition containing at least one element selected from the group consisting of Ca, Sr, and Ba, at least one element selected from the group consisting of Mg and Zn, at least one element selected from the group consisting of Eu, Ce, Tb, and Mn, Si, O, and Cl; and bringing the calcined product in contact with a fluorine-containing substance and heat-treating the calcined product in an inert gas atmosphere at a temperature in a range of 200° C. or more and 450° C. or less.
Abstract:
Provided is a fluoride phosphor that can improve reliability in a light-emitting device. The fluoride phosphor includes fluoride particles and an oxide covering at least a portion of the surface of the fluoride particles. The oxide contains at least one element selected from the group consisting of Si, Al, Ti, Zr, Sn, and Zn, and a content percentage of the oxide is in a range from 2 mass % to 30 mass %. The fluoride particles have a composition containing an element M including at least one element selected from the group consisting of Group 4 elements, Group 13 elements, and Group 14 elements, an alkali metal, Mn, and F, and when the number of moles of the alkali metal is 2, the number of moles of Mn is in a range greater than 0 and less than 0.2, the number of moles of the element M is a range greater than 0.8 and less than 1, and the number of moles of F is in a range greater than 5 and less than 7.
Abstract:
Provided is a light-emitting material containing a phosphor that emits red light with high luminance. The light-emitting material contains a fluoride phosphor having a first composition containing an alkali metal including K, Si, Al, Mn, and F. In the first composition, when a total number of moles of the alkali metal is 2, a total number of moles of Si, Al, and Mn is in a range from 0.9 to 1.1, a number of moles of Al is in a range from greater than 0 to 0.1, a number of moles of Mn is in a range from greater than 0 to 0.2, and a number of moles of F is in a range from 5.9 to less than 6.0. The fluoride phosphor has a cubic system crystal structure and has a lattice constant of 0.8138 nm or larger.
Abstract:
The halophosphate phosphor includes a halophosphate including an alkaline earth metal including at least calcium; europium; and a halogen including at least chlorine. An elution amount of chlorine ions after the halophosphate phosphor is brought into contact with 10 times by mass of pure water at 85° C. for five hours is 7 ppm or less.
Abstract:
Disclosed are a production method for a nitride fluorescent material, a nitride fluorescent material and a light emitting device. The production method is for producing a nitride fluorescent material that has, as a fluorescent material core, a calcined body having a composition containing at least one element Ma selected from the group consisting of Sr, Ca, Ba and Mg, at least one element Mb selected from the group consisting of Li, Na and K, at least one element Mc selected from the group consisting of Eu, Ce, Tb and Mn, and Al, and optionally Si, and N, and the method includes preparing a calcined body having the above-mentioned composition, bringing the calcined body into contact with a fluorine-containing substance, and subjecting it to a first heat treatment at a temperature of 100° C. or higher and 500° C. or lower to form a fluoride-containing first film on the calcined body, and forming on the calcined body, a second film that contains a metal oxide containing at least one metal element M2 selected from the group consisting of Si, Al, Ti, Zr, Sn and Zn and subjecting it to a second heat treatment at a temperature in a range of higher than 250° C. and 500° C. or lower.
Abstract:
A method for producing a nitride fluorescent material having high emission luminance can be provided. The method includes heat-treating a raw material mixture containing silicon nitride, silicon, an aluminium compound, a calcium compound, and a europium compound.
Abstract:
Disclosed are an aluminate fluorescent material having a high light emission intensity, and a light emitting device using the same. The aluminate fluorescent material includes a composition represented by the following formula (I). X1pEutMgqMnrAlsOp+t+q+r+1.5s (I) wherein X1 represents at least one element selected from the group consisting of Ba, Sr, and Ca; and p, q, r, s, and t each satisfy 0.5≤p≤1.0, 0≤q
Abstract:
Disclosed are a production method for a nitride fluorescent material, a nitride fluorescent material and a light emitting device. The production method is for producing a nitride fluorescent material that has, as a fluorescent material core, a calcined body having a composition containing at least one element Ma selected from the group consisting of Sr, Ca, Ba and Mg, at least one element Mb selected from the group consisting of Li, Na and K, at least one element Mc selected from the group consisting of Eu, Ce, Tb and Mn, and Al, and optionally Si, and N, and the method includes preparing a calcined body having the above-mentioned composition, bringing the calcined body into contact with a fluorine-containing substance, and subjecting it to a first heat treatment at a temperature of 100° C. or higher and 500° C. or lower to form a fluoride-containing first film on the calcined body, and forming on the calcined body, a second film that contains a metal oxide containing at least one metal element M2 selected from the group consisting of Si, Al, Ti, Zr, Sn and Zn and subjecting it to a second heat treatment at a temperature in a range of higher than 250° C. and 500° C. or lower.
Abstract:
A method for producing a nitride fluorescent material having high emission luminance can be provided. The method includes heat-treating a raw material mixture containing silicon nitride, silicon, an aluminium compound, a calcium compound, and a europium compound.