Abstract:
An anti-staining fabric includes a base cloth and an anti-staining resin. The anti-staining resin is disposed on the base cloth, in which a method of fabricating the anti-staining resin includes the following steps. A first thermal process is performed to mix a polyol, a cross-linking agent, and a choline to form a first mixture, in which a reaction temperature of the first thermal process is between 90° C. and 120° C. A second thermal process is performed to mix the first mixture and a chain extender to form the anti-staining resin, in which the chain extender includes a first reagent and a second reagent, and a reaction temperature of the second thermal process is between 120° C. and 150° C.
Abstract:
A preparation method of separation membrane is provided. First, a polyimide composition including a dissolvable polyimide, a crosslinking agent, and a solvent is provided. The dissolvable polyimide is represented by formula 1: wherein B is a tetravalent organic group derived from a tetracarboxylic dianhydride containing aromatic group, A is a divalent organic group derived from a diamine containing aromatic group, A′ is a divalent organic group derived from a diamine containing aromatic group and carboxylic acid group, and 0.1≤X≤0.9. The crosslinking agent is an aziridine crosslinking agent, an isocyanate crosslinking agent, an epoxy crosslinking agent, a diamine crosslinking agent, or a triamine crosslinking agent. A crosslinking process is performed on the polyimide composition. The polyimide composition which has been subjected to the crosslinking process is coated on a substrate to form a polyimide membrane. A dry phase inversion process is performed on the polyimide membrane.
Abstract:
A method of preparing a thermoplastic composition is provided. The method includes the following steps. A polyetherimide or a polyphenylene sulfide is provided. A polyimide is provided, wherein the glass transition temperature of the polyimide is between 128° C. and 169° C., the 10% thermogravimetric loss temperature of the polyimide is between 490° C. and 534° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and the solid content of the polyimide is 30 wt %, the viscosity of the polyimide is between 100 cP and 250 cP. A melt process is performed to mix the polyetherimide and the polyimide or mix the polyphenylene sulfide and the polyimide to form a thermoplastic composition. Further, a thermoplastic composition is also provided.
Abstract:
A non-woven film for electronic components is provided in the present disclosure. The non-woven film for electronic components includes a polyetherimide substrate and an aerogel. The aerogel is disposed on the polyetherimide substrate. The aerogel has a moisture content between 0.7% and 0.9% and a porosity between 85% and 95%.
Abstract:
A zwitterionic resin is manufactured by a manufacturing method which includes the following steps. A first thermal process is performed on a first crosslinking agent and a choline having hydroxyl group or amino group to form a first mixture, in which the first crosslinking agent includes an isocyanate group. A second thermal process is performed on the first mixture, a second crosslinking agent, a chain extender, and an amino acid to form the zwitterionic resin, in which the chain extender includes a polyol.
Abstract:
A water-repellent fabric includes a base cloth and a water-repellent resin. The water-repellent resin is disposed on the base cloth, in which a method of fabricating the water-repellent resin includes the following steps. A first thermal process is performed to mix a polyol, a cross-linking agent, and a choline to form a first mixture, in which a reaction temperature of the first thermal process is between 90° C. and 120° C. A second thermal process is performed to mix the first mixture and a water repellent to form the water-repellent resin, in which the water repellent includes a hydroxyl group, an amino group, or combinations thereof, and a reaction temperature of the second thermal process is between 120° C. and 150° C.
Abstract:
A poly(amide-imide) is provided. The poly(amide-imide) is represented by formula (1), wherein R is a C6 aryl group, a C7-C8 aralkyl group, a C2-C6 alkoxyalkyl group, or a C3-C18 alkyl group; and 0.02≤X≤0.5.
Abstract:
A manufacturing method for a transparent fiber is provided. The method includes forming a spinning solution containing a polyimide polymer in an organic solvent. The polydispersity index (PDI) of the polyimide polymer is 1.3˜2.6. The spinning solution is used to perform a dry-jet wet spinning step to form a plurality of fibers. Furthermore, the plurality of fibers are subjected to a thermal drawing step to form a plurality of transparent fibers, wherein the temperature of the thermal drawing step is controlled from 215° C. to 350° C. The manufacturing method for a transparent fiber provided in the present invention makes use of a polyimide polymer material and utilizes a dry-jet wet spinning step and a thermal drawing step, which allows the formation of a transparent and high strength polyimide fiber.
Abstract:
A preparation method of separation membrane is provided. First, a polyimide composition including a dissolvable polyimide, a crosslinking agent, and a solvent is provided. The dissolvable polyimide is represented by formula 1: wherein B is a tetravalent organic group derived from a tetracarboxylic dianhydride containing aromatic group, A is a divalent organic group derived from a diamine containing aromatic group, A′ is a divalent organic group derived from a diamine containing aromatic group and carboxylic acid group, and 0.1≦X≦0.9. The crosslinking agent is an aziridine crosslinking agent, an isocyanate crosslinking agent, an epoxy crosslinking agent, a diamine crosslinking agent, or a triamine crosslinking agent. A crosslinking process is performed on the polyimide composition. The polyimide composition which has been subjected to the crosslinking process is coated on a substrate to form a polyimide membrane. A dry phase inversion process is performed on the polyimide membrane.
Abstract:
A method for preparing a polyetherimide/polyester blend chip includes providing a composition. The composition includes a polyetherimide powder and a polyester powder. The polyetherimide powder has a variable diameter in a range of 10 μm to 600 μm. The polyester powder has a variable diameter in a range of 10 μm to 600 μm and a limiting viscosity in a range of 0.85 dl/g to 1.10 dl/g. Then, performing a powder dispersion treatment on the composition. The composition undergoes melt compounding after performing the powder dispersion treatment. The composition is next pelletizing melt compounding.