Abstract:
A polymer comprises reaction product of (a) one or more diacid, diester thereof, glycolide, and (b) one or more polyol, wherein component (a) comprises glycolide or combinations thereof, and component (b) comprises one or more polyol comprising a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract:
The instant invention is a pressure sensitive adhesive composition comprising an ultra-high solid polyurethane dispersion. The ultra-high solid polyurethane dispersion comprises (1) a first component comprising a first polyurethane prepolymer comprising the reaction product of a polyol and polyisocyanate, (2) a second component comprising a media phase selected from the group consisting of a second polyurethane prepolymer emulsion, a low solid content polyurethane dispersion, a seed latex, and combinations thereof; and (3) optionally a chain extender. The ultra-high solid polyurethane dispersion has at least a solid content of at least 60 percent by weight of solid content, based on the total weight of the ultra-high solid polyurethane dispersion, and a viscosity of less than 5000 cps at 20 rpm at 21° C. using spindle #4 with Brookfield viscometer.
Abstract:
An aqueous leather coating composition having improved storage stability includes 1 to 40 weight percent of an emulsifiable polyisocyanate comprising the reaction product of an isocyanurate and an emulsifier, wherein the average isocyanate functionality of the emulsifiable polyisocyanate is 2 to 4.5; and 60 to 99 weight percent of an aqueous polymer dispersion having a Tg of −70 to 40° C. and selected from a (meth)acrylic polymer dispersion, a polyurethane dispersion, a (meth)acrylic polymer/polyurethane hybrid dispersion and a combination comprising one or more of the foregoing aqueous polymer dispersions, wherein all weight percents are on a dry basis, and based on the total dry amount of the emulsifiable polyisocyanate and the aqueous polymer dispersion. The aqueous polymer dispersion can be free of hydroxyl groups. Also disclosed are a method of coating leather with the composition, and a coated leather article.
Abstract:
The instant invention is a composite dispersion, method of producing the same, and articles made therefrom. The composite dispersion according to the instant invention comprises (1) a first seed dispersion comprising (a) a first internal phase; and (b) an external phase, and (2) a second internal phase; wherein the composite dispersion comprises more than 60 percent by the combined weight of the first internal phase and the second internal phase, and the composite dispersion has a viscosity of less than 10,000 cP measured by RV4 spindle at 20 rpm at greater than 60 weight percent total internal phase, and wherein the composite dispersion has a bimodal particle size distribution and a particle size ratio (P2/P1) in the range of 2 to 200.
Abstract:
The instant disclosure provides a die assembly for producing an annular microcapillary product. The die assembly is operatively connectable to an extruder having a thermoplastic material passing therethrough. The die assembly includes a shell, an inner manifold, an outer manifold, and a die assembly. The inner and outer manifolds are positionable in the shell with matrix flow channels thereabout to receive the thermoplastic material therethrough such that matrix layers of the thermoplastic material are extrudable therefrom. The die insert is disposable between the inner and the outer manifolds, and has a distribution manifold with a tip at an end thereof defining microcapillary channels to pass a microcapillary material therethrough whereby microcapillaries are formed between the matrix layers.
Abstract:
Provided is an aqueous composition comprising dispersed particles that comprise a polyurethane, wherein said polyurethane is a reaction product of a group of reactants (GR1), wherein GR1 comprises one or more aromatic polyisocyanates and, a polyol component, wherein said polyol component comprises (a) 50% to 99% by weight, based on the weight of said polyol component, one or more polyester polyols, (b) 0.1% to 10% by weight, based on the weight of said polyol component, one or more diols having a hydrophilic side chain, and (c) 0.9% to 40% by weight, based on the weight of said polyol component, one or more polyols different from (a) and (b). Also provided is a method of bonding a metal foil to a polymer film using such an aqueous composition.
Abstract:
The invention provides a layered structure comprising at least two layers: A) a first layer A, formed from a composition A, comprising a polyurethane; and B) a second layer B, formed from a composition B, comprising at least one functionalized polymer B comprising the following: i) at least one polymerized monomeric unit comprising a functional group selected from the group consisting of the following: a) an acid group, b) an anhydride group, c) a primary or secondary amine group, and d) combinations thereof; or ii) at least one reacted functionalization agent comprising a functional group selected from the group consisting of the following: e) an acid group, f) an anhydride group, g) a primary or secondary amine group, and h) combinations thereof; or iii) combinations thereof; and wherein the functionalized polymer B has a number-average molecular weight greater than 1,000 g/mole, and/or a melt index (I2) less than, or equal to, 2500 g/10 min.
Abstract:
A barrier film comprising a polyester-based polymer with (a) an O2 gas permeability of 0.25 cc-mil/100 in.2 24 hrs atm (5 cc 20 μm/m2 24 hrs atm) at 80% relative humidity (ASTM D-3985) or less, (b) a moisture permeability of 0.5 g-mil/100 in.2 24 hrs atm (9.8 g 20 μm/m2 24 hrs atm) at 38° C. (ASTM F-1249) or less, (c) haze of 1% or less (ASTM D1003), and (d) a glass transition temperature of 100° C. or higher. The polyester-based polymer may comprise reaction product of (a) one or more diacid or diester thereof, and (b) one or more polyol, wherein component (a) comprises 5 to 100 mole %, based on the total amount of component (a), of 2,5-furan dicarboxylic acid, or one or more C1 to C10 alkyl diester thereof, and component (b) comprises ethylene glycol, a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract translation:包含聚酯基聚合物的隔离膜,其具有(a)在80%相对湿度下的氧气渗透率为0.25cc密尔/ 100in.2,24小时atm(5cc20μm/ m 2 24小时atm)(ASTM D- 3985)或更小,(b)在38℃下24小时大气压(9.8g20μm/ m 2 24小时atm)下的透湿度为0.5g密耳/ 100(ASTM F-1249)或更低,( c)雾度为1%以下(ASTM D1003),(d)玻璃化转变温度为100℃以上。 基于聚酯的聚合物可以包含(a)一种或多种二酸或二酯的反应产物和(b)一种或多种多元醇,其中组分(a)占组分总量的5-100摩尔% a),2,5-呋喃二羧酸或其一个或多个C1至C10烷基二酯,组分(b)包括乙二醇,1,3-环己烷二甲醇和1,4-环己烷二甲醇的混合物,或2, 2,4,4-四甲基-1,3-环丁二醇或其组合。
Abstract:
The invention provides a layered structure comprising at least two layers: A) a first layer A formed from a composition A comprising a polyurethane; B) a second layer B formed from a composition B comprising at least one compound selected from the group consisting of the following compounds: a) a compound 1 comprising at least one acid group, b) a compound 2 comprising at least one anhydride group, c) a compound 3 comprising at least one primary amine group and/or at least one secondary amine group, and d) a combination thereof; and wherein the compound has a molecular weight or number average molecular weight, each less than 10,000 g/mole.