21.
公开(公告)号:US20200217999A1
公开(公告)日:2020-07-09
申请号:US16821858
申请日:2020-03-17
Applicant: FUJIFILM Corporation
Inventor: Tetsushi MIYATA , Shunsuke KITAJIMA
IPC: G02B5/22 , G02B5/00 , G02F1/1335 , C08F2/44 , H01L31/0232
Abstract: A resin composition includes a near infrared absorbing colorant, an antioxidant, and a resin, in which a content of the near infrared absorbing colorant is 5 mass % or higher with respect to a total solid content of the resin composition, and the antioxidant includes a hindered amine compound.
-
公开(公告)号:US20200183277A1
公开(公告)日:2020-06-11
申请号:US16789229
申请日:2020-02-12
Applicant: FUJIFILM Corporation
Inventor: Hiroaki TSUYAMA , Takuya TSURUTA , Kyohei ARAYAMA , Kazutaka TAKAHASHI , Tetsushi MIYATA
Abstract: A composition includes: an infrared absorbing pigment; an acid or a base that undergoes neutralization or a salt interchange reaction with the infrared absorbing pigment; an acidic or basic resin; and a solvent, in which in a case where the acid is included, the acidic resin is included, in a case where the base is included, the basic resin is included, and in a case where a pKa of the acid is represented by pKa1A, a conjugate acid pKa of the base is represented by pKa1B, a pKa of the acidic resin is represented by pKa2A, and a conjugate acid pKa of the basic resin is represented by pKa2B, any one of the following Expression A or Expression B is satisfied. pKa1A>pKa2A Expression A pKa1B
-
公开(公告)号:US20190300694A1
公开(公告)日:2019-10-03
申请号:US16443114
申请日:2019-06-17
Applicant: FUJIFILM Corporation
Inventor: Kazutaka TAKAHASHI , Tetsushi MIYATA , Hiromu KOIZUMI
Abstract: A resin composition includes an organic pigment, a resin, and a solvent, in which a content of a Na atom is 0.01 to 50 mass ppm with respect to a total solid content of a resin composition.
-
公开(公告)号:US20180196179A1
公开(公告)日:2018-07-12
申请号:US15912574
申请日:2018-03-06
Applicant: FUJIFILM Corporation
Inventor: Hirotaka TAKISHITA , Tetsushi MIYATA , Masahiro MORI , Kazuto SHIMADA , Ryoji GOTO
CPC classification number: G02B5/26 , B32B7/02 , C09K19/2014 , C09K19/322 , C09K19/36 , C09K19/56 , C09K19/586 , C09K19/588 , C09K2019/0448 , C09K2019/188 , C09K2019/2092 , C09K2019/3408 , G02B5/208 , G02B5/287 , G02B5/3016 , H01L27/14621
Abstract: A laminate includes at least one first reflective layer formed by immobilizing a liquid crystal phase in which a rotational direction of the helical axis is rightward, and at least one second reflective layer formed by immobilizing a liquid crystal phase in which the rotational direction of the helical axis is leftward, in which the laminate has a first transmission band in the wavelength range of 300 to 3,000 nm, the half-width of the first transmission band is 200 nm or less, an average transmittance in a wavelength range from a half-value wavelength A on the short wavelength side of the first transmission band to a half-value wavelength B on the long wavelength side of the first transmission band is 50% or more, and the average transmittance in the wavelength range of 100 nm from the half-value wavelength A to the short wavelength side and the average transmittance in the wavelength range of 100 nm from the half-value wavelength B to the long wavelength side are respectively less than 20%.
-
-
-