Super absorbent polymer and method for preparing same

    公开(公告)号:US10711074B2

    公开(公告)日:2020-07-14

    申请号:US16319057

    申请日:2018-01-23

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a super absorbent polymer and a method for preparing the same. According to the super absorbent polymer and the method for preparing a super absorbent polymer of the present invention, a laponite is contained in a colloidal solution state during polymerization of the monomer composition, and thus achieves an appropriate crosslinking density, thereby contributing to improvement of various physical properties such as a gel strength and a centrifuge retention capacity of the super absorbent polymer.

    Super Absorbent Polymer And Method For Preparing Same

    公开(公告)号:US20200123281A1

    公开(公告)日:2020-04-23

    申请号:US16319057

    申请日:2018-01-23

    Applicant: LG Chem, Ltd.

    Abstract: The present invention relates to a super absorbent polymer and a method for preparing the same. According to the super absorbent polymer and the method for preparing a super absorbent polymer of the present invention, a laponite is contained in a colloidal solution state during polymerization of the monomer composition, and thus achieves an appropriate crosslinking density, thereby contributing to improvement of various physical properties such as a gel strength and a centrifuge retention capacity of the super absorbent polymer.

    Super Absorbent Polymer And Preparation Method Thereof

    公开(公告)号:US20190126240A1

    公开(公告)日:2019-05-02

    申请号:US16093856

    申请日:2018-01-31

    Applicant: LG Chem, Ltd.

    Abstract: The present disclosure relates to a super absorbent polymer, including: a base resin powder comprising a first cross-linked polymer of a water soluble ethylene-based unsaturated monomer containing acidic groups which are at least partially neutralized; and a surface cross-linked layer comprising a second cross-linked polymer further cross-linked from the first cross-linked polymer and formed on the base resin powder, wherein the first cross-linked polymer is bound to a porous zeolite in which a mesopore having a BET surface area of at least 100 m2/g and a porosity of at least 0.2 cm3/g is formed, and a preparation method thereof.