Optical apparatus and method for adjusting amount of light of the same
    21.
    发明授权
    Optical apparatus and method for adjusting amount of light of the same 失效
    用于调节其光量的光学装置和方法

    公开(公告)号:US07116494B2

    公开(公告)日:2006-10-03

    申请号:US10996733

    申请日:2004-11-24

    申请人: Masahiro Yamazaki

    发明人: Masahiro Yamazaki

    IPC分类号: G02B13/18 G02B3/02 G02B7/02

    CPC分类号: G02B27/144 G02B7/023

    摘要: An optical apparatus provided in an optical pickup includes first and second light sources, a light splitting element, a condensing lens, a mounting base, a light receiving element, and a protruding piece formed on the condensing lens. The condensing lens guides transmission light from the first light source or reflection light from the second light source that are split by the light splitting element to the light receiving element. By grasping the protruding piece to protrude in a direction perpendicular to a lens axis of the condensing lens, and adjusting a mounting position of the condensing lens on the mounting base, a sufficient amount of light for stable control of a light output is applied to the light receiving element for light output monitor.

    摘要翻译: 设置在光学拾取器中的光学装置包括第一和第二光源,分光元件,聚光透镜,安装基座,光接收元件和形成在聚光透镜上的突出片。 聚光透镜将来自第一光源的透射光或来自第二光源的反射光引导到由光分离元件分离的光接收元件。 通过将突出部件沿着与会聚透镜的透镜轴线垂直的方向突出并且将聚光透镜的安装位置调整在安装基座上,将足够量的用于稳定控制光输出的光施加到 光输出监视器用光接收元件。

    Narrow angle v-type engine
    22.
    发明申请
    Narrow angle v-type engine 失效
    窄角v型发动机

    公开(公告)号:US20060011153A1

    公开(公告)日:2006-01-19

    申请号:US10529944

    申请日:2003-10-08

    申请人: Masahiro Yamazaki

    发明人: Masahiro Yamazaki

    IPC分类号: F02B75/22 F01L1/26 F02M35/10

    CPC分类号: F02B75/221

    摘要: A V-engine having a plurality of cylinders (2) arranged alternately in two banks comprises a combustion chamber provided for each of the cylinders (2), an intake port (20) which connects the combustion chamber to an intake manifold (50), and an exhaust port (30) which connects the combustion chamber to an exhaust manifold (70). The intake ports (20) of the two banks are all configured so as to pass through one of the banks, and the exhaust ports (30) of the two banks are all configured so as to pass through the other bank. The angle formed by the two banks is set to eight degrees or less.

    摘要翻译: 具有交替设置在两组中的多个气缸(2)的V型发动机包括:为每个气缸(2)设置的燃烧室,将燃烧室连接到进气歧管(50)的进气口(20) 以及将燃烧室连接到排气歧管(70)的排气口(30)。 两组的进气口(20)全部构成为通过其中一个排,并且两个排的排气口(30)都被配置为通过另一个排。 由两组形成的角度设定为8度以下。

    Information processing apparatus, information processing method, and software product
    23.
    发明申请
    Information processing apparatus, information processing method, and software product 审中-公开
    信息处理装置,信息处理方法和软件产品

    公开(公告)号:US20050007444A1

    公开(公告)日:2005-01-13

    申请号:US10886727

    申请日:2004-07-09

    摘要: An information processing apparatus comprises a camera that outputs picture information, a memory which stores concise information related to at least one string of one or more characters and a data communication interface for communication via a network. The information processing apparatus includes a CPU which recognizes a string of one or more characters included in picture information output by the camera and displays a result of recognition and the concise information related to the recognized string of one or more characters in response to a character recognition request by a user. The CPU also controls the data communication interface to communicate via a network and displays information received by the data communication interface, when the user requests detailed information related to the recognized string of one or more characters.

    摘要翻译: 信息处理装置包括输出图像信息的相机,存储与至少一个一个或多个字符串相关的简明信息的存储器和用于经由网络进行通信的数据通信接口。 信息处理装置包括:CPU,其识别由相机输出的图像信息中包含的一个或多个字符的串,并响应于字符识别显示与一个或多个字符的识别串相关的识别结果和简明信息 用户请求 当用户请求与一个或多个字符的识别字符串相关的详细信息时,CPU还控制数据通信接口通过网络通信并显示由数据通信接口接收的信息。

    Method of manufacturing hollow fiber
    25.
    发明授权
    Method of manufacturing hollow fiber 失效
    制造中空纤维的方法

    公开(公告)号:US4385017A

    公开(公告)日:1983-05-24

    申请号:US273306

    申请日:1981-06-15

    摘要: A method of manufacturing a microporous hollow fiber having a high permeability to water characterized in that a spinning solution of (A) polyacrylonitrile, (B) an acrylonitrile copolymer, or (C) an admixture of (A) and (B) in an organic solvent is extruded from an annular slit, while simultaneously extruding an organic core liquid which is a solvent for (A), (B) and (C) or a swelling agent capable of swelling them from an orifice encircled by the annular slit and introducing the extruded spinning solution with the core liquid into an aqueous coagulating bath to coagulate the spinning solution to form the hollow fiber.

    摘要翻译: 一种具有高渗透性的微孔中空纤维的制造方法,其特征在于:(A)聚丙烯腈,(B)丙烯腈共聚物或(C)(A)和(B)的混合物的有机溶剂 溶剂从环形狭缝挤出,同时挤出作为(A),(B)和(C)的溶剂的有机芯液或能够从由环形狭缝包围的孔中膨胀的溶胀剂,并引入 将具有核心液体的挤出纺丝溶液加入到水性凝固浴中以使纺丝溶液凝结以形成中空纤维。

    Biodegradable aliphatic polyester particles and production process thereof
    26.
    发明授权
    Biodegradable aliphatic polyester particles and production process thereof 有权
    生物降解脂肪族聚酯颗粒及其制备方法

    公开(公告)号:US08865304B2

    公开(公告)日:2014-10-21

    申请号:US13452119

    申请日:2012-04-20

    IPC分类号: C08G63/06 C08G63/88 C08G63/08

    摘要: Biodegradable aliphatic polyester particles have: (A) an average particle diameter of 10 to 500 μm, and (B) a quantity of heat of low-temperature crystallization calculated as an exotherm attending on crystallization, detected in the course of heating by DSC, of at least 1 J/g, and preferably: (C) a quantity of heat of crystal melting calculated as an endotherm attending on melting of a crystal, detected in the course of the heating, of less than 100 J/g, and (D) a difference between the quantity of heat of crystal melting and the quantity of heat of low-temperature crystallization of less than 90 J/g. A process for producing the particles comprises grinding a particular biodegradable aliphatic polyester having a weight average molecular weight of at least 50,000 at not lower than 0° C. and lower than the glass transition temperature of the polyester while applying high shearing force.

    摘要翻译: 生物降解性脂肪族聚酯粒子具有:(A)平均粒径为10〜500μm,(B)以DSC为加热过程中检测到的结晶化时的热分解热量, 至少为1J / g,优选为:(C)在加热过程中检测到的以熔融结晶为基准的吸热热量计算为小于100J / g的结晶熔融量,(D )结晶熔融热量与低温结晶热量之差小于90J / g。 制造颗粒的方法包括在施加高剪切力的同时,在不低于0℃并且低于聚酯的玻璃化转变温度的情况下研磨重均分子量为至少50,000的特定的可生物降解的脂族聚酯。

    Coating liquid, gas-barrier multilayer structure and gas-barrier shaped article therefrom, and process for producing gas-barrier multilayer structure
    27.
    发明授权
    Coating liquid, gas-barrier multilayer structure and gas-barrier shaped article therefrom, and process for producing gas-barrier multilayer structure 有权
    涂布液,阻气性多层结构体及其阻气性物品,以及阻气性多层结构体的制造方法

    公开(公告)号:US08808816B2

    公开(公告)日:2014-08-19

    申请号:US12312772

    申请日:2007-09-28

    摘要: Gas-barrier multilayer structures and gas-barrier shaped articles are sufficiently prevented from clouding even when exposed to cold water at 30° C. or below and have excellent gas barrier properties. Processes for producing such gas-barrier multilayer structures, and coating liquids (A) of excellent coating properties that are used to produce the multilayer structures are also provided. A coating liquid (A) includes a solvent mixture of water and an organic solvent and a polycarboxylic acid polymer partially neutralized with a polyvalent metal wherein the polymer is both dissolved and dispersed as particles in the solvent mixture and wherein the particles dispersed account for 5 to 80 wt% of 100 wt% of the polycarboxylic acid polymer partially neutralized with a polyvalent metal.

    摘要翻译: 即使暴露在30℃以下的冷水中也能够充分防止气体阻隔性多层结构和阻气成形体的混浊,具有优异的阻气性。 还提供了用于生产这种阻气性多层结构的方法和用于制备多层结构的具有优异涂层性质的涂布液(A)。 涂布液(A)包括水和有机溶剂的溶剂混合物和用多价金属部分中和的多元羧酸聚合物,其中聚合物都作为颗粒溶解并分散在溶剂混合物中,并且其中分散的颗粒占5〜 80重量%的100重量%的多元羧酸聚合物用多价金属部分中和。

    POLYGLYCOLIC ACID-BASED FIBERS AND METHOD FOR PRODUCING SAME
    29.
    发明申请
    POLYGLYCOLIC ACID-BASED FIBERS AND METHOD FOR PRODUCING SAME 审中-公开
    基于聚甘油酸的纤维及其生产方法

    公开(公告)号:US20120130024A1

    公开(公告)日:2012-05-24

    申请号:US13388762

    申请日:2010-07-14

    IPC分类号: D01F6/92 C08L67/04 B29C47/00

    CPC分类号: D01F6/625 D01F6/92 D02J1/228

    摘要: A method for producing a polyglycolic acid-based fiber, includes a spinning process of obtaining undrawn yarns by melt spinning a polyglycolic acid-based resin composition, which comprises a polyglycolic acid resin and a polylactic acid resin having a weight average molecular weight of 10×104 to 30×104 in a mass ratio of the polyglycolic acid resin to the polylactic acid resin of 70/30 to 99/1. The method also includes a keeping process of keeping the undrawn yarns and a drawing process of obtaining drawn yarns by drawing the kept undrawn yarns.

    摘要翻译: 聚乙醇酸系纤维的制造方法包括使聚乙醇酸系树脂组合物熔融纺丝得到未拉伸丝的纺丝方法,所述聚乙醇酸系树脂组合物含有聚乙醇酸树脂和重均分子量为10×10的聚乳酸树脂 聚乙醇酸树脂与聚乳酸树脂的质量比为70〜30〜99/1的比例为104〜30×104。 该方法还包括保持未拉伸纱线的保持过程和通过拉伸保持的未拉伸纱线来获得拉伸纱线的拉伸过程。

    Junction structure of substrate and joining method thereof
    30.
    发明授权
    Junction structure of substrate and joining method thereof 有权
    基体的结结构及其接合方法

    公开(公告)号:US08134839B2

    公开(公告)日:2012-03-13

    申请号:US12506598

    申请日:2009-07-21

    IPC分类号: H05K1/00

    摘要: A junction structure and a joining method of substrates are provided that stably can join the substrates and achieve high workability during joining. A second substrate 2 to be joined with solder to a first substrate 1 is bent with elasticity generated by a bending portion 9, and first joints 5 on the first substrate 1 and second joints 6 on the second substrate 2 are joined with solder in a state in which the first substrate 1 is brought into contact with, in a direction that increases the bending angle of the bending portion 9, a part where the joints 6 are formed on the second substrate 2.

    摘要翻译: 提供了一种基板的接合结构和接合方法,其可以稳定地连接基板,并且在接合期间实现高的可加工性。 将与焊料接合到第一基板1的第二基板2由弯曲部9产生的弹性弯曲,并且第一基板1上的第一接头5和第二基板2上的第二接头6在焊料中以一种状态接合 其中第一基板1沿着增加弯曲部9的弯曲角度的方向与在第二基板2上形成接头6的部分接触。