摘要:
A thermoplastic molding composition is disclosed. The composition that contains at least one member selected from the group consisting of aromatic polycarbonate and polyester carbonate, a rubber-modified vinyl (co)polymer, and calcium carbonate having average particle diameter of less than 100 nm is particularly suitable for making articles resistant to hydrolysis.
摘要:
ABS moulding materials containing an addition of at least one compound of the lanthanides, process for the preparation of the moulding materials and a method for identifying ABS moulding materials.
摘要:
A thermoplastic, flame-retardant moulding composition having improved mechanical properties is disclosed. The composition contains 40 to 99 parts by weight of a thermoplastic polycarbonate or polyester carbonate, 0.5 to 60 parts by weight of a graft polymer, 0 to 45 parts by weight of a thermoplastic vinyl copolymer, 0.5 to 20 parts by weight of a mixture of at least one mono- and at least one oligo-phosphorus conforming to the general formula and 0.05 to 5 parts by weight of a fluorinated polyolefine.
摘要:
An additive mixture containing a dibenzoate and either or both of a compound containing at least one structural unit and a compound containing at least one structural unit is disclosed. The additive combination enhances the processability of a thermoplastic molding composition that contains a (co)polymer of styrene, methyl methacrylate, acrylonitrile, methacrylonitrile, maleic anhydride and N-substituted maleimide and a graft copolymer.
摘要:
An elastic-thermoplastic graft polymer prepared by a multi-stage free radical polymerization is described. The elastic-thermoplastic graft polymer is prepared by polymerizing (i) one or more monomers containing vinyl groups, and (ii) at least one molecular weight regulating compound, in the presence of (iii) at least one rubber in latex form. The ratio of monomers (M) to the molecular weight regulating compound (MWR) is altered throughout the various stages of the polymerization method. The M:MWR ratio is: from 50:1 to 400:1 in the first stage; from 100:1 to 800:1 in the second stage; and from 200:1 to 2000:1 in the third stage of the polymerization. In at least one further reaction stage of the polymerization, the monomers, in the absence of the molecular weight regulating compound, are polymerized in the presence of the rubber. This further reaction stage occurs before the first stage and/or after the third stage of the polymerization. The multi-stage polymerization is conducted such that: M:MWR (first stage)≦M:MWR (second stage)
摘要:
ABS type thermoplastic moulding compounds obtainable by A) producing a rubber latex with an average particle diameter d.sub.50 of 30 to 160 nm and a gel content of 75 to 100 wt. % B) emulsion polymerization of an amount of butadiene and optionally up to 50 wt. % (with reference to the total amount of monomer in stage B) of a comonomer in the presence of the rubber obtained in stage A, such that a rubber latex (B) with an average particle diameter d.sub.50 =220 to 330 nm and a gel content of 25 to 70 wt. % is produced, C) emulsion polymerization of 40 to 95 parts by wt. of a mixture of styrene and acrylonitrile, which optionally contains up to 50 wt. % (with reference to the total amount of monomers used in stage C) of one or more comonomers, in the presence of 5 to 60 parts by wt. (with reference to the solids) of the rubber obtained in stage B by introducing the monomer in such a way that 55 to 90 wt. % of the monomers are added within the first half of the total monomer introduction time, and D) mixing the polymer obtained in stage C, preferably after first converting it into a powder, with at least one thermoplastic vinyl resin.
摘要:
Thermoplastic moulding materials containing A. 15 to 80 parts by weight of a thermoplastic polycarbonate or polyester carbonate, and B. 4 to 40 parts by weight of a graft polymer of B.1 20 to 60 weight % of one or more monomers on B.2 40 to 80 weight % of one or more graft bases having glass transition temperatures
摘要:
The invention relates to thermoplastic molding compounds of 70 to 99.5% by weight thermoplastic polyamides and 30 to 0.5% by weight hydrogenated nitrile rubber and 0 to 29.5% by weight thermoplastic resin components and, optionally, standard additives in typical quantities. These thermoplastic molding compounds show high strength values, very good moldability and, above all, high weathering resistance.
摘要:
Thermoplastic molding compounds comprising three resin components with different molecular weights and two graft rubbers. The thermoplastic molding compounds have high toughness, adequate heat resistance, adjustable surface gloss and excellent thermoplastic processability. The invention also relates to a process for the production of the molding compounds.
摘要:
Moulding compositions comprisingA) from 5 to 95% by weight of a graft product of a mixture of from 50 to 100 parts by weight of styrene, .alpha.-methylstyrene, vinyl toluene, methyl methacrylate or mixtures thereof and from 0 to 50 parts by weight of acrylonitrile on a particulate silicone rubber having an average particle diameter (d.sub.50) of from 0.10 to 0.50 .mu.m with a total rubber content of from 30 to 90% by weight andB) from 95 to 5% by weight of a graft product of a mixture of from 50 to 100 parts by weight of styrene, .alpha.-methylstyrene, vinyl toluene, methyl methacrylate or mixtures thereof and from 0 to 50 parts by weight of acrylonitrile on a particulate EPDM rubber having an average particle diameter (d.sub.50) of from 0.20 to 1.00 .mu.m with a total rubber content of from 10 to 50% by weight.