摘要:
A porous sintered body is composed of a perovskite-type composite oxide, wherein A-site of the composite oxide are occupied by one or more kinds of first metallic elements selected from the group consisting of calcium and strontium, one or more kinds of second metal elements selected from the group consisting of rare earth elements and yttrium excluding lanthanum and cerium, and lanthanum, the above one or more kinds of the first metallic elements amount to 5 to 70 mol % of the A-sites, and manganese is contained in B-sites of the composite oxide.
摘要:
In order to improve a reliability of a glass joint body, first ceramic member and second ceramic member are connected by using (a) glass consisting of 10.about.65 wt % of SiO.sub.2, 30 wt % or less of Na.sub.20, and the balance of B.sub.2 O.sub.3 and Al.sub.2 O.sub.3, (b) glass including less than 10 wt % of SiO.sub.2, and 30.about.80 wt % of B.sub.2 O.sub.3, (c) glass including substantially none of SiO.sub.2, and 30.about.80 wt % of B.sub.2 O.sub.3, or (d) glass consisting of 10.about.65 wt % of SiO.sub.2, 20 wt % or less of Na.sub.2 O, 30 wt % or less of Al.sub.2 O.sub.3, 20 wt % or less of MgO, and the balance of B.sub.2 O.sub.3.
摘要翻译:为了提高玻璃接合体的可靠性,第一陶瓷部件和第二陶瓷部件通过使用(a)由10重量%的SiO 2,30重量%以下的Na 2 O,和余量的B 2 O 3组成的玻璃连接 和(b)包含小于10重量%的SiO 2和30重量%的B 2 O 3的玻璃,(c)基本上不含SiO 2和30重量%的B 2 O 3的玻璃,或(d)玻璃组成的玻璃 的10重量%的SiO 2,20重量%以下的Na 2 O,30重量%以下的Al 2 O 3,20重量%以下的MgO,余量的B 2 O 3。
摘要:
A beta alumina sintered body having a wide optimum sintering temperature range and a high sodium ion conductivity includes 8.0-10.0 wt % of sodium oxide, 3.0-5.5 wt % of magnesium oxide, 0.01-1.0 wt % of tin oxide, and the remainder of aluminum oxide. This sintered body is manufactured by mixing raw materials including 8.0-10.0 wt % of sodium oxide, 3.0-5.5 wt % of magnesium oxide, 0.01-1.0 wt % of tin oxide, and the remainder of aluminum oxide to obtain raw material powder; forming the raw material powder to obtain a formed body; and sintering the formed body to obtain a beta alumina sintered body.
摘要:
The disclosed polycrystalline transparent sintered body contains Al.sub.2 O.sub.3 and MgO at a molar ratio of (0.54:0.46) to (0.58:0.42) and has an in-line transmittance of more than 77% for 1 mm thickness at a light wavelength of 0.6 .mu.m, which sintered body is produced by preparing fine spinel powder through hydrolysis of an isopropanol solution of aluminum isopropoxide and magnesium isopropoxide, forming a shaped body from the powder, and sintering the shaped body.
摘要:
A cleaning method is provided that includes a step of preparing a cleaning composition containing 57 to 95 wt % of (component a) water, 1 to 40 wt % of (component b) a secondary hydroxy group- and/or tertiary hydroxy group-containing hydroxy compound, (component c) an organic acid, and (component d) a quaternary ammonium compound, the composition having a pH of 5 to 10, and a step of removing plasma etching residue formed above a semiconductor substrate by means of the cleaning composition. There are also provided a process for producing a semiconductor device that includes a step of cleaning plasma etching residue formed above a semiconductor substrate using the cleaning method, and a cleaning composition for removing plasma etching residue formed above a semiconductor substrate that contains 57 to 95 wt % of (component a) water, 1 to 40 wt % of (component b) a secondary hydroxy group- and/or tertiary hydroxy group-containing hydroxy compound, (component c) an organic acid, and (component d) a quaternary ammonium compound, the composition having a pH of 5 to 10.
摘要:
A cleaning method is provided that includes a step of preparing a cleaning composition containing 57 to 95 wt % of (component a) water, 1 to 40 wt % of (component b) a secondary hydroxy group- and/or tertiary hydroxy group-containing hydroxy compound, (component c) an organic acid, and (component d) a quaternary ammonium compound, the composition having a pH of 5 to 10, and a step of removing plasma etching residue formed above a semiconductor substrate by means of the cleaning composition. There are also provided a process for producing a semiconductor device that includes a step of cleaning plasma etching residue formed above a semiconductor substrate using the cleaning method, and a cleaning composition for removing plasma etching residue formed above a semiconductor substrate that contains 57 to 95 wt % of (component a) water, 1 to 40 wt % of (component b) a secondary hydroxy group- and/or tertiary hydroxy group-containing hydroxy compound, (component c) an organic acid, and (component d) a quaternary ammonium compound, the composition having a pH of 5 to 10.
摘要:
A ceramic filter is provided including a substrate, a separation layer comprising titania and having an average pore size in a range of 0.08 to 1 μm and a thickness in a range of 5 to 20 μm, and an intermediate layer formed between the substrate and the separation layer. The intermediate layer includes aggregate particles that are bonded together with glass frits, and aggregate particles of the intermediate layer are smaller than aggregate particles of the substrate and larger than aggregate particles of the separation layer.
摘要:
A ceramic filter has (A) a base body having partition walls made of a ceramic porous body, wherein cells 18 are defined by the partition walls, (B) filer membranes provided on the partition walls, made of a ceramic porous body having an average pore diameter smaller than that of the surface of each partition wall, and (C) a glass seal provided so as to cover at least the end face of the base body, wherein the glass seal is constituted by an alkali-free glass containing silica (SiO2) in an amount of 55 to 65 mol %, zirconia (ZrO2) in an amount of 1 to 10 mol % and at least one kind of alkaline earth metal oxide selected from calcia, baria and strontia but substantially not containing zinc oxide.
摘要:
A ceramic porous body is provided which uses a binder made of a glass that has excellent acid resistance and alkali resistance and which can be used for a long period of time as a filtration filter. The ceramic porous body is formed from ceramic particles that are bonded using a glass binder comprising 5 to 20 mol % of a plurality of metal oxides, selected from the group consisting of Li2O, Na2O, K2O, MgO, CaO, SrO and BaO and containing at least two alkali metal oxides selected from the group consisting of Li2O, Na2O and K2O as an essential component, at least 3 mol % of at least one of ZrO2 and TiO2 as a total amount, and SiO2 and incidental impurities as the balance.
摘要翻译:提供了一种陶瓷多孔体,其使用具有优异的耐酸性和耐碱性的玻璃制粘合剂,并且可以作为过滤器长时间使用。 陶瓷多孔体由使用包含5〜20摩尔%的多种金属氧化物的玻璃粘合剂结合的陶瓷颗粒形成,所述金属氧化物选自Li 2 O 2,Na 2 O, 2 O,K 2 O,MgO,CaO,SrO和BaO,并且含有至少两种选自Li 2 O, 作为必要成分的Na 2 O 2和K 2 O 2,至少3摩尔%的ZrO 2和TiO 2的至少一种, 作为总量的SiO 2和偶氮杂质作为余量。