Thermoplastic resin composition
    32.
    发明授权
    Thermoplastic resin composition 失效
    热塑性树脂组合物

    公开(公告)号:US5424360A

    公开(公告)日:1995-06-13

    申请号:US183429

    申请日:1994-01-19

    摘要: A thermoplastic resin composition having a good balance among rigidity, impact strength and adhesion of coating is provided, which comprises:a total of 100 parts by weight of (a)-(c) wherein (a) is 1-60% by weight of a polyphenylene ether, (b) 0-60% by weight of an alkenyl aromatic resin excluding unhydrogenated alkenyl aromatic block copolymer of tile following component (e) and (c) 40-99% by weight of a polyamide,(d) 1-50 parts by weight of a polyolefin having a modulus of 10000 kg/cm2 or more at room temperature,(e) 1-50 parts by weight of an unhydrogenated alkenyl aromatic block copolymer, and(f) a compatibilizing agent in an amount necessary to improve compatibility of the above components (a) and (c), said (d)-(f) being every 100 parts by weight of (a)-(c), and wherein the thermoplastic resin composition is obtained by melt kneading firstly said (a), (d) and (f) and then secondly said (c) therewith.

    摘要翻译: 提供了一种在刚性,冲击强度和涂层粘附性之间具有良好平衡的热塑性树脂组合物,其包含:总计100重量份的(a) - (c),其中(a)为1-60重量% 聚苯醚,(b)0-60重量%的链烯基芳族树脂,不包括(e)和(c)成分的未氢化的链烯基芳族嵌段共聚物,40-99重量%的聚酰胺,(d)1- 50重量份在室温下模量为10000kg / cm 2以上的聚烯烃,(e)1-50重量份未氢化的链烯基芳族嵌段共聚物,和(f)相容剂,其量为 提高上述组分(a)和(c)的相容性,所述(d) - (f)每100重量份的(a) - (c),其中所述热塑性树脂组合物通过先将所述 (a),(d)和(f),其次是(c)。

    Air battery
    34.
    发明授权
    Air battery 有权
    空气电池

    公开(公告)号:US09379397B2

    公开(公告)日:2016-06-28

    申请号:US13877183

    申请日:2011-10-03

    IPC分类号: H01M8/04 H01M12/06 H01M2/40

    摘要: An air battery having a main body including a container package member, an electrolytic solution contained in the container package member, a cathode having a cathode catalyst that is in contact with the electrolytic solution, and an anode that is in contact with the electrolytic solution; a tank storing the electrolytic solution; a pump circulating the electrolytic solution between the main body and the tank; an oxygen intake incorporating oxygen into the electrolytic solution in the way of circulation of the electrolytic solution; and a pipe arrangement connecting the tank, the pump, the oxygen intake and the main body so that the electrolytic solution circulates in the order thus named, wherein the oxygen intake has an oxygen selective permeable membrane.

    摘要翻译: 一种空气电池,其具有包括容器封装构件的主体,容纳在容器封装构件中的电解液,具有与电解液接触的阴极催化剂的阴极和与电解液接触的阳极; 储存电解液的罐; 使电解液在主体和容器之间循环的泵; 以电解液循环的方式将氧气引入电解液中; 以及连接罐,泵,氧气进口和主体的管道装置,使得电解溶液按照这样命名的顺序循环,其中氧气进入具有氧选择性渗透膜。

    Process for producing propylene resin composition
    35.
    发明授权
    Process for producing propylene resin composition 有权
    制备丙烯树脂组合物的方法

    公开(公告)号:US08293843B2

    公开(公告)日:2012-10-23

    申请号:US11100629

    申请日:2005-04-07

    IPC分类号: C08L23/10 C08F297/08

    摘要: Disclosed are processes for producing polypropylene resin compositions including two or three sorts of propylene-based polymeric materials, the processes including a first step of melt-kneading at least a propylene-α-olefin block copolymer containing a polymer portion composed mainly of propylene and a propylene-α-olefin copolymer portion having a relatively high intrinsic viscosity and a second step of melt-kneading the product of the first step with a propylene-ethylene block copolymer containing a polymer portion composed mainly of propylene and a propylene-ethylene copolymer portion having a relatively low intrinsic viscosity or a polymer portion composed mainly of propylene having a relatively low intrinsic viscosity. In the composition produced by these processes, no or substantially no fish eyes develop.

    摘要翻译: 公开了制备包含两种或三种丙烯类聚合物材料的聚丙烯树脂组合物的方法,该方法包括将至少含有主要由丙烯组成的聚合物部分的丙烯-α-烯烃嵌段共聚物熔融捏合的第一步骤和 具有相对高的特性粘度的丙烯-α-烯烃共聚物部分和将第一步骤的产物与含有主要由丙烯组成的聚合物部分的丙烯 - 乙烯嵌段共聚物和具有丙烯 - 乙烯共聚物部分的丙烯 - 乙烯共聚物部分进行熔融捏合的第二步骤, 相对低的特性粘度或主要由具有相对低的特性粘度的丙烯组成的聚合物部分。 在通过这些方法制备的组合物中,没有或基本上没有鱼眼发育。

    Propylene-ethylene-butene block copolymer and molded article thereof
    36.
    发明授权
    Propylene-ethylene-butene block copolymer and molded article thereof 有权
    丙烯 - 乙烯 - 丁烯嵌段共聚物及其模塑制品

    公开(公告)号:US07858708B2

    公开(公告)日:2010-12-28

    申请号:US12064647

    申请日:2006-08-29

    IPC分类号: C08F255/04 C08F255/02

    摘要: A propylene-ethylene-butene block copolymer is provided which includes from 60 to 85% by weight of a polypropylene portion and from 15 to 40% by weight of a propylene-ethylene-butene random copolymer portion, wherein the copolymer satisfies the requirements (1) and (2) given below. In addition, a molded article including such a propylene-ethylene-butene block copolymer is provided.(1) The random copolymer portion includes a propylene-ethylene random copolymer component (EP) and a propylene-ethylene-butene random copolymer component (EPB) and the copolymer component (EP) has an intrinsic viscosity of from 1.5 to 8 dl/g and an ethylene unit content of from 20 to 50% by weight, and the copolymer component (EPB) has an intrinsic viscosity of from 0.5 to 8 dl/g, an ethylene unit content of from 47 to 77% by weight and a butene unit component of from 3 to 33% by weight and the total of the ethylene unit content and the butene unit content is from 50 to 80% by weight.(2): The propylene-ethylene-butene block copolymer has a melt flow rate of from 5 to 120 g/10 min.

    摘要翻译: 提供了丙烯 - 乙烯 - 丁烯嵌段共聚物,其包含60至85重量%的聚丙烯部分和15至40重量%的丙烯 - 乙烯 - 丁烯无规共聚物部分,其中所述共聚物满足要求(1 )和(2)给出。 此外,提供了包含这种丙烯 - 乙烯 - 丁烯嵌段共聚物的模塑制品。 (1)无规共聚物部分包括丙烯 - 乙烯无规共聚物组分(EP)和丙烯 - 乙烯 - 丁烯无规共聚物组分(EPB),共聚物组分(EP)的特性粘度为1.5至8dl / g 乙烯单元含量为20〜50重量%,共聚物成分(EPB)的特性粘度为0.5〜8dl / g,乙烯单元含量为47〜77重量%,丁烯单元 组分为3至33重量%,乙烯单元含量和丁烯单元含量的总和为50至80重量%。 (2):丙烯 - 乙烯 - 丁烯嵌段共聚物的熔体流动速率为5〜120g / 10分钟。

    VERTICAL ARTICULATED ROBOT
    37.
    发明申请
    VERTICAL ARTICULATED ROBOT 有权
    垂直机器人

    公开(公告)号:US20100162845A1

    公开(公告)日:2010-07-01

    申请号:US12720677

    申请日:2010-03-10

    IPC分类号: B25J18/00 B25J13/00

    摘要: A vertical articulated robot includes a base; a turning base provided on the base so as to be pivotable about a first rotation axis; a first upper arm provided on the turning base so as to be turnable about a second rotation axis that is in a plane perpendicular to the first rotation axis; a second upper arm provided on a distal end portion of the first upper arm so as to be pivotable about a third rotation axis that is perpendicular to the second rotation axis; a front arm provided on a distal end portion of the second upper arm so as to be turnable about a fourth rotation axis that is in a plane perpendicular to the third rotation axis; and a wrist assembly mounted on a distal end portion of the front arm. A motor that rotates the second upper arm is mounted on a frame of the second upper arm.

    摘要翻译: 垂直铰接机器人包括底座; 设置在所述基座上以便绕第一旋转轴线枢转的转动底座; 第一上臂设置在所述转动基座上,以能够围绕垂直于所述第一旋转轴线的平面中的第二旋转轴线旋转; 第二上臂,设置在所述第一上臂的远端部分上,以能够围绕垂直于所述第二旋转轴线的第三旋转轴线枢转; 前臂,设置在所述第二上臂的前端部,以能够围绕与所述第三旋转轴线垂直的平面的第四旋转轴线旋转; 以及安装在所述前臂的前端部的腕部组件。 旋转第二上臂的马达安装在第二上臂的框架上。

    Process for producing propylene resin composition
    38.
    发明申请
    Process for producing propylene resin composition 有权
    制备丙烯树脂组合物的方法

    公开(公告)号:US20100152385A1

    公开(公告)日:2010-06-17

    申请号:US12656841

    申请日:2010-02-17

    IPC分类号: C08L53/00

    摘要: Disclosed are processes for producing polypropylene resin compositions including two or three sorts of propylene-based polymeric materials, the processes including a first step of melt-kneading at least a propylene-α-olefin block copolymer containing a polymer portion composed mainly of propylene and a propylene-α-olefin copolymer portion having a relatively high intrinsic viscosity and a second step of melt-kneading the product of the first step with a propylene-ethylene block copolymer containing a polymer portion composed mainly of propylene and a propylene-ethylene copolymer portion having a relatively low intrinsic viscosity or a polymer portion composed mainly of propylene having a relatively low intrinsic viscosity. In the composition produced by these processes, no or substantially no fish eyes develop.

    摘要翻译: 公开了制备包含两种或三种丙烯类聚合物材料的聚丙烯树脂组合物的方法,该方法包括将至少含有主要由丙烯组成的聚合物部分的丙烯-α-烯烃嵌段共聚物熔融捏合的第一步骤和 具有相对高的特性粘度的丙烯-α-烯烃共聚物部分和将第一步骤的产物与含有主要由丙烯组成的聚合物部分的丙烯 - 乙烯嵌段共聚物和具有丙烯 - 乙烯共聚物部分的丙烯 - 乙烯共聚物部分进行熔融捏合的第二步骤, 相对低的特性粘度或主要由具有相对低的特性粘度的丙烯组成的聚合物部分。 在通过这些方法制备的组合物中,没有或基本上没有鱼眼发育。

    Propylene-Ethylene Block Copolymer and Molded Article Thereof
    39.
    发明申请
    Propylene-Ethylene Block Copolymer and Molded Article Thereof 审中-公开
    丙烯 - 乙烯嵌段共聚物及其成型品

    公开(公告)号:US20080319136A1

    公开(公告)日:2008-12-25

    申请号:US12064694

    申请日:2006-08-29

    IPC分类号: C08L23/16

    摘要: A propylene-ethylene block copolymer comprising from 60 to 85% by weight of a polypropylene portion and from 15 to 40% by weight of a propylene-ethylene random copolymer portion and satisfying the requirements (1) and (2) defined below is provided. In addition, a molded article containing such a propylene-ethylene block copolymer is provided.Requirement (1): the propylene-ethylene random copolymer portion comprises a propylene-ethylene random copolymer component (EP-A) and a propylene-ethylene random copolymer component (EP-B), the copolymer component (EP-A) having an intrinsic viscosity of not less than 4 dl/g but less than 8 dl/g and an ethylene content of from 20 to 60% by weight, and the copolymer component (EP-B) having an intrinsic viscosity of not less than 0.5 dl/g but less than 3 dl/g and an ethylene content of from 40 to 80% by weight.Requirement (2): the propylene-ethylene block has a melt flow rate of from 5 to 120 g/10 min.

    摘要翻译: 提供了包含60至85重量%的聚丙烯部分和15至40重量%的丙烯 - 乙烯无规共聚物部分并满足下述(1)和(2)的要求的丙烯 - 乙烯嵌段共聚物。 另外,提供了含有这种丙烯 - 乙烯嵌段共聚物的成型品。 要求(1):丙烯 - 乙烯无规共聚物部分包括丙烯 - 乙烯无规共聚物组分(EP-A)和丙烯 - 乙烯无规共聚物组分(EP-B),共聚物组分(EP-A) 粘度不小于4dl / g但小于8dl / g,乙烯含量为20至60重量%,特性粘度不小于0.5dl / g的共聚物组分(EP-B) 但小于3dl / g,乙烯含量为40〜80重量%。 要求(2):丙烯 - 乙烯嵌段的熔体流动速率为5〜120g / 10min。

    Process for producing modified polypropylene resin
    40.
    发明授权
    Process for producing modified polypropylene resin 失效
    生产改性聚丙烯树脂的方法

    公开(公告)号:US06919410B2

    公开(公告)日:2005-07-19

    申请号:US10278982

    申请日:2002-10-24

    CPC分类号: C08F8/00 C08F10/06

    摘要: There is provided a process for producing a modified polypropylene resin, which comprises the steps of mixing the following components (A) to (D), and reacting them with one another: (A) 100 parts by weight of a polypropylene resin, (B) 0.1 to 30 parts by weight of a compound having a bond or a functional group selected from the group consisting of a non-aromatic carbon-carbon multiple bond, an oxirane group and a derived carboxyl group, (C) 0.001 to 30 parts by weight of a compound having at least two functional groups reactive to a carboxyl group, and (D) 0.01 to 20 parts by weight of an organic peroxide having a decomposition temperature of from 50 to 120° C., at which temperature a half-life of the organic peroxide is 1 minute.