摘要:
A Ni based cast alloy consisting essentially of C: 0.01 to 0.2% by weight, Si: 0.5 to 4.0% by weight, Cr: 14 to 22% by weight, Mo+W: 4.0 to 10% by weight, B: 0.001 to 0.02% by weight, Co: up to 10% by weight, Al: up to 0.5% by weight, Ti: up to 0.5% by weight, Nb: up to 5.0% by weight, Fe: up to 10% by weight, the balance being Ni and incidental impurities, wherein a γ′ phase precipitates in a matrix phase thereof.
摘要:
A Ni-based alloy member has resistance against grain boundary fracture, fatigue strength, and oxidation resistance at temperatures near 1000° C. or higher. The Ni-based alloy member includes a non-repaired region made of a Ni-based alloy base and a region repaired by welding, which is formed on the non-repaired region and which is made of a buildup-welded layer, the buildup-welded layer being made of a Ni-based alloy containing, by weight, 15% or less of Co, 18-22% of Cr, 0.8-2.0% of Al, 5.0% or less of Ta, 0.5% or less of Mo, 0.5% or less of Ti, 13-18% of W, 0.05-0.13% of C, 0.06% or less of Zr, 0.015% or less of B, 0.4-1.2% of Mn, and 0.1-0.3% of Si, the balance of the alloy being preferably essentially made of Ni.
摘要:
The invention is of a heat resisting martensitic steel comprising, by weight, 0.05 to 0.30% C, not more than 0.50% Si, not more than 0.60% Mn, 8.0 to 13.0% Cr, 0.5 to 3.0% Ni, 1.0 to 3.0% Mo, 0.1 to 1.5% W, 0.5 to 4% Co, 0.05 to 0.35% V, 0.02 to 0.30% in total of one or two elements selected from the group consisting of Nb and Ta, and 0.02 to 0.10% N, wherein a value of the square of a difference between the Ni amount and the Co amount, and the Ni amount are not more than values determined by a straight line drawn on a point A (1.0, 2.7%) and a point B (2.5, 1.0%) in the orthogonal coordinates shown in the attached drawing of FIG. 2 which represents a relationship between the above square value and the Ni amount, and an amount ratio of Mo/(Mo+0.5W) is not less than 0.5. The heat resisting steel is suitably used in various components of a gas turbine.
摘要:
A semiconductor device with a fuse 3a to be cut for a circuit modification, of which passivation film coating the uppermost wiring layer is formed in a two-layer structure including a first insulating film 11 with high filling capability and a second insulating film 12 blocking penetration of moisture or impurities. An opening 21 formed in a specific depth through the insulating films on the fuse 3a is coated by a third insulating film 13 with the blocking capability. This prevents the penetration of moisture or impurities, and the corrosion of the fuse 3a.
摘要:
A medical fluid passage switching apparatus comprising: at least, a rotatable shaft F; a cam C which is rotated in relation to the rotating movement of the shaft F to close and open divided tubes for determining a passage of a fluid; and a housing L having tube accepting holes I and so arranged to enable the holding of the cam C, is provided. More particularly, provided are such a medical fluid passage switching apparatus in a continuous ambulatory peritoneal dialysis (CAPD) system and a tube which is decreased in the diameter and/or thinned in the wall at a region where the cam or a combination of the cam and the clamp is engaged for closing and opening.
摘要:
A Ni-base superalloy consisting essentially of, by weight: 0.05 to 0.20% C, 20 to 25% Co, 15 to 25% Cr, 1.0 to 3.0% Al, 1.0 to 3.0% Ti, 1.0 to 3.0% Nb, 5 to 10% W, and at least 42.5% Ni, the combination of the [Al+Ti] and tungsten contents being determined as shown in FIG. 5. This superalloy has a high thermal-fatigue resistance, a great high-temperature strength, particularly, a great creep rupture strength, and a good weldability. The superalloy is used to form gas turbine nozzles, which are employed in a gas turbine. Using such a gas turbine, a combined power generating system is built.
摘要:
A boiler tube having a double-tube structure constituted by an inner tube and an outer tube integrated with each other. The inner tube is made of an alloy consisting essentially of, by weight, 0.02 to 0.15% of C, 0.5 to 3.5% of Si, not greater than 2% of Mn, 25 to 40% of Ni, 20.5 to 27% of Cr, 0.5 to 3% of Mo, not greater than 1% of Nb and the balance Fe and having a substantially fully austenite structure. The outer tube is made of an alloy consisting essentially of, by weight, 0.02 to 0.2% of C, not greater than 3.5% of Si, not greater than 2% of Mn, 33 to 45% of Ni, 30 to 40% of Cr and the balance Fe and having a substantially fully austenite structure. The inner tube made of the alloy having the composition specified above exhibits a high resistance to steam oxidation without any reduction in high-temperature strength even at elevated steam temperature, while the outer tube made of the alloy having the composition specified above exhibits a superior resistance to corrosion by coal combustion gas.
摘要:
A precipitation hardenable martensitic stainless steel excellent in the stability of martensite, having the high strength, high toughness and high corrosion resistance is provided. The precipitation hardenable martensitic stainless steel contains at a mass rate, C: 0.05-0.10%, Cr: 12.0-13.0%, Ni: 6.0-7.0%, Mo: 1.0-2.0%, Si: 0.01-0.05%, Mn: 0.06-1.0%, Nb: 0.3-0.5%, V: 0.3-0.5%, Ti: 1.5-2.5%, Al: 1.0-2.3%, and the remainder consisting of Fe and an unavoidable impurity.
摘要:
To provide a steam turbine rotor and a steam turbine which are highly reliable.The steam turbine rotor is characterized in that a forged material B having a hollow structure is joined to a forged material A of a Ni group super-alloy by welding, and weld back waves on an inner surface are removed, and the inner surface is smoothed, and a forging material C and a forging material B are joined to each other with a bolt.
摘要:
A solid state imaging device including a pixel region where a plurality of pixel cells 10r1, 10g1-10g3, 10b1-10b2 . . . have been formed. When focusing on a red pixel cell whose color filter has the longer transmission peak wavelength and a blue pixel cell whose color filter has the shorter transmission peak wavelength, the distribution of substrate contacts is denser in a region in the vicinity of a photodiode in the red pixel cell than a region in the vicinity of a photodiode in the blue pixel cell.