Welding method for fluorine-passivated member for welding, fluorine-passivation method after being weld, and welded parts
    41.
    发明授权
    Welding method for fluorine-passivated member for welding, fluorine-passivation method after being weld, and welded parts 有权
    用于焊接的氟钝化部件的焊接方法,焊接后的氟钝化方法以及焊接部件

    公开(公告)号:US06220500B1

    公开(公告)日:2001-04-24

    申请号:US09130583

    申请日:1998-08-07

    IPC分类号: B23K120

    摘要: A welding method for materials to be welded which are subjected to fluoride passivation treatment, and a fluoride passivation retreatment method, wherein, when fluoride passivation retreatment is conducted after welding, there is no generation of particles or dust. The method provides superior resistance to fluorine system gases. During fluoride passivation treatment, hydrogen is added to the gas (the back shield gas) flowing through the materials to be welded. In one embodiment of the welding method, the thickness of the fluoride passivated film in a predetermined range from the butt end surfaces of the materials to be welded is set to 10 nm or less, followed by subsequent welding. Furthermore, the fluoride passivation retreatment method, includes the steps of heating at least the welded parts following welding and flowing a gas containing fluorine gas in the interior portion of the parts.

    摘要翻译: 对经过氟化物钝化处理的待焊接材料的焊接方法以及氟化物钝化再处理方法,其中,在焊接后进行氟化物钝化再处理时,不产生颗粒或灰尘。 该方法提供了优异的耐氟体系气体阻力。 在氟化物钝化处理期间,将氢气流入待焊接材料的气体(背面保护气体)。 在焊接方法的一个实施例中,氟化钝化膜在待焊接材料的对接端面的预定范围内的厚度设定为10nm以下,随后进行焊接。 此外,氟化物钝化再处理方法包括以下步骤:至少在焊接之后加热焊接部分,并且在部件的内部部分使含有氟气的气体流动。

    Lead frame and lead frame material
    42.
    发明授权
    Lead frame and lead frame material 失效
    引线框架和引线框架材料

    公开(公告)号:US5530283A

    公开(公告)日:1996-06-25

    申请号:US518529

    申请日:1995-08-23

    IPC分类号: H01L23/50 H01L23/495

    摘要: An object of the present invention is to provide a lead frame and a material for lead frame which insure excellent bonding and enables substantial reduction of time for production because such processes as plating are not required and furthermore are excellent in abration resistance.The present invention is characterized in that a silver layer having a construction where amplitude of a refracted ray refracted on the (200) surface is 1/3 or more of the amplitude of refracted X ray refracted on the (111) surface comprises an outer lead section of the base material for the lead frame. The base material is preferably copper, copper-alloy, iron, or iron alloy. The silver layer is formed, for instance, by means of silver plating, and the thickness is preferably in a range from 8 m to 30 m. An intermediate layer may be provided between a surface of the base material and the silver layer.

    摘要翻译: 本发明的目的是提供一种引线框架和引线框架材料,其确保良好的接合,并且能够显着缩短生产时间,因为不需要电镀等工艺,并且耐磨性也优异。 本发明的特征在于,具有在(200)表面折射的折射线的振幅为(111)面折射的折射X射线的振幅的1/3以上的结构的银层包括外引线 用于引线框架的基材的截面。 基材优选为铜,铜合金,铁或铁合金。 银层例如通过镀银形成,并且厚度优选在8μm至30μm的范围内。 可以在基材的表面和银层之间设置中间层。

    Metal gasket
    43.
    发明授权
    Metal gasket 有权
    金属垫片

    公开(公告)号:US08807573B2

    公开(公告)日:2014-08-19

    申请号:US13981218

    申请日:2012-01-12

    IPC分类号: F16J15/02 F16J15/08

    摘要: An annular metal gasket for sealing a space between members by being pressed in the vertical direction in a state of being mounted between the members, the metal gasket comprising an annular outer ring having a substantially C-shaped cross-section and having a circumferential-direction opening formed therein, and an annular inner ring fitted inside the outer ring. The inner ring is formed so as to have a polygonal cross-section. Bend parts having an Inner angle larger than 180° are formed between the upper corner part and the inner- and outer-circumference-side corner parts; and between the lower corner part and the inner- and outer-circumference-side corner parts.

    摘要翻译: 一种用于通过在安装在所述构件之间的状态下沿垂直方向被按压而在构件之间密封空间的环形金属衬垫,所述金属衬垫包括具有基本上C形横截面并具有圆周方向的环形外圈 开口形成在其中,以及安装在外圈内的环形内圈。 内圈形成为具有多边形横截面。 内角大于180°的弯曲部分形成在上角部与内周侧和外周侧角部之间; 并且在下角部与内周侧和外周侧角部之间。

    Welding method for fluorine-passivated memberfor welding, fluorine-passivated method after being weld, and welded parts priority data
    46.
    发明申请
    Welding method for fluorine-passivated memberfor welding, fluorine-passivated method after being weld, and welded parts priority data 失效
    用于焊接的氟钝化件的焊接方法,焊接后的氟钝化方法以及焊接部件优先数据

    公开(公告)号:US20050011935A1

    公开(公告)日:2005-01-20

    申请号:US10805555

    申请日:2004-03-19

    摘要: The present invention provides a welding method for materials to be welded which are subjected to fluoride passivation treatment, and a fluoride passivation retreatment method, wherein, when fluoride passivation retreatment was conducted after welding, there is no generation of particles or dust, and superior resistance is provided to fluorine system gases. In the present invention, when materials to be welded comprising stainless steel subjected to fluoride passivation treatment are welded, hydrogen is added to the gas (the back shield gas) flowing through the materials to be welded. Furthermore, in the welding method for materials to be welded which are subjected to fluoride passivation treatment in accordance with the present invention, the thickness of the fluoride passivated film in a predetermined range from the butt end surfaces of the materials to be welded, comprising stainless steel subjected to a fluoride passivation treatment, is set to 10 nm or less, and welding is conducted. Furthermore, in the fluoride passivation retreatment method in accordance with the present invention, after conducting the welding method described above, at least the welded parts are heated, and a gas containing fluorine gas is caused to flow in the interior part.

    摘要翻译: 本发明提供一种待进行氟化物钝化处理的待焊接材料的焊接方法,以及氟化物钝化再处理方法,其中,在焊接后进行氟化物钝化再处理时,不产生颗粒或灰尘,且具有优异的电阻 被提供给氟系气体。 在本发明中,当焊接包含不锈钢的待焊接材料进行氟化物钝化处理时,向流过待焊接材料的气体(背面保护气体)添加氢。 此外,在根据本发明的被氟化物钝化处理的待焊接材料的焊接方法中,氟化钝化膜的厚度在待焊接材料的对接端面的预定范围内,包括不锈钢 进行氟化物钝化处理的钢被设定为10nm以下,进行焊接。 此外,在本发明的氟化物钝化再处理方法中,在进行了上述的焊接方法之后,至少加热了焊接部,并且使含有氟气的气体在内部流动。

    Welding method for welded members subjected to fluoride passivation treatment, fluoride passivation retreatment method, and welded parts
    47.
    发明授权
    Welding method for welded members subjected to fluoride passivation treatment, fluoride passivation retreatment method, and welded parts 失效
    氟化物钝化处理焊接件的焊接方法,氟化物钝化再处理方法和焊接部件

    公开(公告)号:US06818320B2

    公开(公告)日:2004-11-16

    申请号:US09748883

    申请日:2000-12-27

    IPC分类号: B21D3900

    摘要: A welding method for materials to be welded which are subjected to fluoride passivation treatment, and a fluoride passivation retreatment method, wherein, when fluoride passivation retreatment is conducted after welding, there is no generation of particles or dust. The method provides superior resistance to fluorine system gases. During fluoride passivation treatment, hydrogen is added to the gas (the back shield gas) flowing through the materials to be welded. In one embodiment of the welding method, the thickness of the fluoride passivated film in a predetermined range from the butt end surfaces of the materials to be welded is set to 10 nm or less, followed by subsequent welding. Furthermore, the fluoride passivation retreatment method, includes the steps of heating at least the welded parts following welding and flowing a gas containing fluorine gas in the interior portion of the parts.

    摘要翻译: 对经过氟化物钝化处理的待焊接材料的焊接方法以及氟化物钝化再处理方法,其中,在焊接后进行氟化物钝化再处理时,不产生颗粒或灰尘。 该方法提供了优异的耐氟体系气体阻力。 在氟化物钝化处理期间,将氢气流入待焊接材料的气体(背面保护气体)。 在焊接方法的一个实施例中,氟化钝化膜在待焊接材料的对接端面的预定范围内的厚度设定为10nm以下,随后进行焊接。 此外,氟化物钝化再处理方法包括以下步骤:至少在焊接之后加热焊接部分,并且在部件的内部部分使含有氟气的气体流动。

    Long life welding electrode and its fixing structure, welding head, and welding method
    48.
    发明授权
    Long life welding electrode and its fixing structure, welding head, and welding method 有权
    长寿命焊接电极及其固定结构,焊接头和焊接方法

    公开(公告)号:US08420974B2

    公开(公告)日:2013-04-16

    申请号:US10266480

    申请日:2002-10-08

    IPC分类号: B23K9/16 B23K9/24

    摘要: A fixing structure for a welding electrode and a welding head is shown which enable improvement of durability of a welding electrode, improvement of work efficiency in welding, and a reduction of time required for welding and also which make it possible to execute welding for an extended time with high reliability. In the fixing structure, a fixed section of a welding electrode is inserted via a thermally conductive material into an inserting section of a fixing base and a peripheral surface of the fixed section of the welding electrode is uniformly contacted to the fixing base to affix the welding electrode to the fixing base.

    摘要翻译: 示出了用于焊接电极和焊接头的固定结构,其能够提高焊接电极的耐久性,提高焊接中的工作效率,并且减少焊接所需的时间,并且还可以执行用于扩展的焊接 时间高可靠性。 在固定结构中,焊接电极的固定部分经由导热材料插入到固定基座的插入部分中,并且焊接电极的固定部分的周面与固定基座均匀接触以固定焊接 电极到固定基座。

    Gas production facility, gas supply container, and gas for manufacture of electronic devices
    49.
    发明申请
    Gas production facility, gas supply container, and gas for manufacture of electronic devices 审中-公开
    天然气生产设备,气体供应容器和用于制造电子设备的气体

    公开(公告)号:US20110124928A1

    公开(公告)日:2011-05-26

    申请号:US12929271

    申请日:2011-01-12

    CPC分类号: C23C30/00 C23C4/11 C23C8/02

    摘要: An apparatus for producing a gas using a raw material gas having high reactivity, in particular, a fluorinated hydrocarbon, or a vessel for supplying the gas, characterized in that the surface of a portion thereof contacting with the gas has an average roughness of 1 μm or less in terms of a center line average roughness Ra. It is preferred that an oxide-based passivated film such as a film based on chromium oxide, aluminum oxide, yttrium oxide, magnesium oxide or the like is formed on the surface having a roughness controlled as above. The above apparatus and vessel can be suitably used for preventing the contamination of a raw material gas originated from a gas production apparatus or a vessel for supplying the gas.

    摘要翻译: 使用反应性高的原料气体,特别是氟化烃或用于供给气体的容器来制造气体的装置,其特征在于,与气体接触的部分的表面的平均粗糙度为1μm 或更小的中心线平均粗糙度Ra。 优选在具有如上控制的粗糙度的表面上形成氧化物基钝化膜,例如基于氧化铬,氧化铝,氧化钇,氧化镁等的膜。 上述设备和容器可适用于防止源自气体生产设备或用于供应气体的容器的原料气体的污染。

    Backlight unit for liquid crystal display
    50.
    发明授权
    Backlight unit for liquid crystal display 失效
    背光单元用于液晶显示

    公开(公告)号:US07787076B2

    公开(公告)日:2010-08-31

    申请号:US11989424

    申请日:2006-07-21

    IPC分类号: G02F1/1335

    摘要: As a shape on a cross-section vertical to a longitudinal direction (L) of the hot cathode fluorescent lamp (20a (20b)), a light source rear side reflecting plane (62) of a reflector (60) includes a mound portion (623). The mound portion (623) is defined by two recessed inclining planes and protrudes toward a hot cathode fluorescent lamp (20a (20b)).

    摘要翻译: 作为垂直于热阴极荧光灯(20a(20b))的纵向(L)的横截面的形状,反射器(60)的光源后侧反射面(62)包括墩部( 623)。 墩部(623)由两个凹入的倾斜平面限定,朝向热阴极荧光灯(20a(20b))突出。