Abstract:
Disclosed is an expanded polypropylene copolymer resin particle whose base resin is a polypropylene random copolymer resin having a melting point of not more than 145° C., the base resin having a H/W ratio of not more than 8 where H (%) is a maximum height of an elution peak and W (° C.) is a peak width at half a height of the peak in an elution curve obtained from a differential value of eluted content measured by cross fractionation chromatography, and a ratio (Mw/Mn) of a weight-average molecular weight (Mw) and a number-average molecular weight (Mn) being not less than 3.5 in a molecular weight distribution measurement of a whole of eluted components. With such an expanded polypropylene copolymer resin particle, it is possible to provide expanded polypropylene copolymer resin particles which are capable of producing an in-mold expansion-molded article with a low molding heating vapor pressure, and which causes few deformation or shrinkage of an obtained in-mold expansion-molded article (i.e. having a broad molding heating temperature range) even if the in-mold expansion molding is carried out with a high molding heating vapor pressure and has a low decrease in physical properties such as compression strength.
Abstract:
A polypropylene resin composition that has a melt flow rate of 1.5 (g/10 minutes) or more and is obtainable by melt-kneading 94 to 98 parts by weight of (A) a propylene copolymer that comprises a polymer portion being obtainable by polymerizing monomers containing propylene as the major component and having an intrinsic viscosity of 2.0 (dL/g) or more and a copolymer portion being obtainable by copolymerizing propylene and ethylene, 2 to 6 parts by weight of (B) an ethylene polymer having a density of 0.920 g/cm3 or more, and (C) an organic peroxide, provided that the total weight of the propylene copolymer (A) and the ethylene polymer (B).
Abstract translation:一种聚丙烯树脂组合物,其熔体流动速率为1.5(g / 10分钟)以上,通过熔融混炼得到94〜98重量份的(A)丙烯共聚物,该丙烯共聚物包含聚合物部分,该聚合物部分可通过聚合单体 含有丙烯作为主要成分,特性粘度为2.0(dL / g)以上,共聚物部分可通过丙烯与乙烯共聚获得,2〜6重量份的(B)密度为0.920的乙烯聚合物 g / cm 3以上,(C)有机过氧化物,前提是丙烯共聚物(A)和乙烯聚合物(B)的总重量。
Abstract:
The present subject matter relates to processes for irradiating visbroken propylene polymer compositions or extrudates of propylene polymer compositions containing a propylene polymer having a low polydispersity index and a non-phenolic stabilizer.
Abstract:
A polypropylene film comprising 70-90 wt. % polymer (a), 2-10 wt. % polymer (b), 2-10 wt. % polymer (c) and 3-20 wt. % polymer (d) and having a haze of 8-30% (wherein the polymer (a) is a block copolymer prepared by producing a polymer part (component a1) by polymerizing in a first step monomers composed mainly of propylene in the absence of an inert solvent and producing an ethylene/propylene copolymer part (component a2) in a second step by polymerization subsequently carried out in a gas phase; the polymer (b) is an ethylene-based polymer having a density of 0.91-0.97 g/cm3 and a melt flow rate of 5-30 g/10 min; the polymer (c) is an ethylene/α-olefin random copolymer having a density of 0.86-0.90 g/cm3 and a melt flow rate of 0.3-5 g/10 min; and the polymer (d) comprises two or more propylene-based polymers different in molecular weight from each other).
Abstract:
The invention provides for a film including a layer made from a composition, the composition produced from 30 percent by weight or more of a first polymer component (FPC), wherein said FPC includes a copolymer of propylene and from 6 to 30 percent by weight of another alpha-olefin, and having a melting point derived from stereoregular polypropylene sequences, as determined by differential scanning calorimetry (DSC) of 105° C. or less, and a heat of fusion of 45 J/g or less; and a second polymer component (SPC); wherein the SPC includes a thermoplastic polymer other than the FPC.
Abstract:
A polypropylene-based resin composition comprising 61 to 85% by weight of a copolymer (X) of propylene, α-olefin having 4 or more of carbon atoms and/or ethylene, in which a content of a constitutional unit derived from propylene is 86 to 97% by weight, a total of a content of a constitutional unit derived from ethylene and a content of a constitutional unit derived from α-olefin having 4 or more of carbon atoms is 3 to 14% by weight, provided that a total of the content of a constitutional unit derived from propylene, the content of a constitutional unit derived from ethylene and the content of a constitutional unit derived from α-olefin having 4 or more of carbon atoms is defined to be 100% by weight, 1 to 38% by weight of a copolymer (Y) of propylene and α-olefin having 4 or more of carbon atoms, in which a melting point is 115° C. or more, and a content of a constitutional unit derived from α-olefin having 4 or more of carbon atoms is 10 to 30% by weight, and 1 to 38% by weight of a copolymer (Z) of propylene and α-olefin having 4 or more of carbon atoms, in which a melting point is less than 115° C., and a content of a constitutional unit derived from α-olefin having 4 or more of carbon atoms is 30 to 40% by weight, wherein a total of the copolymer (X), the copolymer (Y) and the copolymer (Z) is defined to be 100% by weight.
Abstract:
An extruded air cooled blown film having a) a total thickness of 5 to 500 μm, b) a mono-layer structure or 2 to 9 coextruded layers, c) at least one layer L containing a polymer selected from the group consisting of polypropylene homopolymers, polypropylene random copolymers, hetero-phasic polypropylene block copolymers, or any mixtures thereof, said polymer having a melt flow rate, according to ASTM D-1238, of 0.1 to 10 dg/min at 230° C. and 2.16 kg, said layer L further containing 0.001 to 2%, relative to the weight of the polymer, of a particular nucleating agent, and optionally d) a Modulus according to EN ISO 527 enhanced by at least 10% versus a reference film without the nucleating agent.
Abstract translation:挤出空气冷却的吹塑薄膜,其具有a)总厚度为5至500μm,b)单层结构或2至9个共挤出层,c)至少一层含有选自聚丙烯均聚物 ,聚丙烯无规共聚物,异相聚丙烯嵌段共聚物或其任何混合物,根据ASTM D-1238,所述聚合物在230℃和2.16kg下的熔体流动速率为0.1-10dg / min,所述层 L还相对于聚合物的重量含有0.001至2%的特定成核剂,以及任选地d)根据EN ISO 527的模量相对于不含成核剂的参考膜增强至少10%。
Abstract:
A polymeric master batch for preparing an antimicrobal and antifungal and antiviral polymeric material comprising a slurry of thermoplastic resin, an antimicrobal and antifungal and antiviral agent consisting essentially of water insoluble particles of ionic copper oxide, a polymeric wax and an agent for occupying the charge of the ionic copper oxide.
Abstract:
Unique copolymers comprising propylene, ethylene and/or one or more unsaturated comonomers are characterized as having: at least one, preferably more than one, of the following properties: (i) 13C NMR peaks corresponding to a regio-error at about 14.6 and about 15.7 ppm, the peaks of about equal intensity, (ii) a B-value greater than about 1.4 when the comonomer content of the copolymer is at least about 3 wt %, (iii) a skewness index, Six, greater than about −1.20, (iv) a DSC curve with a Tme that remains essentially the same and a Tmax that decreases as the amount of comonomer in the copolymer is increased, and (v) an X-ray diffraction pattern that reports more gamma-form crystals than a comparable copolymer prepared with a Ziegler-Natta catalyst These polypropylene polymers are made using a nonmetallocene, metal-centered, heteroaryl ligand catalyst. These polymers can be blended with other polymers, and are useful in the manufacture of films, sheets, foams, fibers and molded articles.
Abstract:
Halogen-free, flame-retardant winding film made of polypropylene copolymers, useful for wrapping ventilation lines in air conditioning units, wires or cables and for bundling, insulating, marking, sealing or protecting.