摘要:
Process for preparing a catalyst for the oxidation of methanol to formaldehyde, comprising reacting iron powder and molybdenum trioxide in a Mo/Fe ratio from 1.5 to 5 in an aqueous suspension at temperatures from 20 to 100° C., and subsequently, optionally simultaneously, oxidizing the mixture with an oxidizing agent in a quantity equal to, or greater than the quantity required for the oxidation of the ferrous ion to ferric ion and to oxidize the molybdenum to the valence state 6.
摘要:
Catalysts for oxidation of methanol to formaldehyde, comprising a catalytic mixtures of Fe2(MoO4)3/MoO3, wherein the Mo/Fe atomic ratio ranges from 1.5 to 5, and a compound of cerium molybdenum and oxygen in a quantity from 0.1 to 10% by weight expressed as cerium.
摘要翻译:用于将甲醇氧化成甲醛的催化剂,其包含Fe 2 O 3(MoO 4 N 3)3 MoO 3的催化混合物 >其中Mo / Fe原子比为1.5〜5,铈钼和氧的化合物为0.1〜10重量%,表示为铈。
摘要:
A method for producing a high surface area iron material starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m2/g, and is prepared via a method which comprises reacting a low surface area iron metal with oxygen and an organic acid. The high surface area iron material formed via this method is essentially free of contaminants.
摘要:
A process for producing a high surface area iron material, comprising predominantly low crystalline iron oxides, starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m2/g, and is prepared via a method which comprises reacting a low surface area iron metal with oxygen and an organic acid. The high surface area iron material formed via this method is essentially free of contaminants.
摘要:
Catalysts for oxidation of methanol to formaldehyde, comprising a catalytic mixtures of Fe2(MoO4)3/MoO3, wherein the Mo/Fe atomic ratio ranges from 1.5 to 5, and a compound of cerium molybdenum and oxygen in a quantity from 0.1 to 10% by weight expressed as cerium.
摘要:
Method for removing nitrogen oxides NOx from gas mixtures that contain them, comprising contacting of the gas mixtures with an absorbent material comprising compounds having formula CaCuO2 and/or Ca0.83CuO2 providing X-ray diffraction powder spectra that correspond, for the CaCuO2 compound, to JCPDS card 48-197 and, for the Ca0.83 CuO2, to JCPDS card 48-212, or mixtures of said compounds or compositions containing them.
摘要翻译:包括从含有它们的气体混合物中除去氮氧化物的方法,包括使气体混合物与包含具有式CaCO 2和/或Ca的化合物的吸收材料接触 提供对于CaCl 2 O 2化合物对应于JCPDS卡48-197的X射线衍射粉末光谱,并且对于Ca 3 O 3, NCPC卡48-212,或所述化合物或含有它们的组合物的混合物。
摘要:
Highly pure iron oxides are prepared by reaction of metallic iron, in the form of microspheroidal particles or of scraps or cuttings, with an agitated aqueous solution of a mono- or polycarboxylic acid with a pKa of 0.5 to 6 relative to the first carboxyl and capable of decomposing, by heating in air at 200 to 350° C., to carbon dioxide and water, using 0.03 to 1.5 moles of acid per g-atoms of iron, a water/iron weight ration of 1 to 20, and by oxidation of the ferrous carboxilate to ferric salt, with an agent selected from oxygen, mixtures containing oxygen, hydrogen peroxide, organic peroxides and hydroperoxides.
摘要:
Catalysts in the form of cylindrical hollow granules, suitable for the dehydrogenation of ethylbenzene to styrene, and comprising, as active component, ferric oxide and promoters chosen among oxides of alkaline or alkaline-earth metals, oxides of elements of the lanthanide series, and chromium, tungsten, and molybdenum oxides, characterized by the absence of macroporosities with a radius of more than 50,000 .ANG. and/or by high mechanical characteristics of resistance to axial breaking and to abrasion.
摘要:
Highly pure iron oxides are prepared by reaction of metallic iron, in the form of microspheroidal particles or of scraps or cuttings, with an agitated aqueous solution of a mono- or polycarboxylic acid with a pKa of 0.5 to 6 relative to the first carboxyl and capable of decomposing, by heating in air at 200 to 350° C., to carbon dioxide and water, using 0.03 to 1.5 moles of acid per g-atoms of iron, a water/iron weight ration of 1 to 20, and by oxidation of the ferrous carboxilate to ferric salt, with an agent selected from oxygen, mixtures containing oxygen, hydrogen peroxide, organic peroxides and hydroperoxides.
摘要:
Process for preparing a catalyst for the oxidation of methanol to formaldehyde, comprising reacting iron powder and molybdenum trioxide in a Mo/Fe ratio from 1.5 to 5 in an aqueous suspension at temperatures from 20 to 100° C., and subsequently, optionally simultaneously, oxidizing the mixture with an oxidizing agent in a quantity equal to, or greater than the quantity required for the oxidation of the ferrous ion to ferric ion and to oxidize the molybdenum to the valence state 6.