Light-emitting diode
    1.
    发明申请
    Light-emitting diode 审中-公开
    发光二极管

    公开(公告)号:US20060261350A1

    公开(公告)日:2006-11-23

    申请号:US10554136

    申请日:2004-04-23

    IPC分类号: H01L33/00

    摘要: A light-emitting diode with high luminous efficiency is provided which is free from deformation or defects of a crystal caused by a dopant. The light-emitting diode emits no light of unnecessary wavelengths and has a wide selection of emission wavelengths. The light-emitting diode comprises a light-emitting layer made of an ambipolar semiconductor containing no dopant, and an electron implanting electrode, that is, an n-electrode and a hole implanting electrode, that is, a p-electrode joined to the light-emitting layer.

    摘要翻译: 提供了具有高发光效率的发光二极管,其没有由掺杂剂引起的晶体的变形或缺陷。 发光二极管不发出不必要的波长的光并具有广泛的发射波长选择。 发光二极管包括由不含掺杂剂的双极半导体制成的发光层,以及电子注入电极,即n电极和空穴注入电极,即与光接合的p电极 发光层。

    WDM optical filter and glass substrate for use in the WDM optical filter
    2.
    发明授权
    WDM optical filter and glass substrate for use in the WDM optical filter 失效
    WDM光学滤波器和用于WDM光学滤波器的玻璃基板

    公开(公告)号:US06465105B1

    公开(公告)日:2002-10-15

    申请号:US09630775

    申请日:2000-08-02

    IPC分类号: B32B1706

    摘要: A glass substrate is for use in a WDM optical filter which has an optical multilayer coated on the glass substrate and is formed by glass which has a composition related to the optical multilayer so as to assure stable multiplexing/demultiplexing operation in the optical filter. The glass includes SiO2 as a glass network-former and has an average linear thermal expansion coefficient between 100×10−7/K and 130×10−7/K within a temperature range between −30° C. and +70° C. The glass may include TiO2, Al2O3, and R2O (R: alkali metal element) in addition to SiO2 and may have a hardness suitable for the optical multilayer.

    摘要翻译: 玻璃基板用于WDM光学滤波器,其具有涂覆在玻璃基板上的光学多层膜,并且由具有与光学多层相关的组成的玻璃形成,从而确保滤光器中的稳定的多路复用/解复用操作。 该玻璃包括SiO 2作为玻璃网络形成剂,并且在-30℃至+ 70℃之间的温度范围内具有100×10 -7 / K至130×10 -7 / K之间的平均线性热膨胀系数。玻璃可包括 TiO 2,Al 2 O 3和R 2 O(R:碱金属元素),并且可以具有适合于光学多层的硬度。

    Quantum Dot-Dispersed Light Emitting Device, and Manufacturing Method Thereof
    3.
    发明申请
    Quantum Dot-Dispersed Light Emitting Device, and Manufacturing Method Thereof 失效
    量子点分散发光器件及其制造方法

    公开(公告)号:US20080122341A1

    公开(公告)日:2008-05-29

    申请号:US10587029

    申请日:2005-01-20

    IPC分类号: H01J1/63

    摘要: A light emitting device having practical light emission characteristics is obtained without epitaxial growth.A quantum dot-dispersed light emitting device of the invention includes a substrate 11, an electron injection electrode 12, a hole injection electrode 14, and an inorganic light emitting layer 13 disposed so as to be in contact with both the electrodes. The inorganic light emitting layer 13 contains an ambipolar inorganic semiconductor material and nanocrystals 15 dispersed as luminescent centers in the ambipolar inorganic semiconductor material and is configured so as to be capable of light emission without having, at the interface with the electron injection electrode and/or the hole injection electrode, epitaxial relation therewith.

    摘要翻译: 获得具有实际发光特性的发光器件,而不需外延生长。 本发明的量子点分散发光器件包括基板11,电子注入电极12,空穴注入电极14和与两个电极接触的无机发光层13。 无机发光层13含有双极性无机半导体材料和作为发光中心分散在双极性无机半导体材料中的纳米晶体15,并且被配置为能够在与电子注入电极和/或电子注入电极的界面处发光 空穴注入电极,与其外延关系。

    Light-emitting device of field-effect transistor type
    4.
    发明申请
    Light-emitting device of field-effect transistor type 失效
    场效晶体管型发光器件

    公开(公告)号:US20060043380A1

    公开(公告)日:2006-03-02

    申请号:US10505051

    申请日:2003-02-18

    IPC分类号: H01L33/00

    摘要: A theme is to provide a field-effect light-emitting device that can obtain a long-term reliability and broaden a selectivity of emission wavelength. The invention of this application is a field-effect transistor type light-emitting device having an electron injection electrode, i.e. a source electrode, a hole injection electrode, i.e. a drain electrode, an emission active member disposed between the source electrode and the drain electrode so as to contact with both electrodes, and a field application electrode, i.e. a gate electrode, for inducing electrons and holes in the emission active member, which is disposed in the vicinity of the emission active member via an electrically insulating member or an insulation gap. The emission active member is made of an inorganic semiconductor material having both an electron transporting property and a hole transporting property.

    摘要翻译: 主题是提供可以获得长期可靠性并扩大发射波长的选择性的场效应发光器件。 本申请的发明是一种场效应晶体管型发光器件,其具有电子注入电极,即源电极,空穴注入电极,即漏电极,设置在源电极和漏电极之间的发射有源元件 以及与两个电极接触的场施加电极,即用于在发射有源部件中诱发电子和空穴的场施加电极,其经由电绝缘部件或绝缘间隙设置在发射有源部件附近 。 发射有源部件由具有电子传输性和空穴传输性的无机半导体材料制成。

    Optical glass, glass material for press molding, optical element, and method of manufacturing same
    5.
    发明授权
    Optical glass, glass material for press molding, optical element, and method of manufacturing same 有权
    光学玻璃,压模用玻璃材料,光学元件及其制造方法

    公开(公告)号:US08479539B2

    公开(公告)日:2013-07-09

    申请号:US11315317

    申请日:2005-12-23

    IPC分类号: C03B25/00

    CPC分类号: C03C3/062 Y10S501/901

    摘要: A method of making a press-moldable glass, including melting starting materials, forming a melt, and annealing a formed glass, wherein the melt has a composition such that, (1) when rapidly cooled to room temperature, it becomes glass that has a scattering coefficient of less than 0.005 cm−1 at wavelengths of from 400 to 2,500 nm or comprises crystals with a volumetric ratio of less than 10−6, and (2) when maintained for three hours at a temperature 10° C. higher than the glass transition temperature, maintained for 10 min at a temperature yielding a viscosity of 104.5 to 103.5 dPa·s, and then rapidly cooled to room temperature, (3) the resulting glass has (a) a scattering coefficient of at least one wavelength from 400 to 2,500 nm of greater than 0.01 cm−1 or (b) crystals with a volumetric ratio of greater than 10−5. A temperature for annealing is lower than for glass transition.

    摘要翻译: 一种制造可压制玻璃的方法,包括熔融起始材料,形成熔体并退火成形的玻璃,其中熔体具有如下组成:(1)当快速冷却至室温时,其变为具有 在波长为400至2500nm的散射系数小于0.005cm -1,或包含体积比小于10-6的晶体,和(2)当在比10℃高10℃的温度下保持3小时时 玻璃化转变温度,在104.5〜103.5dPa·s的粘度下保持10分钟,然后迅速冷却至室温,(3)得到的玻璃的(a)至少一个波长的散射系数为400 到2500nm大于0.01cm -1或(b)体积比大于10-5的晶体。 退火温度低于玻璃化转变温度。

    DICHROIC DYE-CONTAINING LIQUID, AND POLARIZER
    6.
    发明申请
    DICHROIC DYE-CONTAINING LIQUID, AND POLARIZER 审中-公开
    含二氧化碳的含液体和极化剂

    公开(公告)号:US20130050823A1

    公开(公告)日:2013-02-28

    申请号:US13638278

    申请日:2011-03-29

    CPC分类号: G02B5/3041 C08K5/0041

    摘要: To provide a dichroic dye-containing liquid that is capable of preventing haze without decrease of adhesiveness of a polarizing layer, and a polarizer.The dichroic dye-containing liquid contains (A) a dichroic dye and (B) a toughness-imparting agent, in which the dichroic dye (A) and the toughness-imparting agent (B) are dispersed or dissolved in an aqueous medium, and a solid content X (% by mass) of the toughness-imparting agent (B) based on the dichroic dye-containing liquid and a 100% modulus Y (MPa) of the toughness-imparting agent (B) satisfy relationships represented by the following expressions (1) and (2): 0.01≦X≦1.0  (1) Y≦0.14X−1.5  (2) and the polarizer contains a substrate having provided sequentially thereon an orientation layer and a polarizing layer, in which the polarizing layer containing a dichroic dye that is oriented and accumulated by using the dichroic dye-containing liquid.

    摘要翻译: 提供能够防止雾度而不降低偏振层的粘附性的二色性含染料液体和偏振片。 二色性染料的液体含有(A)二色性染料和(B)赋予二色性染料(A)和韧性赋予剂(B)在水性介质中分散或溶解的韧性赋予剂, 基于二色性染料的液体的韧性赋予剂(B)的固体成分X(质量%)和韧性赋予剂(B)的100%模量Y(MPa)满足以下的关系 表达式(1)和(2):0.01≦̸ X< ll; 1.0(1)Y< lI; 0.14X-1.5(2),并且所述偏振器包含顺序地设置有取向层和偏振层的基板, 含有通过使用含二色性染料的液体取向和累积的二色性染料。

    PROCESS FOR PRODUCING POLARIZING ELEMENT
    8.
    发明申请
    PROCESS FOR PRODUCING POLARIZING ELEMENT 审中-公开
    生产极化元件的工艺

    公开(公告)号:US20100104745A1

    公开(公告)日:2010-04-29

    申请号:US12603915

    申请日:2009-10-22

    IPC分类号: B05D5/06

    CPC分类号: G02B5/3033 G02B1/105 G02B1/14

    摘要: A process for producing a polarizing element which comprises steps of treating a mixture comprising (A) an alkoxysilane and/or a hexaalkoxydisiloxane, (B) water and (C) an alcohol by heating under a condition of at 40 to 120° C. for 0.5 to 24 hours to prepare a coating solution for an alignment film, coating a substrate with the coating solution for an alignment film prepared above to prepare a sol-gel film, treating the sol-gel film by abrasion in a uniaxial direction to form an alignment layer having marks of abrasion in the uniaxial direction, aligning a dichroic coloring agent on the formed alignment layer by deposition to form a polarizing layer, and forming a protective layer for fixing the coloring agent on the formed polarizing layer. A polarizing element can be produced in simple steps, and separation of the polarizing layer in the steps of the production can be prevented.

    摘要翻译: 一种偏振元件的制造方法,其特征在于,在40〜120℃的条件下,对(A)烷氧基硅烷和/或六烷氧基二硅氧烷,(B)水和(C))醇进行处理, 0.5至24小时以制备用于取向膜的涂布溶液,用上述制备的取向膜用涂布液涂布基材以制备溶胶 - 凝胶膜,通过在单轴方向上的磨损处理溶胶 - 凝胶膜以形成 对准层在单轴方向上具有磨损标记,通过沉积将形成的取向层上的二色性着色剂取向以形成偏振层,并且在形成的偏振层上形成用于固色着色剂的保护层。 可以简单的步骤制造偏振元件,并且可以防止在生产步骤中偏振层的分离。

    Optical glass, glass material for press molding, optical element, and method of manufacturing same

    公开(公告)号:US07015164B2

    公开(公告)日:2006-03-21

    申请号:US10270303

    申请日:2002-10-15

    IPC分类号: C03C3/062

    CPC分类号: C03C3/062 Y10S501/901

    摘要: Disclosed is an optical glass comprising, expressed as weight percentages, greater than or equal to 18 percent and less than 30 percent of SiO2, greater than or equal to 12 percent and less than 23 percent of BaO, 22 to 37 percent TiO2, greater than or equal to 7 percent and less than 16 percent Nb2O5, 5 to 20 percent of Na2O, 0 to 6 percent of K2O, 0 to 5 percent of CaO, 0 to 5 percent of SrO, 0 to 4 percent of ZrO2, 0 to 3 percent of Ta2O5, 0 to 1 percent of Sb2O5, and greater than or equal to 0 percent and less than 0.5 percent of P2O5, and by essentially not comprising PbO, As2O3, and F. The optical glass exhibits a refractive index (nd) greater than or equal to 1.80 and an Abbé number (vd) less than or equal to 30. A method of manufacturing a glass material for press molding is disclosed. This method comprises the steps of melting the glass starting materials, forming the glass melt obtained, and annealing the formed glass and is characterized in that: the glass melt has a composition such that, (1) when rapidly cooled to room temperature, said glass melt becomes glass that has a scattering coefficient of less than 0.005 cm−1 at wavelengths of from 400 to 2,500 nm or comprises crystals with a volumetric ratio of less than 10−6, and (2) when maintained for three hours at a temperature 10° C. higher than the glass transition temperature, maintained for 10 min at a temperature yielding a viscosity of 104.5 to 103.5 dPa·s, and then rapidly cooled to room temperature, said glass melt becomes glass that has a scattering coefficient at at least one wavelength from 400 to 2,500 nm of greater than 0.01 cm−1 or comprises crystals with a volumetric ratio of greater than 10−5; and an annealing of said formed glass is conducted at a temperature lower than the glass transition temperature.

    Laser glasses and laser glass fibers
    10.
    发明授权
    Laser glasses and laser glass fibers 失效
    激光眼镜和激光玻璃纤维

    公开(公告)号:US5764661A

    公开(公告)日:1998-06-09

    申请号:US562601

    申请日:1995-11-24

    摘要: Disclosed are laser glasses composed of a Ga--Na--S glasses doped with one or more kinds of activating ions, laser glass fibers comprising a core and a clad wherein the core is composed of the above-mentioned laser glasses of the present invention and optical fiber amplifiers comprising a pumping source, a laser glass fiber and a means for introducing pumping light and signal light into the laser glass fiber wherein the laser glass fiber is the above-mentioned laser glass fiber of the present invention. The laser glasses of the present invention show high radiative quantum efficiency and host glass stability and can be produced easily.

    摘要翻译: 公开了由掺杂有一种或多种活化离子的Ga-Na-S玻璃组成的激光玻璃,包括芯和激光玻璃纤维,其中芯由本发明的上述激光玻璃和光学 光纤放大器包括泵浦源,激光玻璃纤维和用于将激光和信号光引入激光玻璃纤维的装置,其中激光玻璃纤维是本发明的上述激光玻璃纤维。 本发明的激光玻璃显示出高的辐射量子效率和主体玻璃的稳定性,并且可以容易地制造。