Process for Preparing Barium Titanate
    2.
    发明申请
    Process for Preparing Barium Titanate 失效
    制备钛酸钡的方法

    公开(公告)号:US20090202425A1

    公开(公告)日:2009-08-13

    申请号:US11989856

    申请日:2006-08-01

    IPC分类号: C01G23/00

    摘要: The present invention relates to a hydrothermal synthesis for preparing barium titanate powder as the essential material for a multi-layer ceramic capacitor. The object of the invention is to prepare barium titanate powder having high purity, particle size of submicron order, uniform particle distribution and excellent crys tallinity , by reacting hydrous titanic acid compound prepared via sulfuric acid process with crystalline titanium oxide and barium hydroxide, as the starting material, at a temperature between 60° C. and 300° C. under a pressure between 5 Kgf/cm2 and 50 Kgf/cm2. The process for preparing barium titanate according to the present invention provides barium titanate powder having Ba/Ti molar ratio of 1.000±0.002 and high purity by applying calcination under reductive condition to the solid product obtained from hydrous titanic acid compound prepared via sulfuric acid process with crystalline titanium oxide and barium hydroxide, as the starting substances, to convert barium sulfate, which was produced from residual sulfide in the raw material, to barium titanate.

    摘要翻译: 本发明涉及一种制备钛酸钡粉末作为多层陶瓷电容器的基本材料的水热合成方法。 本发明的目的是通过使通过硫酸方法制备的含水钛酸化合物与结晶二氧化钛和氢氧化钡反应,制备具有高纯度,亚微米级数,粒子分布均匀和优异的结晶度的钛酸钡粉末,作为 起始材料,温度为60℃至300℃,压力为5Kgf / cm2至50Kgf / cm2。 根据本发明的制备钛酸钡的方法通过在还原条件下对从通过硫酸方法制备的含水钛酸化合物获得的固体产物进行煅烧,提供具有1.000±0.002的Ba / Ti摩尔比的钛酸钡粉末和高纯度, 结晶二氧化钛和氢氧化钡作为起始物质,将由原料中的残留硫化物生成的硫酸钡转化为钛酸钡。

    Process for preparing barium titanate
    4.
    发明授权
    Process for preparing barium titanate 失效
    制备钛酸钡的方法

    公开(公告)号:US07854916B2

    公开(公告)日:2010-12-21

    申请号:US11989856

    申请日:2006-08-01

    IPC分类号: C01G23/00 C01F11/02

    摘要: The present invention relates to a hydrothermal synthesis for preparing barium titanate powder as the essential material for a multi-layer ceramic capacitor. The object of the invention is to prepare barium titanate powder having high purity, particle size of submicron order, uniform particle distribution and excellent crystallinity, by reacting hydrous titanic acid compound prepared via sulfuric acid process with crystalline titanium oxide and barium hydroxide, as the starting material, at a temperature between 60° C. and 300° C. under a pressure between 5 Kgf/cm2 and 50 Kgf/cm2. The process for preparing barium titanate according to the present invention provides barium titanate powder having Ba/Ti molar ratio of 1.000±0.002 and high purity by applying calcination under reductive condition to the solid product obtained from hydrous titanic acid compound prepared via sulfuric acid process with crystalline titanium oxide and barium hydroxide, as the starting substances, to convert barium sulfate, which was produced from residual sulfide in the raw material, to barium titanate.

    摘要翻译: 本发明涉及一种制备钛酸钡粉末作为多层陶瓷电容器的基本材料的水热合成方法。 本发明的目的是通过使通过硫酸方法制备的含水钛酸化合物与结晶二氧化钛和氢氧化钡作为起始物来制备具有高纯度,亚微米级数,亚微米粒径分布和优异结晶度的钛酸钡粉末 材料,在5kgf / cm 2至50Kgf / cm 2之间的压力下在60℃至300℃的温度下进行。 根据本发明的制备钛酸钡的方法通过在还原条件下对从通过硫酸方法制备的含水钛酸化合物获得的固体产物进行煅烧,提供具有1.000±0.002的Ba / Ti摩尔比的钛酸钡粉末和高纯度, 结晶二氧化钛和氢氧化钡作为起始物质,将由原料中的残留硫化物生成的硫酸钡转化为钛酸钡。