METHOD OF FABRICATING A COMPONENT USING A FUGITIVE COATING
    2.
    发明申请
    METHOD OF FABRICATING A COMPONENT USING A FUGITIVE COATING 审中-公开
    使用消耗性涂料来制造组分的方法

    公开(公告)号:US20120114868A1

    公开(公告)日:2012-05-10

    申请号:US12943563

    申请日:2010-11-10

    摘要: A method of fabricating a component is provided. The method includes depositing a fugitive coating on a surface of a substrate, where the substrate has at least one hollow interior space. The method further includes machining the substrate through the fugitive coating to form one or more grooves in the surface of the substrate. Each of the one or more grooves has a base and extends at least partially along the surface of the substrate. The method further includes forming one or more access holes through the base of a respective one of the one or more grooves to connect the respective groove in fluid communication with the respective hollow interior space. The method further includes filling the one or more grooves with a filler, removing the fugitive coating, disposing a coating over at least a portion of the surface of the substrate, and removing the filler from the one or more grooves, such that the one or more grooves and the coating together define a number of channels for cooling the component.

    摘要翻译: 提供了一种制造组件的方法。 该方法包括在衬底的表面上沉积短片,其中衬底具有至少一个中空的内部空间。 该方法还包括通过短暂涂层来加工衬底以在衬底的表面中形成一个或多个凹槽。 所述一个或多个凹槽中的每一个具有基部并至少部分地沿着所述基底的表面延伸。 该方法还包括通过一个或多个凹槽中的相应一个凹槽的基部形成一个或多个访问孔,以将相应的沟槽与相应的中空内部空间流体连通。 该方法还包括用填充物填充一个或多个凹槽,去除短暂涂层,在基底的表面的至少一部分上设置涂层,以及从一个或多个凹槽中移除填料,使得一个或多个凹槽 更多的凹槽和涂层一起限定了用于冷却部件的多个通道。

    WELDING PROCESS AND CORROSION-RESISTANT FILLER ALLOY AND CONSUMABLES THEREFOR
    3.
    发明申请
    WELDING PROCESS AND CORROSION-RESISTANT FILLER ALLOY AND CONSUMABLES THEREFOR 审中-公开
    焊接工艺和耐腐蚀填料合金及其消耗品

    公开(公告)号:US20110240715A1

    公开(公告)日:2011-10-06

    申请号:US12751177

    申请日:2010-03-31

    IPC分类号: B23K31/02 C22C19/05

    摘要: A nickel-based alloy and welding processes and consumables that use the alloy as a weld filler metal to fabricate, weld overlay, and repair components, including components of nuclear power plant reactors that contact the hot coolant water of the reactor. The nickel-based alloy consists of, by weight, 26 to about 30% chromium, 2 to about 4% iron, 2 to about 4% manganese, 2 to about 3% niobium, 1 to about 3% molybdenum, not more than 0.6% titanium, not more than 0.03% carbon, not more than 0.05% nitrogen, not more than 0.6% aluminum, not more than 0.5% silicon, not more than 0.01% copper, not more than 0.02% phosphorus, not more than 0.01% sulfur, with the balance nickel and incidental impurities.

    摘要翻译: 使用合金作为焊接填料金属的镍基合金和焊接工艺和消耗品,以制造,焊接覆盖层和修复部件,包括接触反应堆的热冷却水的核电站反应堆的部件。 镍基合金以重量计包含26至约30%的铬,2至约4%的铁,2至约4%的锰,2至约3%的铌,1至约3%的钼,不超过0.6 %钛,不超过0.03%的碳,不超过0.05%的氮,不超过0.6%的铝,不超过0.5%的硅,不超过0.01%的铜,不超过0.02%的磷,不大于0.01% 硫,余量为镍和杂质。

    SURFACE MODIFIED MAGNETIC MATERIAL
    5.
    发明申请
    SURFACE MODIFIED MAGNETIC MATERIAL 审中-公开
    表面改性磁性材料

    公开(公告)号:US20130196145A1

    公开(公告)日:2013-08-01

    申请号:US13361334

    申请日:2012-01-30

    IPC分类号: B32B3/00 B05D3/10 B32B15/04

    摘要: An article exhibiting magnetic properties, a method for providing corrosion resistance to an article, and an electric machine element are disclosed. The article comprises a substrate comprising a first portion of a magnetic material, the magnetic material exhibiting magnetic properties. The article further comprises a transition layer comprising a second portion of the magnetic material and a first portion of a coating material. The transition layer is disposed on at least a portion of the substrate. The article further comprises an outer layer comprising a second portion of the coating material. The outer layer is disposed on at least a portion of the transition layer.

    摘要翻译: 本发明公开了一种具有磁特性的物品,对制品提供耐腐蚀性的方法以及电机元件。 所述制品包括包含磁性材料的第一部分的基底,所述磁性材料具有磁性。 该制品还包括包含磁性材料的第二部分和涂层材料的第一部分的过渡层。 过渡层设置在基板的至少一部分上。 该制品还包括包含涂层材料的第二部分的外层。 外层设置在过渡层的至少一部分上。

    CORROSION AND WEAR RESISTANT ORGANIC COATINGS
    9.
    发明申请
    CORROSION AND WEAR RESISTANT ORGANIC COATINGS 审中-公开
    腐蚀和耐磨有机涂料

    公开(公告)号:US20140037850A1

    公开(公告)日:2014-02-06

    申请号:US13596399

    申请日:2012-08-28

    IPC分类号: B05D3/02 B05D3/12

    摘要: The present invention provides a method of protecting refinery equipment, the method comprising: (a) applying an uncured organic coating comprising a curable epoxy phenol novolac resin and a curing agent comprising a vicinal primary diamine moiety to a surface of refinery equipment susceptible to corrosion and/or wear; and (b) curing the uncured coating to form a cured coating having a viscosity of at least 2,000,000 centipoise; wherein the uncured organic coating has a viscosity of less than 500,000 centipoise, and wherein the uncured coating is substantially free of components comprising secondary and tertiary amine groups, and wherein the uncured coating is characterized by a latent viscosity of at least 2,000,000 when cured for 1 hour at 50° C.

    摘要翻译: 本发明提供了一种保护炼油设备的方法,所述方法包括:(a)将包含可固化环氧苯酚酚醛清漆树脂的未固化有机涂层和包含邻位伯胺部分的固化剂施加到易于腐蚀的炼油设备的表面,以及 /或磨损; 和(b)固化未固化的涂层以形成粘度为至少2,000,000厘泊的固化涂层; 其中所述未固化的有机涂层具有小于500,000厘泊的粘度,并且其中所述未固化涂层基本上不含包含仲胺和叔胺基团的组分,并且其中所述未固化涂层的特征在于当固化1时的潜在粘度为至少2,000,000 小时在50°C