Emulsion water paint and process for its production using epoxy
acrylic-resolve resin blends
    1.
    发明授权
    Emulsion water paint and process for its production using epoxy acrylic-resolve resin blends 失效
    乳液水性涂料及其使用环氧丙烯酸树脂树脂的生产工艺

    公开(公告)号:US5110847A

    公开(公告)日:1992-05-05

    申请号:US632681

    申请日:1990-12-24

    Abstract: An o/w water paint having excellent dispersibility and stability is prepared according to a phase conversion process comprising adding ammonia or an amine and water to a solution of an epoxy resin, a hardener resin, and an acrylic resin in an organic solvent or to a molten mixture of these resins to neutralize the acrylic resin. In view of adhesion of a coat to metal and workability, branched alkylamines or heterocyclic amines are suitable as the neutralizing amines. In applying this paint, steam optionally containing fine water droplets is preferably applied to a wet coat prior to drying. Furthermore, a process for the continuous production of an emulsion type water paint comprising a carboxyl group-containing acrylic resin component, an epoxy resin component and a curing agent resin component for the epoxy resin is disclosed.

    Abstract translation: 根据相转化方法制备具有优异的分散性和稳定性的o / w水性涂料,其包括将氨或胺和水加入到有机溶剂中的环氧树脂,固化剂树脂和丙烯酸树脂的溶液中,或者 这些树脂的熔融混合物中和丙烯酸树脂。 考虑到涂层与金属的粘合性和可加工性,支链烷基胺或杂环胺适合作为中和胺。 在施加该涂料时,优选在干燥之前将潮湿的涂层施加任选地含有细小水滴的蒸汽。 此外,公开了连续制造包含含羧基的丙烯酸树脂组分,环氧树脂组分和用于环氧树脂的固化剂树脂组分的乳液型水性涂料的方法。

    Aqueous paint
    2.
    发明授权
    Aqueous paint 失效
    水性油漆

    公开(公告)号:US5763507A

    公开(公告)日:1998-06-09

    申请号:US770003

    申请日:1996-12-19

    CPC classification number: C09D151/08 C08F283/10

    Abstract: An aqueous paint which exhibits improved dispersion property in the water and dispersion stability, has a low viscosity enabling the painting operation to be efficiently carried out, and cures at low temperatures within short periods of time to form a coating which after cured exhibits high degree of workability, high corrosion resistance, and elutes out little into the content. The aqueous paint comprises an epoxy acrylate resin prepared by modifying, with a (meth)acrylic monomer, a copolymerized epoxy resin having a number average molecular weight of 8,000 to 15,000 and containing, as phenolic components, a bisphenol-A component and a bisphenol-F component at a molar ratio of from 5:5 to 8:2, and a curing agent of a thermosetting resin having a methylol group.

    Abstract translation: 表现出改善的水分散性和分散稳定性的水性涂料具有低粘度,能够有效地进行涂装操作,并且在短时间内在低温下固化形成涂层,其在固化后显示高度的 可加工性,耐腐蚀性高,并且内容很少洗脱。 水性涂​​料包括通过用(甲基)丙烯酸单体改性数均分子量为8,000至15,000的共聚环氧树脂制备的环氧丙烯酸酯树脂,并且作为酚类组分含有双酚A组分和双酚A组分, F组分,摩尔比为5:5至8:2的固化剂和具有羟甲基的热固性树脂的固化剂。

    Welded can and process for preparation thereof
    3.
    发明授权
    Welded can and process for preparation thereof 失效
    焊接罐及其制备方法

    公开(公告)号:US4477501A

    公开(公告)日:1984-10-16

    申请号:US443213

    申请日:1982-11-19

    Abstract: Disclosed is a coated welded can having a metal-exposed face inclusive of a seam covered with a coating, wherein the coating comprises at least one organic resin coating layer and at least one metal film, and at least the portion of the organic resin coating that adheres to the metal-exposed face is comprised of a copolymer of ethylene with a carbonyl group-containing, ethylenically unsaturated monomer or a blend containing this copolymer.In this coated welded can, the adhesion of the coating, the corrosion resistance of the seam and the appearance characteristics of the seam are highly improved. Furthermore, the coating of this welded can is not damaged by such processing as flanging, beading or double-seaming or when the welded can is subjected to the retort sterilization.

    Abstract translation: 公开了一种具有金属暴露面的涂覆焊接罐,其包括覆盖有涂层的接缝,其中所述涂层包括至少一个有机树脂涂层和至少一个金属膜,并且所述有机树脂涂层的至少一部分 粘附到金属暴露面上由乙烯与含羰基的烯属不饱和单体的共聚物或含有该共聚物的共混物组成。 在这种涂层焊接罐中,涂层的附着力,接缝的耐腐蚀性和接缝的外观特性得到了很大的改善。 此外,这种焊接的罐的涂层不会受到诸如凸缘,珠粒或双重接缝之类的处理或当焊接罐进行蒸煮灭菌时的损坏。

    Plastisol composition
    4.
    发明授权
    Plastisol composition 失效
    增塑剂组合物

    公开(公告)号:US5441994A

    公开(公告)日:1995-08-15

    申请号:US242843

    申请日:1994-05-16

    CPC classification number: C08F8/00 C08F2810/20 Y10S525/902

    Abstract: An acrylic resin plastisol composition that forms coatings or molded articles having excellent anticreep property. The plastisol composition maintains excellent fluidity required for the coating and molding even after preserved for extended periods of time and further exhibits excellent gelation property upon heating, enabling the obtained coating or the molded article to exhibit excellent resistance against the relaxation of stress. The plastisol composition comprises a dispersing medium composed chiefly of a plasticizer and acrylic resin grains dispersed in said dispersing medium, wherein said acrylic resin grains have a functional group selected from the group consisting of carboxyl group, hydroxyl group, epoxy group, methylol group and etherified methylol group, and said dispersing medium contains a crosslinking agent that has reactivity to said functional group in a state of being at least partly solubilized in said dispersing medium.

    Abstract translation: 一种形成具有优异抗蚀性能的涂料或模制品的丙烯酸树脂增塑溶胶组合物。 即使在长时间保存之后,增塑溶胶组合物也保持涂布和成型所需的优异的流动性,并且在加热时进一步显示出优异的凝胶化性能,使得所得到的涂层或模塑制品具有优异的抗应力松弛性。 增塑溶胶组合物包含主要由增塑剂组成的分散介质和分散在所述分散介质中的丙烯酸树脂颗粒,其中所述丙烯酸树脂颗粒具有选自羧基,羟基,环氧基,羟甲基和醚化的官能团 羟甲基,并且所述分散介质含有在至少部分溶解于所述分散介质中的状态下与所述官能团具有反应性的交联剂。

    Can end sealing rubber composition containing a styrene-butadiene
rubbery copolymer, a tackifier and a filler
    6.
    发明授权
    Can end sealing rubber composition containing a styrene-butadiene rubbery copolymer, a tackifier and a filler 失效
    可以封端含有苯乙烯 - 丁二烯橡胶共聚物,增粘剂和填料的密封橡胶组合物

    公开(公告)号:US4189418A

    公开(公告)日:1980-02-19

    申请号:US858208

    申请日:1977-12-07

    Abstract: A can end sealing rubber composition(A) consisting essentially of a styrene-butadiene rubbery copolymer, a tackifier and a filler, and(B) having (1) a creep resistance coefficient K defined by the following equation of at least 0.1 but not exceeding 0.6,K=log J.sub.90.sup.C (10)-log J.sub.90.sup.C (1) wherein J.sub.90.sup.C (10) is the creep compliance measured 10 minutes after exerting a load when a fabricated article of the composition as a specimen is compressed in water at 90.degree. C. by a parallel plate plastometer, and J.sub.90.sup.C (1) is the creep compliance measured 1 minute after exerting a load when the specimen is compressed in water at 90.degree. C. by a parallel plate plastomer,and (2) a creep compliance J.sub.25.sup.C (1) of at least 3.times.10.sup.-9 cm.sup.2 /dyne but not exceeding 1.times.10.sup.-6 cm.sup.2 /dyne, the creep compliance being measured 1 minute after exerting a load when the specimen is compressed in water at 25.degree. C. by a parallel plate plastometer.

    Abstract translation: 一种基本上由苯乙烯 - 丁二烯橡胶共聚物,增粘剂和填料组成的罐端密封橡胶组合物(A)和(B)具有(1)由下式定义的抗蠕变系数K至少为0.1但不超过 0.6,K = log J90C(10)-log J90C(1)其中J90C(10)是在作为样品的组合物的制品在90℃的水中压缩时施加负荷后10分钟测量的蠕变柔量。 J90C(1)是当试样在90℃的水中通过平行板塑性体压缩后施加载荷1分钟后测得的蠕变柔量,(2)蠕变顺应性J25C(1) )为至少3×10 -9 cm 2 /达因但不超过1×10 -6 cm 2 /达因,当试样在25℃的水中通过平行平板式塑性计压缩时,在施加载荷1分钟后测量蠕变柔量。

    Acrylic plastisol adhesion structure
    8.
    发明授权
    Acrylic plastisol adhesion structure 失效
    丙烯酸增塑溶胶粘结结构

    公开(公告)号:US5677053A

    公开(公告)日:1997-10-14

    申请号:US671677

    申请日:1996-06-28

    Abstract: An adhesion structure in which the gel of an acrylic plastisol is strongly adhered to the metallic base material, featuring excellent resistance against corrosion and exhibiting small whitening tendency even under severe conditions for treatment with hot water such as retort processing, and a method of producing the same structure. The acrylic plastisol is applied onto the metallic base material or onto the metallic base material having an organic coating provided with a layer of a thermosetting resin which contains a bisphenol-type epoxy resin and a phenolic resin at a weight ratio of from 99:1 to 85:15, and is gelled by heating and is, at the same time, adhered to the base material via the thermosetting resin layer. The acrylic plastisol is gelled and is strongly adhered onto the thermosetting resin layer within short periods of time. The obtained adhesion structure exhibits excellent resistance against peeling, corrosion and retorting.

    Abstract translation: 丙烯酸增塑溶胶的凝胶强烈地粘附到金属基材上的粘合结构,即使在用于用诸如蒸馏处理的热水处理的苛刻条件下也具有优异的耐腐蚀性和显示出小的白化趋势的粘合结构,以及制备 相同的结构。 将丙烯酸增塑溶胶施加到金属基材或金属基材上,所述金属基材具有有机涂层,该有机涂层具有含有双酚型环氧树脂和酚醛树脂的热固性树脂层,重量比为99:1至 85:15,通过加热凝胶化,同时通过热固性树脂层附着在基材上。 丙烯酸增塑溶胶凝胶化,并在短时间内牢固地附着在热固性树脂层上。 获得的粘合结构表现出优异的抗剥离,腐蚀和蒸煮的性能。