公开(公告)号:US10669403B2
公开(公告)日:2020-06-02
申请号:US15419283
申请日:2017-01-30
Applicant: BASF SE
Inventor: Stephen Mark Andrews , Joseph James Fay , Roswell Easton King , Mohammad Zafar , Zhisheng Chen , Thomas Friend Thompson , Feng Zuo
IPC: C08K13/02 , C08K3/013 , C08K3/015 , E04D5/06 , E04F13/18 , E04D13/15 , C08K5/00 , C08K5/132 , C08K5/134 , C08K5/17 , C08K5/32 , C08K5/3475 , C08K5/3492 , C08K5/526 , C08L23/06 , C08L23/12 , B32B27/32 , C08K5/3435 , C08K3/22 , C08K3/26 , C08K3/34 , C08K5/053 , C08K5/138 , C08K5/52 , B32B7/02
Abstract: A polyolefin composition includes a polyolefin substrate having incorporated therein a nucleating agent and a filler, wherein the composition exhibits an impact strength of >35 in-lb measured according to ASTM D4226, and a coefficient of linear thermal expansion of
-
公开(公告)号:US10259931B2
公开(公告)日:2019-04-16
申请号:US15920877
申请日:2018-03-14
Applicant: BASF SE
Inventor: Werner Hoelzl , Bruno Rotzinger , Kai-Uwe Schoening , Roswell Easton King
IPC: C08K5/29 , C08K5/529 , C08K5/523 , C07F9/655 , C07F9/6574 , C08K5/04 , C08K5/5377 , C08K5/098
Abstract: The invention relates to a composition comprising an organic material susceptible to oxidative, thermal or light-induced degradation and a compound of formula I-P, I-O or I-M Further embodiments are a compound of formula I-P, I-O or I-M, a process for protection of the organic material by the compound, the use of the compound for stabilizing the organic material, an additive composition comprising the compound, a process for manufacturing the compound and intermediates involved therein.
-
公开(公告)号:US20140225038A1
公开(公告)日:2014-08-14
申请号:US14345998
申请日:2012-09-27
Applicant: BASF SE
Inventor: Jiong Yu , Roswell Easton King
CPC classification number: C08K5/134 , C08K5/1345 , C08K5/52 , C08K5/526
Abstract: The present invention relates to two processes for providing stable liquid blends of a) pentaerythritol tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, b) octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate and c) tris-(2,4-di-tert-butylphenyl)phosphite. The first process comprises preparing a solid mixture comprising about 2 parts to about 3 parts by weight a), about 2 parts to about 3 parts by weight b) and about 2 parts to about 12 parts by weight c), heating the mixture to 185° C. or higher for a sufficient time to obtain a clear liquid blend of a), b) and c), cooling the liquid blend to a temperature of from 90° C. to 140° C. and maintaining the liquid blend at a temperature of from 90° C. to 140° C. The second process comprises preparing a solid mixture comprising about 2 parts to about 3 parts by weight a) and about 2 parts to about 3 parts by weight b), heating the mixture to 90° C. or higher for a sufficient time to obtain a clear liquid mixture of a) and b), adding about 2 parts to about 12 parts by weight c) thereto to obtain a clear liquid blend of a), b) and c) and maintaining the liquid blend at a temperature of from 90° C. to 140° C. The liquid blends of a), b) and c) are stable at the temperature at which they are maintained for greater than 120 hours.
Abstract translation: 本发明涉及用于提供稳定的液体混合物的两种方法,其中a)季戊四醇四(3-(3,5-二 - 叔丁基-4-羟基苯基)丙酸酯,b)3-(3,5-二叔丁基 丁基-4-羟基苯基)丙酸酯和c)三 - (2,4-二叔丁基苯基)亚磷酸酯。 第一种方法包括制备固体混合物,其包含约2重量份至约3重量份的a),约2重量份至约3重量份的b)和约2重量份至约12重量份的c),将混合物加热至185 ℃或更高一段时间以获得a),b)和c)的澄清液体共混物,将液体共混物冷却至90℃至140℃的温度,并将液体共混物保持在 温度为90℃至140℃。第二种方法包括制备固体混合物,其包含约2重量份至约3重量份的a)和约2重量份至约3重量份的b),将混合物加热至90℃ ℃或更高,以获得a)和b)的澄清液体混合物,加入约2份至约12份(重量)的c),得到a),b)和c)的澄清液体共混物, 并将液体共混物保持在90℃至140℃的温度.a),b)和c)的液体共混物在其a 维持时间超过120小时。
-
公开(公告)号:US20180201760A1
公开(公告)日:2018-07-19
申请号:US15920877
申请日:2018-03-14
Applicant: BASF SE
Inventor: Werner Hoelzl , Bruno Rotzinger , Kai-Uwe Schoening , Roswell Easton King
IPC: C08K5/529 , C08K5/5377 , C08K5/04 , C07F9/6574 , C07F9/655 , C08K5/523
CPC classification number: C08K5/529 , C07F9/65517 , C07F9/65744 , C08K5/04 , C08K5/098 , C08K5/523 , C08K5/5377 , C08L23/12 , C08L23/00
Abstract: The invention relates to a composition comprising an organic material susceptible to oxidative, thermal or light-induced degradation and a compound of formula I-P, I-O or I-M Further embodiments are a compound of formula I-P, I-O or I-M, a process for protection of the organic material by the compound, the use of the compound for stabilizing the organic material, an additive composition comprising the compound, a process for manufacturing the compound and intermediates involved therein.
-
公开(公告)号:US20170137613A1
公开(公告)日:2017-05-18
申请号:US15419283
申请日:2017-01-30
Applicant: BASF SE
Inventor: Stephen Mark Andrews , Joseph James Fay , Roswell Easton King , Mohammad Zafar , Zhisheng Chen , Thomas Friend Thompson , Feng Zuo
Abstract: A polyolefin composition includes a polyolefin substrate having incorporated therein a nucleating agent and a filler, wherein the composition exhibits an impact strength of >35 in-lb measured according to ASTM D4226, and a coefficient of linear thermal expansion of
-
公开(公告)号:US20160244591A1
公开(公告)日:2016-08-25
申请号:US15025015
申请日:2014-09-24
Applicant: BASF SE
Inventor: Stephen Mark Andrews , Joseph James Fay , Roswell Easton King , Mohammad Zafar , Zhisheng Chen , Thomas Friend Thompson , Feng Zuo
IPC: C08K5/3435 , C08K5/52 , C08K3/22 , C08K13/02 , C08K3/26 , C08K3/34 , C08K5/138 , C08K5/3475 , C08K5/053
CPC classification number: C08K13/02 , B32B7/02 , C08K3/013 , C08K3/015 , C08K3/22 , C08K3/2279 , C08K3/26 , C08K3/34 , C08K5/0041 , C08K5/0058 , C08K5/0066 , C08K5/053 , C08K5/132 , C08K5/1345 , C08K5/138 , C08K5/17 , C08K5/32 , C08K5/3435 , C08K5/3475 , C08K5/3492 , C08K5/52 , C08K5/526 , C08K2003/2224 , C08K2003/2241 , C08K2003/265 , C08K2201/014 , C08L23/06 , C08L23/12 , C08L2205/02 , C08L2205/24 , C08L2207/062 , E04D5/06 , E04D13/15 , E04F13/18 , Y10T428/2495 , C08L23/02 , C08L53/00
Abstract: Polyolefin compositions useful for construction articles for outdoor use, for instance house siding, cladding, soffit or roofing. The compositions comprise a polyolefin substrate which has incorporated therein one or more additives selected from the group consisting of a) one or more ultraviolet light absorbers, b) one or more hindered amine light stabilizers and c) one or more antioxidants. Advantageously, the polyolefin substrate also has incorporated therein d) one or more colorants, e) one or more fillers, f) one or more flame retardants and optionally g) one or more antimicrobial compounds. The compositions exhibit certain performance levels according to standard tests, for example impact strength of >35 in-lb per ASTM D4226, coefficient of linear thermal expansion of
Abstract translation: 用于户外用建筑物的聚烯烃组合物,例如房屋壁板,包层,拱顶或屋顶。 所述组合物包含其中掺入一种或多种选自以下的添加剂的聚烯烃基材:a)一种或多种紫外光吸收剂,b)一种或多种受阻胺光稳定剂和c)一种或多种抗氧化剂。 有利的是,聚烯烃基材也已经加入其中d)一种或多种着色剂,e)一种或多种填料,f)一种或多种阻燃剂和任选的g)一种或多种抗微生物化合物。 根据标准测试,组合物表现出一定的性能水平,例如根据ASTM D4226的冲击强度> 35英寸-1,根据ASTM D696的线性热膨胀系数<4.5×10E-05 in / in / ft和任选可接受的颜色均匀性 根据ASTM D6864和/或根据ASTM D2244的预期应用可接受的低ΔE颜色和/或根据ASTM的UL-94 V-1或V-0等级和/或<200的火焰蔓延指数 E-84。
-
公开(公告)号:US10428204B2
公开(公告)日:2019-10-01
申请号:US15025015
申请日:2014-09-24
Applicant: BASF SE
Inventor: Stephen Mark Andrews , Joseph James Fay , Roswell Easton King , Mohammad Zafar , Zhisheng Chen , Thomas Friend Thompson , Feng Zuo
IPC: C08K5/3435 , C08K5/52 , E04F13/18 , E04D13/15 , C08L23/02 , C08K3/36 , C08K3/34 , C08K13/02 , C08K3/22 , C08K5/138 , C08K5/03 , C08K3/013 , C08K3/015 , E04D5/06 , C08K5/00 , C08K5/132 , C08K5/134 , C08K5/17 , C08K5/32 , C08K5/3475 , C08K5/3492 , C08K5/526 , C08L23/06 , C08L23/12 , C08K3/26 , C08K5/053 , B32B7/02
Abstract: Polyolefin compositions useful for construction articles for outdoor use, for instance house siding, cladding, soffit or roofing. The compositions comprise a polyolefin substrate which has incorporated therein one or more additives selected from the group consisting of a) one or more ultraviolet light absorbers, b) one or more hindered amine light stabilizers and c) one or more antioxidants. Advantageously, the polyolefin substrate also has incorporated therein d) one or more colorants, e) one or more fillers, f) one or more flame retardants and optionally g) one or more antimicrobial compounds. The compositions exhibit certain performance levels according to standard tests, for example impact strength of >35 in-lb per ASTM D4226, coefficient of linear thermal expansion of
-
公开(公告)号:US09951207B2
公开(公告)日:2018-04-24
申请号:US15119317
申请日:2015-02-13
Applicant: BASF SE
Inventor: Werner Hoelzl , Bruno Rotzinger , Kai-Uwe Schoening , Roswell Easton King
IPC: C08K5/15 , C07D307/00 , C08K5/529 , C08K5/523 , C07F9/655 , C07F9/6574 , C08K5/04 , C08K5/5377 , C08K5/098
CPC classification number: C08K5/529 , C07F9/65517 , C07F9/65744 , C08K5/04 , C08K5/098 , C08K5/523 , C08K5/5377 , C08L23/12 , C08L23/00
Abstract: The invention relates to a composition comprising an organic material susceptible to oxidative, thermal or light-induced degradation and a compound of formula 1-P, 1-O or I-M. Further embodiments are a compound of formula 1-P, 1-O or 1-M, a process for protection of the organic material by the compound, the use of the compound for stabilizing the organic material, an additive composition comprising the compound, a process for manufacturing the compound and intermediates involved therein.
-
公开(公告)号:US09045618B2
公开(公告)日:2015-06-02
申请号:US14345998
申请日:2012-09-27
Applicant: BASF SE
Inventor: Jiong Yu , Roswell Easton King
CPC classification number: C08K5/134 , C08K5/1345 , C08K5/52 , C08K5/526
Abstract: The present invention relates to two processes for providing stable liquid blends of a) pentaerythritol tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, b) octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate and c) tris-(2,4-di-tert-butylphenyl)phosphite. The first process comprises preparing a solid mixture comprising about 2 parts to about 3 parts by weight a), about 2 parts to about 3 parts by weight b) and about 2 parts to about 12 parts by weight c), heating the mixture to 185° C. or higher for a sufficient time to obtain a clear liquid blend of a), b) and c), cooling the liquid blend to a temperature of from 90° C. to 140° C. and maintaining the liquid blend at a temperature of from 90° C. to 140° C. The second process comprises preparing a solid mixture comprising about 2 parts to about 3 parts by weight a) and about 2 parts to about 3 parts by weight b), heating the mixture to 90° C. or higher for a sufficient time to obtain a clear liquid mixture of a) and b), adding about 2 parts to about 12 parts by weight c) thereto to obtain a clear liquid blend of a), b) and c) and maintaining the liquid blend at a temperature of from 90° C. to 140° C. The liquid blends of a), b) and c) are stable at the temperature at which they are maintained for greater than 120 hours.
Abstract translation: 本发明涉及用于提供稳定的液体混合物的两种方法,其中a)季戊四醇四(3-(3,5-二 - 叔丁基-4-羟基苯基)丙酸酯,b)3-(3,5-二叔丁基 丁基-4-羟基苯基)丙酸酯和c)三 - (2,4-二叔丁基苯基)亚磷酸酯。 第一种方法包括制备固体混合物,其包含约2重量份至约3重量份的a),约2重量份至约3重量份的b)和约2重量份至约12重量份的c),将混合物加热至185 ℃或更高一段时间以获得a),b)和c)的澄清液体共混物,将液体共混物冷却至90℃至140℃的温度,并将液体共混物保持在 温度为90℃至140℃。第二种方法包括制备固体混合物,其包含约2重量份至约3重量份的a)和约2重量份至约3重量份的b),将混合物加热至90℃ ℃或更高,以获得a)和b)的澄清液体混合物,加入约2份至约12份(重量)的c),得到a),b)和c)的澄清液体共混物, 并将液体共混物保持在90℃至140℃的温度.a),b)和c)的液体共混物在其a 维持时间超过120小时。
-
-
-
-
-
-
-
-