公开(公告)号:US10259935B2
公开(公告)日:2019-04-16
申请号:US15540582
申请日:2016-01-13
Applicant: Borealis AG
Inventor: Linus Karlsson , Bernt-Ake Sultan , Fredrik Skogman , Joerg H. M. Ruder , Claus Beisert
Abstract: The present invention relates to a flame retardant polypropylene composition for a conduit, appliance, and/or automotive wire, comprising a flame retardant composition comprising: a) a base resin comprising a heterophasic propylene copolymer which comprises a polypropylene homo- or copolymer matrix and an ethylene propylene rubber dispersed in said matrix, and b) a metal hydroxide or hydrated compound, wherein the heterophasic propylene copolymer has a MFR2 below 0.8 g/10 min and a xylene cold soluble (XCS) fraction content between 1 and 15 wt % based on the total weight of the heterophasic propylene copolymer.
-
公开(公告)号:US10173358B2
公开(公告)日:2019-01-08
申请号:US14649939
申请日:2013-12-17
Applicant: BOREALIS AG
Inventor: Thierry Toullec , Paul Laurenson , Bart Verheule , Ola Fagrell , Linus Karlsson
IPC: B29L7/00 , B29L9/00 , C08F8/42 , C08J5/00 , C08K5/00 , C08K5/57 , H01B3/44 , B29C47/00 , B29C47/02 , B29C47/88 , B29C47/92 , B29K83/00 , B29L23/00 , C08L43/04
Abstract: A process for for making a cross-linked polyethylene article includes: (A) feeding a blend comprising a cross-linkable silane-group containing polyethylene copolymer and at least one additive to an extruder, (B) feeding a liquid comprising a silanol condensation catalyst to said extruder to form a mixture with said blend, (C) extruding said mixture to form an article and (D) cross-linking said article. The article may be a pipe or cable.
-
3.
公开(公告)号:US20180265689A1
公开(公告)日:2018-09-20
申请号:US15780973
申请日:2016-12-13
Applicant: BOREALIS AG
Inventor: Bernt-Ake Sultan , Linus Karlsson , Oscar Prieto
CPC classification number: C08L33/10 , C08G77/04 , C08K3/016 , C08L23/0876 , C08L33/08 , C08L2201/02 , H01B3/10 , H01B3/441 , H01B3/447 , H01B3/46 , H01B7/295 , C08L83/04 , C08L23/08
Abstract: The present invention relates to a halogen-free flame retardant polymer composition comprising a polar ethylene copolymer comprising an acrylate with a bulky end group, inorganic flame retardant filler and a silicone fluid or gum. The present invention is also directed to a cable comprising the halogen-free flame retardant polymer, a layered structure, a cable and to a process for producing the polar ethylene copolymer.
-
公开(公告)号:US20180016426A1
公开(公告)日:2018-01-18
申请号:US15540582
申请日:2016-01-13
Applicant: Borealis AG
Inventor: Linus Karlsson , Bernt-Ake Sultan , Fredrik Skogman , Joerg H.M. Ruder , Claus Beisert
CPC classification number: C08L23/12 , C08K3/22 , C08K2003/2224 , C08L23/16 , C08L2201/02 , C08L2203/202 , C08L2207/02 , C09K21/02 , H01B7/295
Abstract: The present invention relates to a flame retardant polypropylene composition for a conduit, appliance, and/or automotive wire, comprising a flame retardant composition comprising: a) a base resin comprising a heterophasic propylene copolymer which comprises a polypropylene homo- or copolymer matrix and an ethylene propylene rubber dispersed in said matrix, and b) a metal hydroxide or hydrated compound, wherein the heterophasic propylene copolymer has a MFR2 below 0.8 g/10 min and a xylene cold soluble (XCS) fraction content between 1 and 15 wt % based on the total weight of the heterophasic propylene copolymer.
-
公开(公告)号:US20240409731A1
公开(公告)日:2024-12-12
申请号:US18699789
申请日:2022-10-10
Applicant: BOREALIS AG
Inventor: Susanne Nilsson , Victoria Karlsson , Bernt-Åke Sultan , Elisabeth Ribarits , Linus Karlsson , Lars Efraimsson
Abstract: The present invention relates to a flame retardant polymer composition comprising (A) 2.0 to 15.0 wt % of a copolymer of ethylene comprising units selected from the group consisting of methyl acrylate, methyl methacrylate or mixtures thereof; (B) 0 to 4.0 wt % of a polyethylene and/or polypropylene containing units originating from maleic acid anhydride; (C) 0.1 to 3.0 wt % of a silicon fluid and/or silicone gum; (D) 40.0 to 55.0 wt % of a magnesium hydroxide; (E) 2.0 to 15.0 wt % of a copolymer of ethylene and alpha olefin comonomer units having from 4 to 10 carbon atoms, which has a density of from 860 to 910 kg/m3, determined according to ISO 1183; (F) 18.0 to 35.0 wt % of a copolymer of ethylene and alpha olefin comonomer units having from 4 to 10 carbon atoms, which has a density of from 920 to 960 kg/m3, determined according to ISO 1183, and a melt flow rate MFR5 of from 0.05 to 2.50 g/10 min, determined according to ISO 1133 at a temperature of 190° C. and a load of 5.0 kg; and (G) 0 to 8.0 wt % of carbon black, wherein all weight percentages are based on the total weight of the flame retardant polymer composition; an article, such as a wire or cable, comprising said flame retardant polymer composition; and the use of said flame retardant polymer composition for the production of an article, such as a wire or cable.
-
公开(公告)号:US20190194437A1
公开(公告)日:2019-06-27
申请号:US16288693
申请日:2019-02-28
Applicant: Borealis AG
Inventor: Linus Karlsson , Bernt-Ake Sultan , Fredrik Skogman , Joerg H.M. Ruder , Claus Beisert
CPC classification number: C08L23/12 , C08K3/22 , C08K2003/2224 , C08L23/16 , C08L2201/02 , C08L2203/202 , C08L2207/02 , C09K21/02 , H01B7/295
Abstract: The present invention relates to a flame retardant polypropylene composition for a conduit, appliance, and/or automotive wire, comprising a flame retardant composition comprising: a) a base resin comprising a heterophasic propylene copolymer which comprises a polypropylene homo- or copolymer matrix and an ethylene propylene rubber dispersed in said matrix, and b) a metal hydroxide or hydrated compound, wherein the heterophasic propylene copolymer has a MFR2 below 0.8 g/10 min and a xylene cold soluble (XCS) fraction content between 1 and 15 wt % based on the total weight of the heterophasic propylene copolymer.
-
7.
公开(公告)号:US20150314509A1
公开(公告)日:2015-11-05
申请号:US14649939
申请日:2013-12-17
Applicant: Borealis AG
Inventor: Thierry Toullec , Paul Laurenson , Bart Verheule , Ola Fagrell , Linus Karlsson
CPC classification number: B29C47/0004 , B29C47/0009 , B29C47/0014 , B29C47/0016 , B29C47/0021 , B29C47/0023 , B29C47/02 , B29C47/88 , B29C47/8895 , B29C47/92 , B29K2083/00 , B29K2995/0058 , B29L2007/00 , B29L2009/00 , B29L2023/22 , C08F8/42 , C08F2810/20 , C08J5/00 , C08J2343/04 , C08K5/0025 , C08K5/0091 , C08K5/57 , H01B3/441 , C08L43/04
Abstract: The present invention relates to a process for making a cross-linked polyethylene article and to the use of such a process in the production of pipes or cables. The process comprises: (A) feeding a blend comprising a cross-linkable silane-group containing polyethilene copolymer and at least one additive to an extruder, (B) feeding a liquid comprising a silanol condensation catalyst to said extruder to form a mixture with said blend, (C) extruding said mixture to form an article and (D) cross-linking said article.
Abstract translation: 本发明涉及制造交联聚乙烯制品的方法以及在生产管道或电缆中使用这种方法。 该方法包括:(A)将包含可交联的含硅烷基团的聚乙烯共聚物和至少一种添加剂的共混物进料到挤出机中,(B)将包含硅烷醇缩合催化剂的液体进料到所述挤出机以形成与所述 共混,(C)挤出所述混合物以形成制品,和(D)交联所述制品。
-
-
-
-
-
-