摘要:
The use of a liquid polymethyl phenyl siloxane or a liquid polydimethyl siloxane, in combination with calcium stearate, pentaerythritol tetrastearate, bis-stearylamide of ethylene diamine or mixtures thereof for improving the physical properties of ABS-polymers.
摘要:
ABS-moulding compositions of (a) 5 to 70% by weight of one or more graft products and (b) 95 to 30% by weight of one or more thermoplastic resins with a content of 0.05 to 2.0% by weight (based on total mixture) of a silico urethane derivative to improve notched impact strength.
摘要:
ABS-moulding compositions of (a) 5 to 70% by weight of one or more graft products and (b) 95 to 30% by weight of one or more thermoplastic resins with a content of 0.05 to 1% by weight (based on total moulding composition) of a perfluoroalkane acid or a derivative thereof to improve notched impact strength.
摘要:
A thermoplastic moulding composition which comprises: (A) from 99.99 to 94% by weight of an ABS composition comprising: (a) from 5 to 70% by weight of one or more rubber-based graft polymers; and (b) from 95 to 30% by weight of one or more thermoplastic resins; and (B) from 0.01 to 6.0% by weight of one or more compounds corresponding to the following general formula: ##STR1## wherein R represents hydrogen, C.sub.1 -C.sub.4 -alkyl or carboxyl; R.sup.1 represents hydrogen or methyl; and R.sup.2 represents carboxyl, and which may also contain from 0.1 to 3% by weight of one or more compounds corresponding to the formula: ##STR2##
摘要:
Moulding compositions based on ABS-graft polymers, containing:A. 5 to 70 parts, by weight of a graft polymer obtained by grafting 20 to 60 parts by weight of a mixture of styrene and acrylonitrile in a ratio, by weight, of 95 : 5 to 60 : 40 onto 80 to 40 parts, by weight, of polybutadiene or a butadiene copolymer with a butadiene content of > 30% with an average particle diameter of 0.26 to 0.65 .mu. and a grafting degree of 0.15 to 0.7;B. 0 to 50 parts, by weight, of a graft polymer obtained by polymerizing 40 to 60 parts, by weight, of a mixture of styrene and acrylonitrile in a ratio, by weight, of 95 : 5 to 60 : 40 onto 60 to 40 parts, by weight, of polybutadiene or a butadiene copolymer with a butadiene content of more than 30%, with an average particle diameter of from 0.05 to 0.25 .mu. and a grafting degree of 0.4 to 0.9; andC. 25 to 95 parts, by weight, of a copolymer of styrene and/or .alpha.-methyl styrene on the one hand and acrylonitrile on the other hand in a ratio by weight, of 80 : 20 to 60 : 40 with an average molecular weight M.sub.w (weight average) of from 50,000 to 200,000 and a molecular heterogeneity U of 4.5 to 1.0; such thatD. the ratios, by weight, of styrene (including .alpha.-methyl styrene if present) to acrylonitrile satisfy the following conditions: ##EQU1##
摘要:
Isolating thermoplastic or thermoelastic polymers in the form of a powder of limited water and precipitant content and uniform grain size from their aqueous dispersions wherein(i) a polymer dispersion and a precipitant are intensively mixed at an uptake of mechanical energy of 0.2 to 0.6 KWh per m.sup.3 of dispersion thus causing high turbulence,(ii) the polymer is precipitated while in this state of high turbulence at a temperature below the sintering temperature of the polymer,(iii) the precipitated polymer particles are agglomerated and hardened while still in contact with the aqueous liquor either in one or in several stages, and(iv) the aqueous liquor and agglomerated polymer particles are separated from one another.
摘要:
Process for the removal of residual monomers from ABS polymers prepared by emulsion polymerization, wherein from 0.1 to 10% by weight, based on the solids content in the latex, of an electrolyte such as an acid or a salt are added to a latex containing an ABS polymer, and the mixture is at the same time heated to a temperature of from 55.degree. to 120.degree. C. while the residual monomer and part of the water are removed by distillation.
摘要:
The present invention relates to thermoplastic moulding compositions consisting of polycarbonates, graft polymers and copolymers, which are characterized in that they contain special graft polymers and/or special copolymers, with the result that these moulding compositions possess a very homogeneous rubber distribution and furthermore possess very good toughness and heat stability and substantially improved heat distortion resistance.
摘要:
Polycarbonate molding compositions resistant to light aging and exhibiting an improved notched impact strength are disclosed. The compositions which are based on an aromatic polycarbonate, aromatic polyester carbonate or a polyester, contain a redox-catalyzed graft polymer of resin-forming monomers on a rubber, a phosphorus compound and a fluorinated polyolefin.
摘要:
Thermoplastic molding compositions containingA) ABS-type resin,B) aromatic polycarbonate resins,C) a compound bearing several carboxyl groups or mixtures thereof and optionallyD) further polymer resins,characterized in that an ABS resin with at least one basically acting additive is used as component A, component C is selected from compounds having a molecular weight of from 150 to 260 having at least two carboxyl groups (--COOH) in the molecule, and the weight ratio of basically acting additive in A: carboxyl groups in C is from 5:1 to 1:1.