Wire saw process
    1.
    发明申请
    Wire saw process 审中-公开
    线锯工艺

    公开(公告)号:US20090032006A1

    公开(公告)日:2009-02-05

    申请号:US11888264

    申请日:2007-07-31

    IPC分类号: B28D1/08

    摘要: This invention provides a method for increasing the cutting performance of a wire saw, in cutting a substrate, by increasing the association of the abrasive particles in the cutting slurry and the cutting wire, the enhancement being caused by the use of thickening agents in the cutting slurry or by increasing the attraction of the abrasive particles to the cutting wire.

    摘要翻译: 本发明提供了一种通过增加切割浆料和切割丝中的磨料颗粒的关联性来提高线锯在切割基材中的切割性能的方法,这是由于在切割中使用增稠剂引起的增强 浆料或通过增加磨料颗粒到切割丝线的吸引力。

    Slurry composition containing non-ionic polymer and method for use
    2.
    发明申请
    Slurry composition containing non-ionic polymer and method for use 有权
    含非离子聚合物的浆料组合物及其使用方法

    公开(公告)号:US20090126713A1

    公开(公告)日:2009-05-21

    申请号:US12317254

    申请日:2008-12-19

    摘要: A wiresaw cutting fluid composition of the present invention comprises about 25 to about 75% by weight of a particulate abrasive suspended in an aqueous carrier containing a polymeric viscosity modifier that comprises a polymer including a majority of non-ionic monomer units (preferably 100 mol % non-ionic monomer units), has a number average molecular weight (Mn) of at least about 5 kDa, and is present in the composition at a concentration sufficient to provide a Brookfield viscosity for the composition in the range of about 50 to about 1000 cP, e.g., 50 to about 700 cP, at about 25° C. at a spindle rotation rate of about 60 rpm. In one embodiment, the viscosity modifier comprises a polymer having a weight average molecular weight (Mw) of at least about 200 kDa. When a viscosity modifier of 200 kDa or greater Mw is utilized, a preferred wiresaw cutting method the cutting fluid is circulated and applied by pumps and nozzles operating at a relatively low shear rate of not more than about 104 s−1.

    摘要翻译: 本发明的线切割液组合物包含约25至约75重量%的悬浮在含有载体的水性载体中的颗粒磨料,所述颗粒磨料包含聚合物粘度调节剂,其包含大部分非离子单体单元的聚合物(优选为100摩尔% 非离子单体单元)具有至少约5kDa的数均分子量(Mn),并且以足以提供组合物的Brookfield粘度在约50至约1000范围内的浓度存在于组合物中 cP,例如50至约700cP,在约25℃下以约60rpm的主轴转速进行。 在一个实施方案中,粘度调节剂包含重均分子量(Mw)为至少约200kDa的聚合物。 当使用200kDa或更大的Mw的粘度调节剂时,优选的切线切割方法是通过以不大于约104s -1的较低剪切速率操作的泵和喷嘴循环施加切削液。

    GST CMP slurries
    3.
    发明授权
    GST CMP slurries 有权
    GST CMP浆料

    公开(公告)号:US08778211B2

    公开(公告)日:2014-07-15

    申请号:US13551423

    申请日:2012-07-17

    摘要: The present invention provides chemical-mechanical polishing (CMP) compositions suitable for polishing a substrate comprising a germanium-antimony-tellurium (GST) alloy. The CMP compositions of the present invention are aqueous slurries comprising a particulate abrasive, a water-soluble surface active agent, a complexing agent, and a corrosion inhibitor. The ionic character of the surface active material (e.g., cationic, anionic, or nonionic) is selected based on the zeta potential of the particulate abrasive. A CMP method for polishing a GST alloy-containing substrate utilizing the composition is also disclosed.

    摘要翻译: 本发明提供了适用于抛光包含锗 - 锑 - 碲(GST)合金的基材的化学机械抛光(CMP)组合物。 本发明的CMP组合物是包含颗粒磨料,水溶性表面活性剂,络合剂和腐蚀抑制剂的水性浆料。 基于颗粒磨料的ζ电位来选择表面活性材料(例如阳离子,阴离子或非离子)的离子特性。 还公开了利用该组合物研磨含GST合金的基材的CMP方法。

    Manufacturing method of ferromolybdenum from molybdenite
    4.
    发明授权
    Manufacturing method of ferromolybdenum from molybdenite 有权
    来自辉钼矿的钼铁的制造方法

    公开(公告)号:US08268034B2

    公开(公告)日:2012-09-18

    申请号:US12995870

    申请日:2010-10-20

    IPC分类号: C22C38/12

    摘要: Provided is a manufacturing method of ferromolybdenum from molybdenite concentrate, and more particularly, a manufacturing method of ferromolybdenum with copper content of 0.5% or less from molybdenite with high copper content without carrying out a separate copper removing process by putting molybdenite, aluminum metal and iron metal, in a heating furnace and reacting them at high temperature to manufacture the ferro molybdenum at the lower portion thereof, forming a slag using aluminum sulfide and iron sulfide as the main components at the upper portion thereof, and putting most of the copper (80 to 95%) existing in the molybdenite in a slag layer. The exemplary embodiment can shorten a process as compared to a metallothermic reduction (Thermit) method of the related art and reduce the consumption of a reducing agent, i.e., aluminum.

    摘要翻译: 本发明提供来自辉钼矿精矿的钼铁的制造方法,特别是铜含量高于铜含量为0.5%以下的铁钼的制造方法,不进行通过将辉钼矿,铝金属和铁 金属,在加热炉中并在高温下使其反应以在其下部制造铁钼,在其上部使用硫化铝和硫化铁作为主要成分形成炉渣,并将大部分铜(80 至95%)存在于辉钼矿中的渣层中。 与现有技术的金属热还原(Thermit)方法相比,示例性实施方案可以缩短工艺,并且减少还原剂即铝的消耗。

    Manufacturing Method of Ferromolybdenum From Molybdenite
    5.
    发明申请
    Manufacturing Method of Ferromolybdenum From Molybdenite 有权
    钼辉钼矿的制造方法

    公开(公告)号:US20120174709A1

    公开(公告)日:2012-07-12

    申请号:US12995870

    申请日:2010-10-20

    IPC分类号: C22C1/02 C22B4/06

    摘要: Provided is a manufacturing method of ferromolybdenum from molybdenite concentrate, and more particularly, a manufacturing method of ferromolybdenum with copper content of 0.5% or less from molybdenite with high copper content without carrying out a separate copper removing process by putting molybdenite, aluminum metal and iron metal, in a heating furnace and reacting them at high temperature to manufacture the ferro molybdenum at the lower portion thereof, forming a slag using aluminum sulfide and iron sulfide as the main components at the upper portion thereof, and putting most of the copper (80 to 95%) existing in the molybdenite in a slag layer. The exemplary embodiment can shorten a process as compared to a metallothermic reduction (Thermit) method of the related art and reduce the consumption of a reducing agent, i.e., aluminum.

    摘要翻译: 本发明提供来自辉钼矿精矿的钼铁的制造方法,特别是铜含量高于铜含量为0.5%以下的铁钼的制造方法,不进行通过将辉钼矿,铝金属和铁 金属,在加热炉中并在高温下使其反应以在其下部制造铁钼,在其上部使用硫化铝和硫化铁作为主要成分形成炉渣,并将大部分铜(80 至95%)存在于辉钼矿中的渣层中。 与现有技术的金属热还原(Thermit)方法相比,示例性实施方案可以缩短工艺,并且减少还原剂即铝的消耗。

    Slurry composition containing non-ionic polymer and method for use
    6.
    发明授权
    Slurry composition containing non-ionic polymer and method for use 有权
    含非离子聚合物的浆料组合物及其使用方法

    公开(公告)号:US08157876B2

    公开(公告)日:2012-04-17

    申请号:US12317254

    申请日:2008-12-19

    摘要: A wiresaw cutting fluid composition of the present invention comprises about 25 to about 75% by weight of a particulate abrasive suspended in an aqueous carrier containing a polymeric viscosity modifier that comprises a polymer including a majority of non-ionic monomer units (preferably 100 mol % non-ionic monomer units), has a number average molecular weight (Mn) of at least about 5 kDa, and is present in the composition at a concentration sufficient to provide a Brookfield viscosity for the composition in the range of about 50 to about 1000 cP, e.g., 50 to about 700 cP, at about 25° C. at a spindle rotation rate of about 60 rpm. In one embodiment, the viscosity modifier comprises a polymer having a weight average molecular weight (Mw) of at least about 200 kDa. When a viscosity modifier of 200 kDa or greater Mw is utilized, a preferred wiresaw cutting method the cutting fluid is circulated and applied by pumps and nozzles operating at a relatively low shear rate of not more than about 104 s−1.

    摘要翻译: 本发明的线切割液组合物包含约25至约75重量%的悬浮在含有载体的水性载体中的颗粒磨料,所述颗粒磨料包含聚合物粘度调节剂,其包含大部分非离子单体单元的聚合物(优选为100摩尔% 非离子单体单元)具有至少约5kDa的数均分子量(Mn),并且以足以提供组合物的Brookfield粘度在约50至约1000范围内的浓度存在于组合物中 cP,例如50至约700cP,在约25℃下以约60rpm的主轴转速进行。 在一个实施方案中,粘度调节剂包含重均分子量(Mw)为至少约200kDa的聚合物。 当使用200kDa或更大的Mw的粘度调节剂时,优选的切线切割方法是通过以不大于约104s -1的较低剪切速率操作的泵和喷嘴循环施加切削液。