摘要:
This invention provides an improved porous structure for semiconductor devices and a process for making the same. This process may be applied to an existing porous structure 28, which may be deposited, for example, between patterned conductors 24. The method may comprise providing a substrate comprising a microelectronic circuit and a porous silica layer, the porous silica layer having an average pore diameter between 2 and 80 nm; and heating the substrate to one or more temperatures between 100 and 490 degrees C. in a substantially halogen-free atmosphere, whereby one or more dielectric properties of the porous dielectric are improved. In some embodiments, the atmosphere comprises a phenyl-containing atmosphere, such as hexaphenyldisilazane. In some embodiments, the method further comprises cooling the substrate and exposing the substrate to a substantially halogen-free atmosphere comprising either a phenyl-containing compound, such as hexaphenyldisilazane; or a methyl-containing compound, such as hexamethyldisilazane. It has been found that a porous structure treated in such a manner generally exhibits improved dielectric properties relative to an untreated sample.
摘要:
This invention has enabled a new, simple nanoporous dielectric fabrication method. In general, this invention uses a polyol, such as glycerol, as a solvent. This new method allows both bulk and thin film aerogels to be made without supercritical drying, freeze drying, or a surface modification step before drying. Prior art aerogels have required at least one of these steps to prevent substantial pore collapse during drying. Thus, this invention allows production of nanoporous dielectrics at room temperature and atmospheric pressure, without a separate surface modification step. Although not required to prevent substantial densification, this new method does not exclude the use of supercritical drying or surface modification steps prior to drying. In general, this new method is compatible with most prior art aerogel techniques. Although this new method allows fabrication of aerogels without substantial pore collapse during drying, there may be some permanent shrinkage during aging and/or drying.
摘要:
Processes for producing gel compositions comprising: esterifying a portion of the surface of a gel composition sufficient to produce a gel composition having a rod density of less than or equal to 0.15 g/cc, and/or a tap density of less than or equal to 0.2 g/cc through contact with at least one esterification agent and at least one catalyst. The processes may be utilized to produce low density gel compositions without the need for a supercritical drying step or thermal treatment.
摘要:
This pertains generally to precursors and deposition methods suited to aerogel thin film fabrication of nanoporous dielectrics. A method of forming a nanoporous dielectric on a semiconductor substrate is disclosed. By a method according to the present invention, a precursor sol is applied as a nongelling thin film 14 to a semiconductor substrate 10. This substrate may contain patterned conductors 12, gaps 13, and/or other structures. A portion of the solvent is evaporated from the thin film 14 to produce a reduced thickness film 18. Film 18 is gelled and may be aged. A surface modification agent is introduced to the reaction atmosphere in a vaporish form, e.g., a vapor, mist, aerosol, or similar form. The surface modifier can then diffuse into, condense onto, and/or settle onto the wet gel and then diffuse throughout the thin film. This vaporish introduction of the surface modification agent ensures that there are no strong fluid flows across the wafer that might damage the wet gel. It can also be compatible with standard processing equipment and can potentially be used with other reaction atmosphere controls that reduce premature drying of the gel.
摘要:
A process for producing surface modified metal oxide and/or organo-metal oxide compositions comprising esterifying at least a portion of the metal oxide and/or organo-metal oxide composition through contact with at least one esterification agent and at least one catalyst wherein the esterification agent and the catalyst are in the liquid phase. The process may be utilized to produce hydrophobic metal oxide and/or organo-metal oxide compositions at ambient temperature and/or ambient pressure conditions.
摘要:
This invention has enabled a new, simple thin film nanoporous dielectric fabrication method. In general, this invention uses glycerol, or another low volatility compound, as a solvent. This new method allows thin film aerogels/low density xerogels to be made without supercritical drying, freeze drying, or a surface modification step before drying. Thus, this invention allows production of nanoporous dielectrics at room temperature and atmospheric pressure, without a separate surface modification step. Although this new method allows fabrication of aerogels without substantial pore collapse during drying, there may be some permanent shrinkage during aging and/or drying. This invention allows controlled porosity thin film nanoporous aerogels to be deposited, gelled, aged, and dried without atmospheric controls. In another aspect, this invention allows controlled porosity thin film nanoporous aerogels to be deposited, gelled, rapidly aged at an elevated temperature, and dried with only passive atmospheric controls, such as limiting the volume of the aging chamber.
摘要:
This pertains generally to precursors and deposition methods suited to aerogel thin film fabrication of nanoporous dielectrics. An aerogel precursor sol is disclosed. This aerogel precursor sol contains a metal alkoxide (such as TEOS) and a solvent, but no gelation catalyst. By a method according to the present invention, such a precursor sol is applied as a nongelling thin film 14 to a semiconductor substrate 10. This substrate may contain patterned conductors 12, gaps 13, or other structures. An independent gelation catalyst (preferably, vapor phase ammonia) is added to promote rapid gelation of the thin film sol 14 at the desired time. One advantage is that it allows substantially independent control of gelation and pore fluid evaporation. This independent catalyst introduction allows additional processing steps to be performed between sol deposition and the onset of substantial gelation. One potential step is to evaporate a portion of the pore fluid solvent. Additional advantages of independent catalyst introduction are that it reduces the need for process steps requiring critical timing and provides a large increase in the pot life of the precursor sol.
摘要:
This invention pertains generally to aging methods suited to aerogel thin film fabrication, and particularly to techniques for improving gel strength and/or aerogel dielectric constant by a rapid aging technique, which avoid damage or premature drying of wet gel thin films during aging. A substrate having a wet gel thin film deposited thereon is contacted with a saturated water vapor atmosphere, preferably at an elevated pressure and a temperature greater than 100.degree. C. The method may comprise a vapor-phase exchange step to remove low boiling point pore liquids such as ethanol prior to or during aging. The method may also comprise a vapor-phase exchange step to replace water in the wet gel with another pore liquid such as acetone to stop the aging process and prepare the wet gel for drying. A vapor-phase aging catalyst (e.g. ammonia) may also be used to enhance the aging process. The present invention allows aging of wet gel thin films to be completed in a few minutes instead of the days generally required for conventional bulk gel aging.
摘要:
This invention has enabled a new, simple nanoporous dielectric fabrication method. In general, this invention uses a glycol, such as ethylene glycol, as a solvent. This new method allows both bulk and thin film aerogels to be made without supercritical drying, freeze drying, or a surface modification step before drying. Prior art aerogels have required at least one of these steps to prevent substantial pore collapse during drying. Thus, this invention allows production of nanoporous dielectrics at room temperature and atmospheric pressure, without a separate surface modification step. Although not required to prevent substantial densification, this new method does not exclude the use of supercritical drying or surface modification steps prior to drying. In general, this new method is compatible with most prior art aerogel techniques. Although this new method allows fabrication of aerogels without substantial pore collapse during drying, there may be some permanent shrinkage during aging and/or drying.
摘要:
This invention has enabled a new, simple thin film nanoporous dielectric fabrication method. In general, this invention uses glycerol, or another low volatility compound, as a solvent. This new method allows thin film aerogels/low density xerogels to be made without supercritical drying, freeze drying, or a surface modification step before drying. Thus, this invention allows production of nanoporous dielectrics at room temperature and atmospheric pressure, without a separate surface modification step. Although this new method allows fabrication of aerogels without substantial pore collapse during drying, there may be some permanent shrinkage during aging and/or drying. This invention allows controlled porosity thin film nanoporous aerogels to be deposited, gelled, aged, and dried without atmospheric controls. In another aspect, this invention allows controlled porosity thin film nanoporous aerogels to be deposited, gelled, rapidly aged at an elevated temperature, and dried with only passive atmospheric controls, such as limiting the volume of the aging chamber.