Abstract:
A cellulose fiber dispersion polyethylene resin composite material formed by dispersing a cellulose fiber into a polyethylene resin, in which a proportion of the above-described cellulose fiber is 1 part by mass or more and 70 parts by mass or less in a total content of 100 parts by mass of the polyethylene resin and the cellulose fiber, and the polyethylene resin satisfies a relationship: 1.7>half-width (Log(MH/ML))>1.0 in a molecular weight pattern obtained by gel permeation chromatography measurement, and a formed body and a pellet using the same, a production method therefor, and a recycling method for the cellulose fiber adhesion polyethylene thin film piece.
Abstract:
A cellulose-fiber-dispersing polyolefin resin composite material, containing a polyolefin resin containing a polypropylene resin, and a cellulose fiber dispersed in the polyolefin resin, in which a proportion of the cellulose fiber is 1 mass part or more and 70 mass parts or less in a total content of 100 mass parts of the polyolefin resin and the cellulose fiber, and the water absorption ratio satisfies the following Formula: (Water absorption ratio [%])
Abstract:
A polyolefin-based thermoplastic elastomer and a crosslinked body of the same which can undergo a silane-crosslinking process excellent in productivity and have a rubber property required as a substitute material for EPDM is disclosed herein and can use a silane-crosslinkable ethylene-propylene copolymer characterized in that an organic peroxide (B) and a silane coupling agent (C) are compounded with an ethylene-propylene copolymer resin (A) which comprises 5 to 25% by mass of an ethylene component and 75 to 95% by mass of a propylene component, and whose MFR measured at 230° C. and with a load of 2.16 kg applied is 20.0 g/10 min or less. and further a compounded amount of the organic peroxide is 0.1 to 0.6 pts. mass based on 100 pts. mass of the ethylene-propylene copolymer resin (A) and a one-minute half-life temperature of the organic peroxide is 175.2° C. or less.
Abstract:
A laminate, containing two or more polyolefin resin layers, wherein at least one polyolefin resin layer (A) contains a cellulose fiber including a cellulose fiber having a fiber length of 0.3 mm or more dispersed in the layer; a content of the cellulose fiber in the polyolefin resin layer (A) is 1% by mass or more and less than 60% by mass; and wherein a polyolefin resin layer (B) different from the polyolefin resin layer (A) is laminated in contact with the polyolefin resin layer (A).
Abstract:
A cellulose-fiber-dispersing polyolefin resin composite material, containing a polyolefin resin and a cellulose fiber dispersed in the polyolefin resin, in which the composite material contains the cellulose fiber of 3 mass % or more and less than 70 mass %, and when the composite material is subjected to the abrasion test according to ISO 6722 under the following test conditions, the amount of abrasion after 5,000 reciprocations satisfies the [Formula 1]: (Amount of abrasion [mm] of the cellulose-fiber-dispersing polyolefin resin composite material)
Abstract:
A cellulose-fiber-dispersing polyolefin resin composite material, containing a polyolefin resin containing a polypropylene resin, and a cellulose fiber dispersed in the polyolefin resin, in which a proportion of the cellulose fiber is 1 mass part or more and 70 mass parts or less in a total content of 100 mass parts of the polyolefin resin and the cellulose fiber, and the polyolefin resin satisfies the expression: Mz/Mw≥4, which is a ratio of Z-average molecular weight Mz to weight-average molecular weight Mw to be obtained by a gel permeation chromatography measurement; a pellet or a formed body using this composite material; and a production method for the composite material.