摘要:
Disclosed is a phosphated galvanized steel sheet comprising a steel sheet, a zinc-plating layer of η single phase which is formed on at least one side of the steel sheet and contains Ni in an amount of not less than 10 ppm by mass and not more than the solubility limit thereof, and a phosphate layer which is formed on the zinc-plating layer and contains Mg in an amount of not less than 0.1 % by mass and less than 2.0 % by mass. Although this steel sheet is not subjected to sealing, it has corrosion resistance equivalent to or higher than those of conventional steel sheets which have been subjected to sealing, while having excellent blackening resistance.
摘要:
The phosphate-treated zinc-coated steel sheet has: a steel sheet; a zinc-coating layer of a single η-phase containing Ni in a range from 10 ppm by mass to solid solution limit, being formed on at least one side of the steel sheet; and a phosphate-treated layer containing Mg in a range from not less than 0.1% by mass to less than 2.0% by mass, being formed on the zinc-coating layer. The steel sheet without treated by sealing has corrosion resistance equivalent to or higher than that of conventional products treated by sealing, and also has excellent blackening resistance.
摘要:
A lithium-containing composite oxide represented by the formula 1: LixNi1-y-z-v-wCoyAlzM1vM2wO2 is used as a positive electrode active material for a non-aqueous electrolyte secondary battery. The element M1 is at least one selected from the group consisting of Mn, Ti, Y, Nb, Mo, and W. The element M2 includes at least two selected from the group consisting of Mg, Ca, Sr, and Ba, and the element M2 includes at least Mg and Ca. The formula 1 satisfies 0.97≦x≦1.1, 0.05≦y≦0.35, 0.005≦z≦0.1, 0.0001≦v≦0.05, and 0.0001≦w≦0.05. The primary particles have a mean particle size of 0.1 μm or more and 3 μm or less, and the secondary particles have a mean particle size of 8 μm or more and 20 μm or less.
摘要:
A lithium-containing composite oxide represented by the formula 1: LixNi1-y-z-v-wCoyAlzM1vM2wO2 is used as a positive electrode active material for a non-aqueous electrolyte secondary battery. The element M1 is at least one selected from the group consisting of Mn, Ti, Y, Nb, Mo, and W. The element M2 includes at least two selected from the group consisting of Mg, Ca, Sr, and Ba, and the element M2 includes at least Mg and Ca. The formula 1 satisfies 0.97≦x≦1.1, 0.05≦y≦0.35, 0.005≦z≦0.1, 0.0001≦v≦0.05, and 0.0001≦w≦0.05. The primary particles have a mean particle size of 0.1 μm or more and 3 μm or less, and the secondary particles have a mean particle size of 8 μm or more and 20 μm or less.
摘要翻译:作为非水电解质二次电池用正极活性物质,使用由式1表示的含锂复合氧化物:LixNi1-y-z-v-wCoyAlzM1vM2wO2。 元素M1是选自Mn,Ti,Y,Nb,Mo和W中的至少一种元素。元素M2包括选自Mg,Ca,Sr和Ba中的至少两种元素,并且 元素M2至少包括Mg和Ca。 式1满足0.97 <= x <= 1.1,0.05 <= y <=0.35,0.005≤z≤0.1,0.0001≤v≤0.05,0.0001≤w≤0.05。 初级粒子的平均粒径为0.1μm以上3μm以下,二次粒子的平均粒径为8μm以上且20μm以下。
摘要:
A positive electrode active material for non-aqueous electrolyte secondary battery composed of a lithium nickel composite oxide having high capacity and superior heat stability, a production method that is suitable for its industrial production, and a non-aqueous electrolyte secondary battery having high safety. The positive electrode active material for non-aqueous electrolyte secondary battery includes a lithium nickel composite oxide having by the following general formula (1): LibNi1-aM1aO2 (1) (wherein M1 represents at least one kind of element selected from transition metal elements other than Ni, the second group elements and the thirteenth group elements; a satisfies 0.01≦a≦0.5; and b satisfies 0.85≦b≦1.05). The amount of lithium at the surface of the lithium nickel composite oxide is 0.10% by mass or lower. The positive electrode active material is obtained by water washing fired powder at a temperature range of 10 to 40° C., and then filtering and drying the same.
摘要:
The coating composition includes a methacrylic resin prepared by copolymerization of styrene or a substituted styrene (A), a methacrylic ester obtained from an alcohol having at least two carbon atoms and methacrylic acid (B), and an olefinic compound having at least one carboxylic group (C), in which the molar ratio thereof is 1:(0.05 to 44.5):(0.12 to 13). A metal sheet lubricated with the coating composition has superior characteristics of dissolution of the film in an alkaline solution, chemical processing, paint dryness, blocking resistance, corrosion resistance, stability of coating composition, and press formability (powdering resistance and galling resistance).
摘要:
A positive electrode active material for a nonaqueous electrolyte secondary battery that is constituted by a lithium nickel composite oxide that combines a high capacity with excellent thermal stability, a manufacturing method suitable for industrial production, and a nonaqueous electrolyte secondary battery of high safety. A positive electrode active material for a nonaqueous electrolyte secondary battery includes a lithium nickel composite oxide represented by the following composition formula (1): LibNi1-aM1aO2 (1) (where M1 represents at least one element selected from transition metal elements other than Ni, elements of the second group of the Periodic System and elements of the thirteenth group of the Periodic System; a satisfies the condition 0.01≤a≤0.5; and b satisfies the condition 0.85≤b≤1.05). The content of carbon in the lithium nickel composite oxide is equal to or less than 0.08% by mass.
摘要:
The present invention provides a cathode active material that makes possible a high capacity nonaqueous electrolyte secondary battery that has excellent discharge load characteristics that provide both good cycle characteristics and thermal stability. The cathode active material comprises a lithium nickel composite oxide having the compositional formula LiNi1−aMaO2 (where, M is at least one kind of element that is selected from among a transitional metal other than Ni, a group 2 element, and group 13 element, and 0.01≦a≦0.5) to which fine lithium manganese composite oxide particle adhere to the surface thereof. This lithium nickel composite oxide is obtained by adding manganese salt solution to a lithium nickel composite oxide slurry, causing manganese hydroxide that contains lithium to adhere to the surface of the lithium nickel composite oxide particles, and then baking that lithium nickel composite oxide.
摘要:
To curb a decline in the high-rate performance of non-aqueous electrolyte secondary batteries and improve safety at the time of an internal short circuit, a non-aqueous electrolyte secondary battery includes a positive electrode, a negative electrode, a separator, and a non-aqueous electrolyte wherein the positive electrode includes a positive electrode active material capable of absorbing and desorbing lithium ions, the positive electrode active material includes a secondary particle, and the secondary particle is an aggregate containing primary particles and a silicon oxide. The primary particles contain a lithium nickel composite oxide. The silicon oxide is present in at least grain boundaries between the primary particles.