摘要:
A steel sheet with a metallic coating is provided. A composition of the metallic coating includes from 2.0 to 24.0% by weight of zinc, from 7.1 to 12.0% by weight of silicon, optionally from 1.1 to 8.0% by weight of magnesium, and optionally additional elements chosen from Pb, Ni, Zr, or Hf. The content by weight of each additional element is less than 0.3%. A balance of the composition is aluminum, unavoidable impurities and residual elements. A ratio Al/Zn is from 4.0 to 6.0.
摘要:
A metallic foil for lightning strike protection in a composite aerospace structure having a length, a width, and a thickness of not more than 30 microns. There are a plurality of pores of a predefined geometric shape extending through the thickness of the metallic foil and being distributed across a surface area defined by the length and the width of the metallic foil. The plurality of pores in the aggregate define an open area of not more than 40% of the surface area and the metallic foil has a weight of not more than 115 g/m2. The metallic foil has a weight to conductivity ratio of not more than 0.40 gram-ohms per square.
摘要:
One aspect of this copper alloy for an electronic and electrical equipment contains: more than 2.0 mass % to 36.5 mass % of Zn; 0.10 mass % to 0.90 mass % of Sn; 0.15 mass % to less than 1.00 mass % of Ni; and 0.005 mass % to 0.100 mass % of P, with the balance containing Cu and inevitable impurities, wherein atomic ratios of amounts of elements satisfy 3.00
摘要:
The present disclosure relates to a graphite oxide-containing resin formulation, including: 15-80 parts by weight of a polyamideimide precursor, 0.01-10 parts by weight of a graphite oxide as a dispersant, 10-400 parts by weight of an inorganic powder, and 20-350 parts by weight of a solvent.
摘要:
Present invention provides an electro-deposited copper foil having the equivalent low-profile surface as in a conventional low-profile electro-deposited copper foil and extremely large mechanical strength and a method for manufacturing the same. The electro-deposited copper foil is formed by depositing fine copper crystal grains having a small deviation of grain-diameter. The electro-deposited copper foil has a low-profile and glossy surface and has extremely large mechanical strength expressed by a tensile strength as received of 70 kgf/mm2 to 100 kgf/mm2 and has a tensile strength after heating (180° C. for 60 minutes) corresponding to 85% or more of the tensile strength as received. The electro-deposited copper foil is manufactured by electrolysis using a sulfuric acid base copper electrolytic solution containing a compound composed of a benzene ring having a sulfo group bonded thereto, a sulfonate of an active sulfur compound and a polymer of a quaternary ammonium salt having a cyclic structure.
摘要翻译:本发明提供了一种电镀铜箔,其具有与传统的薄型电沉积铜箔相当的低轮廓表面和极大的机械强度及其制造方法。 电沉积铜箔通过沉积具有小直径偏差的细铜晶粒形成。 电沉积铜箔具有低轮廓和光泽的表面,并且具有由70kgf / mm 2至100kgf / mm 2的拉伸强度表示的非常大的机械强度,并且具有加热后的拉伸强度(180℃,对于 60分钟),相当于收到的拉伸强度的85%以上。 电解铜箔通过使用含有由与其结合的具有磺基的苯环构成的化合物的硫酸基铜电解液,活性硫化合物的磺酸盐和季铵盐的聚合物进行电解而制造,所述季铵盐具有 循环结构。
摘要:
A metal foil including: a steel layer whose thickness is 10 to 200 μm; an alloy layer which contains Fe and Al and which is formed on the steel layer; and an Al-containing metal layer arranged on the alloy layer, wherein, when a cutting-plane line of a surface of the Al-containing metal layer is defined as a contour curve and an approximation straight line of the contour curve is defined as a contour average straight line, a maximum point, whose distance from the contour average straight line is more than 10 μm, is absent on the contour curve, and a thickness of the alloy layer is 0.1 to 8 μm and the alloy layer contains an Al7Cu2Fe intermetallic compound or FeAl3 based intermetallic compounds.
摘要:
Provided is a hot-dip galvanized steel sheet having excellent adhesiveness at ultra-low temperatures as well as fine spangles, and a method of manufacturing the same. According to the present invention, a hot-dip galvanized steel sheet having excellent adhesiveness at ultra-low temperatures includes a base steel sheet, a composite layer formed on the base steel sheet and including transition metal, an inhibition layer formed on the composite layer and including a iron-aluminum (Fe—Al) based intermetallic compound, and a zinc (Zn)-plated layer formed on the inhibition layer, in which an average diameter of spangles in the zinc-plated layer is 150 μm or less, and a method of manufacturing the hot-dip galvanized steel sheet is provided.
摘要:
By forming a nickel-based coating layer or a cobalt-based coating layer having a coating thickness of 0.005 μm or larger and 0.05 μm or smaller on an outermost surface of a tin-based surface layer of a terminal material of low-insertion force in which an asperity shape of an interface between a copper-tin alloy layer and a tin-based surface layer is controlled, it is possible to reduce insertion force of fitting even though all-purpose tin-plated terminal material is used by combination.
摘要:
There is provided a surface-treated steel sheet for battery containers. The surface-treated sheet is used to form a battery container for a battery. The battery uses a nonaqueous electrolytic solution as an electrolytic solution. The surface-treated steel sheet is characterized by the features as below. The surface-treated steel sheet includes a base material made of steel and an iron-nickel diffusion layer formed by performing thermal diffusion treatment after forming a nickel plating layer at least on a surface of the base material to be located at the inner surface side of the battery container. The iron-nickel diffusion layer has an outermost layer of which a ratio of Ni and Fe is 7.5 or less as a molar ratio of Ni/Fe. The iron-nickel diffusion layer has a thickness of 0.6 μm or more.
摘要:
The present invention provides a carrier-attached copper foil, wherein an ultrathin copper foil is not peeled from the carrier prior to the lamination to an insulating substrate, but can be peeled from the carrier after the lamination to the insulating substrate. A carrier-attached copper foil comprising a copper foil carrier, an intermediate layer laminated on the copper foil carrier, and an ultrathin copper layer laminated on the intermediate layer, wherein the intermediate foil is configured with a Ni layer in contact with an interface of the copper foil carrier and a Cr layer in contact with an interface of the ultrathin copper layer, said Ni layer containing 1,000-40,000 μg/dm2 of Ni and said Cr layer containing 10-100 μg/dm2 of Cr is provided.